    • 3. 发明授权
    • Catalyst for olefinic hydrocarbon polymerization and process and
producing olefinic hydrocarbon polymer
    • 用于烯烃聚合的催化剂和制备和生产烯烃聚合物
    • US5191041A
    • 1993-03-02
    • US821037
    • 1992-01-16
    • Hayato SabaKeisaku YamamotoAkio ImaiKiyoyuki SugimoriKizuku Wakatsuki
    • Hayato SabaKeisaku YamamotoAkio ImaiKiyoyuki SugimoriKizuku Wakatsuki
    • C08F10/00
    • C08F10/00
    • An inert hydrocarbon solvent-soluble catalyst for polymerization of olefinic hydrocarbons and a process for producing an olefinic polymer using the same are disclosed, the catalyst being composed of (A) a reaction product obtained by reacting (a) at least one vanadium compound represented by formula:VO(OR).sub.m X.sub.3-mwherein R represents a hydrocarbon group; X represents a halogen atom; and m represents a real number of from 0 to 3, and (b) a dihydroxy hydrocarbon compound constituted of a straight chain hydrocarbon skeleton containing from 2 to 12 carbon atoms and having a hydroxyl group at each of both terminals thereof and at least one hydrocarbon branch bonded to said hydrocarbon skeleton in an inert hydrocarbon solvent at an (a) to (b) molar ratio of from 1:0.5 to 1:1.4 and (B) at least one organoaluminum compound represented by formula:R'.sub.n AlX'.sub.3-nwherein R' represents a hydrocarbon group; X' represents a halogen atom; and n represents a real number more than 0 and less than 3. Olefinic hydrocarbon polymers having narrow distributions of molecular weight and composition can be produced with high efficiency and high polymerization activity without being accompanied by obstruction or contamination of equipment due to precipitation of a catalyst.
    • 公开了一种用于烯烃聚合的惰性烃溶剂可溶性催化剂和使用其的制备烯烃聚合物的方法,该催化剂由(A)通过使(a)至少一种钒化合物 式:VO(OR)mX3-m其中R表示烃基; X表示卤原子; m表示0〜3的实数,(b)由含有2〜12个碳原子的直链烃骨架构成的二羟基烃化合物,其两末端具有羟基,至少一个烃 在(a)至(b)摩尔比为1:0.5至1:1.4的惰性烃溶剂中与所述烃骨架键合的至少一种有机铝化合物,和(B)至少一种由式:R'nAlX'3- n其中R'表示烃基; X'表示卤原子; 并且n表示大于0且小于3的实数。可以以高效率和高聚合活性生产具有窄分子量和组成分布的烯属烃聚合物,而不伴随催化剂沉淀引起的设备阻塞或污染 。
    • 7. 发明授权
    • Rubber composition for tire treads
    • 轮胎胎面橡胶组合物
    • US5430086A
    • 1995-07-04
    • US165164
    • 1993-12-10
    • Yuichi SaitoToru FukumotoShuji ImaokaKeisaku YamamotoKizuku WakatsukiMitsuji Tsuji
    • Yuichi SaitoToru FukumotoShuji ImaokaKeisaku YamamotoKizuku WakatsukiMitsuji Tsuji
    • B60C1/00C08K3/04C08L9/06
    • C08K3/04B60C1/0016C08L9/06C08L2205/02C08L7/00C08L9/00C08L9/08Y10S152/905
    • A rubber composition for tire treads comprising a rubber component consisting essentially of (A) 20 to 100% by weight of a solution-polymerized styrene-butadiene copolymer rubber having a Mooney viscosity ML.sub.1+4 of 30 to 200 at 100.degree. C. prepared by copolymerization of styrene, butadiene and a polyvinyl aromatic compound followed by coupling with a trifunctional or tetrafunctional coupling agent, and (B) 0 to 80% by weight of at least one rubber selected from the group consisting of an emulsion-polymerized styrene-butadiene rubber, a butadiene rubber, natural rubber and a synthetic polyisoprene rubber; and (C) 50 to 250 parts by weight of a carbon black having an iodine adsorption number of not less than 60 mg/g and an oil absorption of not less than 110 ml/100 g per 100 parts by weight of said rubber component; the tan .delta. peak temperature Tg of the cured product of said rubber composition being from -40.degree. to +5.degree. C. The tread rubber composition can be processed without causing bagging with a good dispersibility of carbon black and provides tires having a low rolling resistance and a high grip characteristic.
    • 一种用于轮胎胎面的橡胶组合物,其包含基本上由(A)20-100重量%的在100℃下门尼粘度ML1 + 4为30至200的溶液聚合的苯乙烯 - 丁二烯共聚物橡胶组成的橡胶组分,其由 苯乙烯,丁二烯和聚乙烯基芳族化合物的共聚合,然后与三官能或四官能偶联剂偶合,和(B)0至80重量%的至少一种选自乳液聚合的苯乙烯 - 丁二烯橡胶 丁二烯橡胶,天然橡胶和合成聚异戊二烯橡胶; 和(C)每100重量份所述橡胶组分50至250重量份的碘吸附数不小于60mg / g和吸油量不小于110ml / 100g的炭黑; 所述橡胶组合物的固化产物的tanδ峰值温度Tg为-40℃至+5℃。胎面橡胶组合物可以在不引起炭黑的良好分散性的情况下进行加工而且具有低滚动阻力的轮胎 和高抓地力特性。
    • 8. 发明授权
    • Butadiene copolymer and process for preparing same
    • 丁二烯共聚物及其制备方法
    • US5290878A
    • 1994-03-01
    • US72488
    • 1993-06-07
    • Keisaku YamamotoKizuku WakatsukiMitsuji TsujiYuichi Saito
    • Keisaku YamamotoKizuku WakatsukiMitsuji TsujiYuichi Saito
    • C08C19/42C08F8/00C08F36/00C08F36/06C08F236/06C08F236/10C08K5/00C08L9/00C08F8/42
    • C08F236/10
    • An elastomeric butadiene copolymer prepared by a process which comprises copolymerizing butadiene, a polyvinyl aromatic compound and optionally styrene in a hydrocarbon solvent in the presence of an organolithium polymerization initiator and subjecting the resulting copolymer having lithium at the polymer end or ends to a coupling reaction with a trifunctional or tetrafunctional coupling agent, said butadiene copolymer satisfying the following conditions: (a) the content of styrene is at most 50% by weight, (b) the content of vinyl bonds in the butadiene portion is from 10 to 90% by weight, (c) the molecular weight distribution curve obtained by a high performance liquid chromatography has at least three peaks, and 5 to 60% by weight of all the polymer chains have a molecular weight which is at least 5 times the molecular weight in terms of standard polystyrene corresponding to the peak appearing on the lowest molecular weight side of the high performance liquid chromatogram, and (d) the Mooney viscosity (ML.sub.1+4, 100.degree. C.) is from 30 to 200. The butadiene copolymer has an improved processability with excellent resilience, wet grip property, abrasion resistance and mechanical properties, and is suitable for tire use.
    • 一种弹性体丁二烯共聚物,该方法包括在有机锂聚合引发剂存在下,使丁二烯,聚乙烯基芳族化合物和任选的苯乙烯在烃溶剂中共聚,并将所得到的聚合物末端或末端的锂共聚物与 所述丁二烯共聚物满足以下条件:(a)苯乙烯含量至多为50重量%,(b)丁二烯部分中的乙烯基键含量为10〜90重量% ,(c)通过高效液相色谱获得的分子量分布曲线具有至少三个峰,并且所有聚合物链的5至60重量%的分子量的分子量至少为分子量的5倍 对应于在高效液相色谱的最低分子量侧出现的峰的标准聚苯乙烯,和(d)t 门尼粘度(ML1 + 4,100℃)为30〜200。丁二烯共聚物具有优异的回弹性,湿抓地性,耐磨性和机械性能的加工性,适用于轮胎使用。