    • Method of manufacturing polycrystalline silicon rod
    • 多晶硅棒的制造方法
    • US08328935B2
    • 2012-12-11
    • US12418165
    • 2009-04-03
    • Michihiro MizunoShinichi KurotaniShigeyoshi NetsuKyoji Oguro
    • Michihiro MizunoShinichi KurotaniShigeyoshi NetsuKyoji Oguro
    • C30B23/00C30B25/00C30B28/12C30B28/14
    • C01B33/03C01B33/035
    • The present invention is a method of manufacturing polycrystalline silicon rods, wherein silicon is deposited onto a silicon core wire by a chemical vapor deposition (CVD) method such that a silicon member, which is cut out from a single-crystalline silicon ingot at an off-angle range of 5 to 40 degrees relative to a crystal habit line of the ingot, is used as the silicon core wire. The single-crystalline silicon ingot is preferably grown by a Czochralski (CZ) method or floating zone (FZ) method, such that the ingot preferably has an interstitial oxygen concentration of 7 ppma to 20 ppma. Silicon rods produced by this method are less likely to suffer a breakage caused by cleavage during the growth process of polycrystalline silicon during CVD, and exhibit improved FZ method success rates. The polycrystalline silicon rods produced by this method also have low impurity contamination and high single-crystallization efficiency.
    • 本发明是一种制造多晶硅棒的方法,其中通过化学气相沉积(CVD)方法将硅沉积到硅芯线上,使得从断开的单晶硅锭切出的硅构件 使用相对于锭的晶体习性线5〜40度的角度范围,作为硅芯线。 单晶硅锭优选通过切克劳斯基(CZ)法或浮动区(FZ)法生长,使得锭优选具有7ppma至20ppma的间隙氧浓度。 通过该方法制造的硅棒在CVD期间不太可能在多晶硅生长过程中由于断裂引起的断裂,并且显示出改进的FZ方法成功率。 通过该方法制造的多晶硅棒也具有低杂质污染和高单结晶效率。