会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明授权
    • Method of forming ONO-type sidewall with reduced bird's beak
    • 用鸟喙形成ONO型侧壁的方法
    • US07910429B2
    • 2011-03-22
    • US10821100
    • 2004-04-07
    • Zhong DongChuck JangChing-Hwa ChenChunchieh HuangJin-Ho KimVei-Han ChanChung Wai LeungChia-Shun HsiaoGeorge KovallSteven Ming Yang
    • Zhong DongChuck JangChing-Hwa ChenChunchieh HuangJin-Ho KimVei-Han ChanChung Wai LeungChia-Shun HsiaoGeorge KovallSteven Ming Yang
    • H01L21/336
    • H01L21/28273H01L29/42328H01L29/513H01L29/7881
    • Conventional fabrication of sidewall oxide around an ONO-type memory cell stack usually produces Bird's Beak because prior to the fabrication, there is an exposed sidewall of the ONO-type memory cell stack that exposes side parts of a plurality of material layers respectively composed of different materials. Certain materials in the stack such as silicon nitrides are more difficult to oxidize than other materials in the stack such polysilicon. As a result oxidation does not proceed uniformly along the multi-layered height of the sidewall. The present disclosure shows how radical-based fabrication of sidewall dielectric can help to reduce the Bird's Beak formation. More specifically, it is indicated that short-lived oxidizing agents (e.g., atomic oxygen) are able to better oxidize difficult to oxidize materials such as silicon nitride and the it is indicated that the short-lived oxidizing agents alternatively or additionally do not diffuse as deeply through already oxidized layers of the sidewall such as silicon oxide layers. As a result, a more uniform sidewall dielectric can be fabricated with more uniform breakdown voltages along it height.
    • 通常在ONO型存储单元堆叠周围制造侧壁氧化物通常产生鸟喙,因为在制造之前,存在ONO型存储单元堆叠的暴露的侧壁,其暴露分别由不同的多个材料层组成的多个材料层的侧面部分 材料 堆叠中的某些材料如氮化硅比堆叠中的其它材料更难以氧化,这样的多晶硅。 结果,氧化不沿着侧壁的多层高度均匀地进行。 本公开显示了基于侧壁电介质的基于基础的制造有助于减少鸟喙形成。 更具体地,表明短寿命氧化剂(例如原子氧)能够更好地氧化难以氧化的材料如氮化硅,并且表明短寿命氧化剂交替地或另外不扩散为 深深地通过侧壁的已氧化层,例如氧化硅层。 结果,可以制造更均匀的侧壁电介质,沿其高度具有更均匀的击穿电压。
    • 5. 发明申请
    • Use of multiple etching steps to reduce lateral etch undercut
    • 使用多个蚀刻步骤来减少横向蚀刻底切
    • US20060211255A1
    • 2006-09-21
    • US11432222
    • 2006-05-10
    • Chunchieh HuangChia-Shun HsiaoJin-Ho KimKuei-Chang TsaiBarbara HaseldenDaniel Wang
    • Chunchieh HuangChia-Shun HsiaoJin-Ho KimKuei-Chang TsaiBarbara HaseldenDaniel Wang
    • H01L21/302
    • H01L27/105H01L27/115H01L27/11526H01L27/11539
    • In integrated circuit fabrication, an etch is used that has a lateral component. For example, the etch may be isotropic. Before the isotropic etch of a layer (160), another etch of the same layer is performed. This other etch can be anisotropic. This etch attacks a portion (160X2) of the layer adjacent to the feature to be formed by the isotropic etch. That portion is entirely or partially removed by the anisotropic etch. Then the isotropic etch mask (420) is formed to extend beyond the feature over the location of the portion subjected to the anisotropic etch. If that portion was removed entirely, then the isotropic etch mask may completely seal off the feature to be formed on the side of that portion, so the lateral etching will not occur. If that portion was removed only partially, then the lateral undercut will be impeded because the passage to the feature under the isotropic etch mask will be narrowed.
    • 在集成电路制造中,使用具有侧向分量的蚀刻。 例如,蚀刻可以是各向同性的。 在层(160)的各向同性蚀刻之前,执行相同层的另一蚀刻。 这种其他蚀刻可以是各向异性的。 该蚀刻攻击通过各向同性蚀刻形成的与特征相邻的层的部分(160×2)。 该部分被各向异性蚀刻完全或部分地去除。 然后,各向同性蚀刻掩模(420)被形成为延伸超过经过各向异性蚀刻的部分的位置的特征。 如果完全去除该部分,则各向同性蚀刻掩模可以完全密封要在该部分侧面上形成的特征,因此不会发生横向蚀刻。 如果该部分仅部分被去除,则横向底切将被阻碍,因为在各向同性蚀刻掩模下的特征的通过将变窄。
    • 9. 发明申请
    • Precision creation of inter-gates insulator
    • US20070264776A1
    • 2007-11-15
    • US11801301
    • 2007-05-08
    • Zhong DongChuck JangChunchieh Huang
    • Zhong DongChuck JangChunchieh Huang
    • H01L21/336
    • H01L29/511H01L29/40114
    • An ONO-type inter-poly insulator is formed by depositing intrinsic silicon on an oxidation stop layer. In one embodiment, the oxidation stop layer is a nitridated top surface of a lower, and conductively-doped, polysilicon layer. In one embodiment, atomic layer deposition (ALD) is used to precisely control the thickness of the deposited, intrinsic silicon. Heat and an oxidizing atmosphere are used to convert the deposited, intrinsic silicon into thermally-grown, silicon dioxide. The oxidation stop layer impedes deeper oxidation. A silicon nitride layer and an additional silicon oxide layer are further deposited to complete the ONO structure before an upper, and conductively-doped, polysilicon layer is formed. In one embodiment, the lower and upper polysilicon layers are patterned to respectively define a floating gate (FG) and a control gate (CG) of an electrically re-programmable memory cell. In an alternative embodiment, after the middle, silicon nitride of the ONO structure is defined, another layer of intrinsic silicon is deposited, by way of for example, ALD. Heat and an oxidizing atmosphere are used to convert the second deposited, intrinsic silicon into thermally-grown, silicon dioxide. An ONO structure with two thermally-grown, and spaced apart, silicon oxide layers is thereby provided.
    • 10. 发明申请
    • Precision creation of inter-gates insulator
    • 精密创建栅极间绝缘体
    • US20050106793A1
    • 2005-05-19
    • US10718008
    • 2003-11-19
    • Zhong DongChuck JangChunchieh Huang
    • Zhong DongChuck JangChunchieh Huang
    • H01L21/28H01L29/51H01L21/336
    • H01L29/511H01L21/28273
    • An ONO-type inter-poly insulator is formed by depositing intrinsic silicon on an oxidation stop layer. In one embodiment, the oxidation stop layer is a nitridated top surface of a lower, and conductively-doped, polysilicon layer. In one embodiment, atomic layer deposition (ALD) is used to precisely control the thickness of the deposited, intrinsic silicon. Heat and an oxidizing atmosphere are used to convert the deposited, intrinsic silicon into thermally-grown, silicon dioxide. The oxidation stop layer impedes deeper oxidation. A silicon nitride layer and an additional silicon oxide layer are further deposited to complete the ONO structure before an upper, and conductively-doped, polysilicon layer is formed. In one embodiment, the lower and upper polysilicon layers are patterned to respectively define a floating gate (FG) and a control gate (CG) of an electrically re-programmable memory cell. In an alternative embodiment, after the middle, silicon nitride of the ONO structure is defined, another layer of intrinsic silicon is deposited, by way of for example, ALD. Heat and an oxidizing atmosphere are used to convert the second deposited, intrinsic silicon into thermally-grown, silicon dioxide. An ONO structure with two thermally-grown, and spaced apart, silicon oxide layers is thereby provided.
    • 通过在氧化停止层上沉积本征硅来形成ONO型多晶硅绝缘体。 在一个实施方案中,氧化停止层是较低且导电掺杂的多晶硅层的氮化顶表面。 在一个实施例中,原子层沉积(ALD)用于精确控制沉积的本征硅的厚度。 使用热和氧化气氛将沉积的本征硅转化成热生长的二氧化硅。 氧化停止层阻碍更深的氧化。 在形成上部和导电掺杂的多晶硅层之前,进一步沉积氮化硅层和另外的氧化硅层以完成ONO结构。 在一个实施例中,下部和上部多晶硅层被图案化以分别限定电可重新编程的存储器单元的浮动栅极(FG)和控制栅极(CG)。 在替代实施例中,在中间形成ONO结构的氮化硅之后,通过例如ALD沉积另一层本征硅。 使用热和氧化气氛将第二沉积的本征硅转化成热生长的二氧化硅。 由此提供具有两个热生长和间隔开的氧化硅层的ONO结构。