    • 7. 发明授权
    • Production of rigid polyurethane foams
    • 生产刚性聚氨酯泡沫
    • US5895792A
    • 1999-04-20
    • US935911
    • 1997-09-23
    • Udo RotermundRenate HempelHolger SeifertWerner Wiegmann
    • Udo RotermundRenate HempelHolger SeifertWerner Wiegmann
    • C08J9/12C08G18/06C08G18/48C08G18/50
    • C08G18/5033C08G18/482C08G2101/0025C08G2101/0033C08G2101/005C08G2101/0058C08G2101/0083
    • In a process for producing rigid polyurethane foams having improved heat distortion resistance and reduced thermal conductivity by reactinga) polyisocyanates withb) compounds containing hydrogen atoms reactive toward isocyanates, in the presence ofc) water, and, if desired,d) physically acting blowing agents ande) catalysts and known auxiliaries and/or additives, the compounds b) containing hydrogen atoms reactive toward isocyanates are a polyol mixture comprisingb1) a polyol which can be prepared by addition of ethylene oxide and/or propylene oxide onto a hexitol or a hexitol mixture, with the total hexitol content of the polyol mixture being from 15 to 30% by weight, based on the polyol mixture, andb2) a polyol which can be prepared by addition of ethylene oxide and/or propylene oxide onto one or more aromatic amines, with the total amine content of the polyol mixture being from 1 to 10% by weight, based on the polyol mixture, and the amount of the polyol mixture in the component b) is from 60 to 100 parts by mass per 100 parts by mass of the component b).
    • 在制备具有改善的耐热变形性和降低热导率的硬质聚氨酯泡沫体的方法中,通过使a)多异氰酸酯与b)在c)水和(如果需要)d)的存在下,对含有氢原子的异氰酸酯反应的化合物d) 发泡剂和e)催化剂和已知的助剂和/或添加剂,包含对异氰酸酯具有反应性的氢原子的化合物b)是多元醇混合物,其包含b1)可以通过在己糖醇中加入环氧乙烷和/或环氧丙烷制备的多元醇 或己糖醇混合物,其中多元醇混合物的总己糖醇含量为基于多元醇混合物的15至30重量%,和b2)可通过将环氧乙烷和/或环氧丙烷加成到一个上制备的多元醇 或更多的芳族胺,多元醇混合物的总胺含量基于多元醇混合物为1至10重量%,并且组分中的多元醇混合物的量 b)相对于100质量份组分b)为60〜100质量份。
    • 8. 发明授权
    • Process for the production of rigid polyurethane foams
    • 生产硬质聚氨酯泡沫的方法
    • US5886062A
    • 1999-03-23
    • US904894
    • 1997-08-01
    • Karl-Werner DietrichTorsten HeinemannManfred Dietrich
    • Karl-Werner DietrichTorsten HeinemannManfred Dietrich
    • C08G18/32C08G18/48C08G18/50C08G18/66C08G101/00
    • C08G18/482C08G18/329C08G18/4891C08G18/5021C08G18/5033C08G18/6696C08G2101/0025
    • This invention provides a process for producing rigid polyurethane foams by reacting A) a polyol component with B) a polyisocyanate component in the presence of C) water, D) at least one catalyst, and, optionally, E) at least one blowing agent. This process specifically requires A) a polyol component which comprises: 1) a polyol containing at least two isocyanate-reactive hydrogen atoms and comprising: a) a mixture of i) an addition product having a OH number of at least 500 of diamines or polyamines containing primary and/or secondary amino groups with alkylene oxides, and ii) castor oil, and/or b) one or more reaction products obtained by reacting i) an addition product having a OH number of at least 500 of diamines or polyamines containing primary and/or secondary amino groups with alkylene oxides, and ii) castor oil; and 2) at least one compound containing at least two isocyanate-reactive hydrogen atoms. Suitable polyisocyanates B) for the present invention are those containing an NCO group content of from 20 to 48% by weight.
    • 本发明提供一种生产刚性聚氨酯泡沫体的方法,该方法通过在C)水,D)至少一种催化剂和任选的E)至少一种发泡剂的存在下,使A)多元醇组分与B)多异氰酸酯组分反应。 该方法特别要求A)多元醇组分,其包括:1)含有至少两个异氰酸酯反应性氢原子的多元醇,其包含:a)i)具有OH数至少为500的二胺或多胺的加成产物 含有伯和/或仲氨基与烯化氧,和ii)蓖麻油和/或b)一种或多种反应产物,其通过使i)具有OH数为至少500个的二胺或含有伯胺的多胺的加成产物 和/或具有环氧烷烃的仲氨基,和ii)蓖麻油; 和2)至少一种含有至少两个异氰酸酯反应性氢原子的化合物。 适用于本发明的多异氰酸酯B)是含有20至48重量%的NCO基团含量的那些。