    • Method of making welded can body
    • 焊罐罐体制作方法
    • US4595326A
    • 1986-06-17
    • US648214
    • 1984-09-07
    • Kenji MatsunoKazuhisa Ishibashi
    • Kenji MatsunoKazuhisa Ishibashi
    • B23K11/24B23K11/06B23K11/30
    • B23K11/309B23K11/063
    • There is provided a method of making a welded can body having a mash seam weld which includes a heat affected zone extending continuously in the longitudinal direction thereof and is formed with no pitting. The weld is formed by mash seam welding a lapped portion of a can body preform made of a surface treated steel sheet while allowing an alternating current to flow through the lapped portion via a water-cooled elongated electrode and a water-cooled rotary electrode. The alternating current has a crest factor satisfying an expression 1.5.ltoreq.Ip/Ie.ltoreq.2.0, where Ie and Ip designate an effective value and a peak value, respectively, of the alternating current.
    • 提供了一种制造具有压薄缝焊接的焊接罐体的方法,其包括在其纵向方向上连续延伸的热影响区域,并且没有形成点蚀。 焊接是通过压薄焊接由表面处理钢板制成的罐体预制件的重叠部分,同时允许交流电流通过水冷细长电极和水冷旋转电极流过研磨部分而形成的。 交流电流具有满足1.5≤Ip/ Ie <2.0的波峰因数,其中Ie和Ip分别表示交流电的有效值和峰值。
    • 5. 发明授权
    • Methods and apparatus for manufacturing tubes
    • 用于制造管子的方法和装置
    • US4800250A
    • 1989-01-24
    • US64548
    • 1987-06-22
    • Michio WatanabeKazuhisa IshibashiKenji MatsunoHideo Kurashima
    • Michio WatanabeKazuhisa IshibashiKenji MatsunoHideo Kurashima
    • B21D51/26B21C37/08B23K26/26B23K26/00
    • B21C37/0822B21C37/08B23K26/262
    • A method and apparatus for guiding the opposed edges of sheet material into substantially abutting edge-to-edge relationship with one another and thereafter welding said edges by a high energy welding source to form a seam. The invention enables the continuous high speed butt welding of the sheet material to form cylindrical bodies. The apparatus includes three elements, a mandrel, a mandrel holder and tube holders. Sheet material is fed to around said mandrel and advanced by a tube holder with an edge of two opposite edges of said sheet material being in intimate contact with a basis plane of said mandrel holder. Another edges is slided into contact with above mentioned edge of sheet material making abutting relationship after passing through the basis plane of said mandrel holder. These abutting edges pass a high energy zone of a welder and butt welded to make a tube.
    • 一种用于将片材的相对边缘引导成彼此基本上邻接的边缘到边缘关系的方法和装置,然后通过高能量焊接源焊接所述边缘以形成接缝。 本发明能够使片材的连续高速对接焊接形成圆柱体。 该装置包括三个元件,心轴,心轴保持器和管座。 片材被馈送到所述心轴周围并由管保持器推进,其中所述片材的两个相对边缘的边缘与所述心轴保持器的基础平面紧密接触。 另外的边缘与上述片材的边缘滑动接触,在穿过所述心轴保持器的基面之后形成邻接关系。 这些邻接边缘通过焊机的高能区域并对接焊接以制造管。
    • 9. 发明授权
    • Process for production of aluminum hydroxide from ore containing alumina
    • 从含氧化铝的矿石生产氢氧化铝的方法
    • US5545384A
    • 1996-08-13
    • US465620
    • 1995-06-05
    • Takuo HaratoTakahiro IshidaYoshio KumagaeMichikazu InamiKazuhisa IshibashiMitsuaki Murakami
    • Takuo HaratoTakahiro IshidaYoshio KumagaeMichikazu InamiKazuhisa IshibashiMitsuaki Murakami
    • C01F7/06C01F7/47C01F7/00C01F7/02C22B21/00
    • C01F7/062C01F7/47
    • A process for the production of aluminum hydroxide from an alumina-containing ore comprising, in a process for the production of aluminum hydroxide involving extraction of alumina from an alumina-containing ore by an aqueous alkaline solution, supplying a slurry containing the alumina-containing ore at a high solid content which is prepared from a small amount of an alkaline solution together with an aqueous alkaline solution which is so preheated to a temperature that a preheated temperature is enough high to have a temperature after the mixing with the slurry which is higher than an extraction temperature of alumina, simultaneously or after the mixing them, to an extraction apparatus comprising of a tube reactor, extracting alumina from the alumina-containing ore under extraction conditions of a temperature of 120.degree.-160.degree. C. and an extraction time within 10 minutes, separating dissolution residue from an extract solution immediately after the extraction, desilicating the extract solution, and adding seeds of aluminum hydroxide to the extract solution which is desilicated so as to precipitate aluminum hydroxide. By the production process, it is possible to economically produce aluminum hydroxide with little contamination by silica from the alumina-containing ore with a high content of the reactive silica.
    • 一种用于从含氧化铝的矿石生产氢氧化铝的方法,包括在生产氢氧化铝的方法中涉及通过碱性水溶液从含氧化铝的矿石中提取氧化铝,提供含有含氧化铝的矿石 在高固体含量下,由少量的碱性溶液与碱性水溶液一起制备,碱水溶液如此预热至预热温度足够高以使浆料混合后的温度高于 将氧化铝的同时或混合后的提取温度提取到包括管式反应器的提取装置中,在120-116℃的提取条件下从含氧化铝的矿石中提取氧化铝,提取时间在 10分钟后,在提取后立即从提取液中分离出溶解残渣,使提取物脱硅 溶液,并将氢氧化铝的种子加入到脱液的提取液中以沉淀氢氧化铝。 通过生产过程,可以经济地生产具有高含量的反应性二氧化硅的来自含氧化铝的矿石几乎不受二氧化硅污染的氢氧化铝。