    • Method and treatment device for the cooling of highly heated metal components
    • 用于冷却高度加热的金属部件的方法和处理装置
    • US06434949B2
    • 2002-08-20
    • US09822016
    • 2001-03-30
    • Peter BotzlerCarsten DeusLutz Wolkers
    • Peter BotzlerCarsten DeusLutz Wolkers
    • F25D2500
    • C21D1/84C21D1/613C21D1/667C21D1/767C21D9/0068
    • A method for cooling metal components highly heated in a chamber includes effecting a uniform cooling of an entire metal component. The metal component has regions each with a given mass, some of the regions having a larger mass than others of the regions. Housings are provided around regions with the relatively larger masses. The regions are subjected to the inert cooling gas in a controlled manner to a differing extent based upon the mass size. The housings are individually subjected separately with the inert cooling gas. A treatment device for cooling metal components includes a reservoir for holding inert cooling gas and a chamber for receiving a metal component to be cooled. The chamber is connected to the reservoir and has a housing for each of the regions with the larger mass. Each of the housing has an inlet orifice separately connected to the reservoir.
    • 用于冷却在室内高度加热的金属组分的方法包括实现整个金属组分的均匀冷却。 金属组分具有各自具有给定质量的区域,一些区域具有比其他区域更大的质量。 围绕具有相对较大质量的区域提供外壳。 这些区域以受控的方式以基于质量大小的不同程度进行惰性冷却气体。 这些外壳分别用惰性冷却气体承受。 用于冷却金属部件的处理装置包括用于保持惰性冷却气体的储存器和用于接收待冷却的金属部件的室。 该室连接到储存器,并且具有用于具有较大质量的每个区域的壳体。 每个壳体具有分别连接到储存器的入口孔口。
    • 5. 发明授权
    • Process for the vacuum coating of metal components
    • 金属部件真空镀膜工艺
    • US06589608B2
    • 2003-07-08
    • US09821856
    • 2001-03-30
    • Carsten DeusJoachim SenfLutz Wolkers
    • Carsten DeusJoachim SenfLutz Wolkers
    • C23C1646
    • C23C28/3215C23C8/02C23C8/10C23C28/321C23C28/345
    • A process for producing a homogeneous oxide layer on metal components includes uniformly heating the components, in all their regions, in a vacuum chamber and, after a predetermined temperature has been reached, exposing the components to an oxygen-containing gas for a predetermined period and at a predetermined pressure. The metal components are coated with MCrAlY or PtAl. The preheating temperature is between 750 and 850° C., preferably, approximately 800° C. Preferably, the thickness of the homogeneous oxide layer is between 0.01 and 5 &mgr;m. The heating is preferably by electron radiation. The predetermined period is approximately 10 minutes, and the predetermined pressure is between 1×10−3 and 8×10−2 mbar.
    • 用于在金属部件上制造均匀氧化物层的方法包括在真空室中在其所有区域中均匀加热组分,并且在达到预定温度之后,将组分暴露于含氧气体一段预定时间, 在预定压力下。 金属组分涂覆有MCrAlY或PtAl。 预热温度为750-850℃,优选为约800℃。优选地,均匀氧化物层的厚度为0.01至5μm。 加热优选通过电子辐射。 预定时间约为10分钟,预定压力为1×10 -3至8×10 -2毫巴。