    • 2. 发明授权
    • Process for producing carboxylic acid esters and catalysts therefor
    • 制备羧酸酯及其催化剂的方法
    • US5922900A
    • 1999-07-13
    • US922558
    • 1997-09-03
    • Stefan WielandPeter Panster
    • Stefan WielandPeter Panster
    • B01J31/06C07B61/00C07C67/08C07C69/14C07C69/80C07C67/00C08G77/00C08G79/00
    • C07C67/08
    • A process for producing carboxylic acid esters by the following steps:a) preparation of a reaction mixture containing an alcohol and a carboxylic acid and/or a carboxylic anhydride and/or a carboxylic acid ester and or a partially esterified carboxylic acid,b) heating of this mixture to the suitable reaction temperature in the presence of a solid polysiloxane insoluble in the reaction medium and having sulphonic acid groups with intensive thorough mixing accompanied by continuous separation of the reaction water which forms, wherein the polysiloxane used as the catalyst in modified by treatment with a soluble aluminum, titanium or zirconium compound, and the spherical particles thereof have a diameter of 0.01 to 3 mm, a specific surface of 0.1 to 1200 m.sup.2 /g, a specific pore volume of 0.01 to 6.0 ml/g and a bulk density of 50 to 1000 g/l.
    • 一种通过以下步骤制备羧酸酯的方法:a)制备含有醇和羧酸和/或羧酸酐和/或羧酸酯和/或部分酯化的羧酸的反应混合物,b)加热 该混合物在不溶于反应介质的固体聚硅氧烷存在下具有适当的反应温度,并且具有强烈浓缩的磺酸基团,伴随着形成的反应水的连续分离,其中用作催化剂的聚硅氧烷被改性为 用可溶性铝,钛或锆化合物处理,其球形颗粒的直径为0.01〜3mm,比表面积为0.1〜1200m2 / g,比孔体积为0.01〜6.0ml / g,体积 密度为50〜1000g / l。
    • 6. 发明授权
    • Shaped organosiloxane polycondensates, process for their preparation and
use
    • 成型有机硅氧烷缩聚物,其制备和使用过程
    • US5466767A
    • 1995-11-14
    • US340877
    • 1994-11-15
    • Stefan WielandPeter PansterHorst Grethe
    • Stefan WielandPeter PansterHorst Grethe
    • C08G77/48C08G77/54C08G77/58C08G77/26C08G77/22C08G77/30
    • C08G77/54C08G77/48C08G77/58
    • Disclosed are shaped organosiloxane polycondensates in the form of macroscopic spherical particles with a diameter of 0.01 to 2.5 mm, a specific surface area of 0.01 to 1000 m.sup.2 /g, a specific pore volume of 0.01 to 5 ml/g, and a bulk density of 50 to 1000 g/l, consisting of units of the formula (I):X--R.sup.1 (I)and/or the formula (II):R.sup.2 --Y--R.sup.3 (II)and the formula (III): ##STR1## as well as optionally, in addition, units of the formula ##STR2## wherein R.sup.1 to R.sup.3 are identical or different and represent a group of the formula (V): ##STR3## R.sup.4 being bonded directly to the X or Y group and representing a linear or branched, fully saturated or unsaturated alkylene group, a cycloalkylene group, a phenylene group or a unit of the formula ##STR4## and M corresponding to a Si, Ti or Zr atom. Also disclosed are a process for preparation and use.
    • 公开了直径为0.01〜2.5mm,比表面积为0.01〜1000m2 / g,比孔体积为0.01〜5ml / g的宏观球状颗粒形状的成型有机硅氧烷缩聚物,体积密度为 由式(I):X-R1(I)和/或式(II):R2-Y-R3(Ⅱ)和式(Ⅲ)组成的单位为50〜1000g / (III)的化合物,另外还有式(IV)的单元,其中R 1至R 3相同或不同并且表示式(Ⅴ)的基团:或Y基团,并且表示直链或支链的 完全饱和或不饱和的亚烷基,亚环烷基,亚苯基或下式的单元,即对应于Si,Ti或Zr原子的式“IMAGE”或“IMAGE”和M。 还公开了一种制备和使用的方法。
    • 9. 发明授权
    • Process for preparing glycide by epoxidation using polymeric
organosiloxane ammonium salts of oxoacids of the elements V, Nb, Ta,
Mo, and W
    • 使用元素V,Nb,Ta,Mo和W的含氧酸的聚合有机硅氧烷铵盐通过环氧化制备糖苷的方法
    • US5286885A
    • 1994-02-15
    • US53248
    • 1993-04-28
    • Peter GoetzStefan WielandPeter PansterGustaaf GoorRainer Siegmeier
    • Peter GoetzStefan WielandPeter PansterGustaaf GoorRainer Siegmeier
    • C08G77/54C08G77/58C07D301/12C07D303/14
    • C08G77/54C08G77/58
    • The invention relates to polymeric organosiloxane ammonium salts having a silica-like skeleton and including units of Formula (I): ##STR1## wherein R.sup.1 and R.sup.2 are identical or different and signify a group of Formula (II): ##STR2## wherein R.sup.5 is an alkylene group and the oxygen atoms are saturated by silicon atoms of additional groups corresponding to Formula (II), optionally with the insertion of cross-linking agents; R.sup.3 represents groups corresponding to R.sup.1 or R.sup.2, or hydrogen or an alkyl group; R.sup.4 represents hydrogen or an alkyl group; x is the charge number of an oxo anion of a monooxo-, isopolyoxo- or heteropolyoxo acid of the elements vanadium, niobium, tantalum, molybdenum or tungsten; and oxo groups of the X anion also may be replaced by peroxo groups. The invention also includes methods of preparing the salts of Formula (I) from salts of the type (R.sup.1 R.sup.2 R.sup.3 R.sup.4 N.sup.+).sub.y Y wherein Y is different from X. The invention further includes the use of the salts of Formula (I) as catalyst for oxidation reactions using peroxo compounds as an oxidation agent.
    • 本发明涉及具有二氧化硅样骨架并包括式(I)的单元的聚合有机硅氧烷铵盐:(*化学结构*)(I)其中R1和R2相同或不同并且表示式(II)的基团: (*化学结构*)(II)其中R5是亚烷基并且氧原子被对应于式(II)的另外的基团的硅原子饱和,任选地插入交联剂; R3表示对应于R1或R2的基团,或氢或烷基; R4表示氢或烷基; x是元素钒,铌,钽,钼或钨元素的单氧,异羟基或杂多酸的氧阴离子的电荷数; X阴离子的氧基也可以被过氧基取代。 本发明还包括从其中Y不同于X的类型(R 1 R 2 R 3 R 4 N +)y Y的盐制备式(I)的盐的方法。本发明还包括使用式(I)的盐作为氧化反应的催化剂,其使用 过氧化合物作为氧化剂。