    • 2. 发明授权
    • Alloy, in particular a solder alloy, for joining workpieces
    • 合金,特别是焊料合金,用于连接工件
    • US06231693B1
    • 2001-05-15
    • US08983472
    • 1998-04-23
    • Erich LugscheiderWolfgang TillmannHongshou Zhuang
    • Erich LugscheiderWolfgang TillmannHongshou Zhuang
    • B23K3526
    • B23K35/268B23K35/262
    • The invention, which enables wider use to be made of soft-soldering techniques, concerns an alloy, in particular a solder alloy, a method of joining workpieces by soldering using the solder alloy and the use of the alloy for soldering. The alloy proposed is characterized in that it contains at least 1% by wt. of an element or a mixture of elements from sub-group IVa and/or Va in the periodic table, at least 0.01% by wt. of an element or a mixture of elements from the lanthanide series; optionally at least 0.5% of silver or copper or indium or a mixture silver and/or copper and/or indium; and optionally at least 0.01% by wt. of gallium, the remainder consisting of tin or lead or a mixture of tin and lead plus, as applicable, the usual impurities. The alloy proposed can be used as solder in oxygen-containing atmospheres such as air, can be used at relatively low temperatures and efficiently wets normally difficult to wet surfaces such as ceramic surfaces. In a further embodiment of the invention, the solder alloy can be used without flux.
    • 能够更广泛地使用软钎焊技术的本发明涉及合金,特别是焊料合金,通过使用焊料合金进行焊接以及使用合金来焊接工件的方法。 提出的合金的特征在于其含有至少1重量%。 元素的元素或元素的混合物,元素周期表中Ⅳa族和/或Ⅴa族元素的混合物,至少为0.01%(重量)。 元素或来自镧系元素的元素的混合物; 任选至少0.5%的银或铜或铟或混合物银和/或铜和/或铟; 和任选地至少0.01重量%。 的镓,其余的由锡或铅组成,或者锡和铅的混合物加上通常的杂质。 所提出的合金可以用作含氧气氛如空气中的焊料,可以在相对低的温度下使用,并且通常难以湿润表面如陶瓷表面。 在本发明的另一个实施例中,可以使用焊剂合金而没有焊剂。
    • 4. 发明授权
    • Wear and corrosion resistant nickel-base alloy
    • 耐磨和耐腐蚀的镍基合金
    • US4118254A
    • 1978-10-03
    • US784376
    • 1977-04-04
    • Otto KnotekErich LugscheiderWolfgang Wichert
    • Otto KnotekErich LugscheiderWolfgang Wichert
    • C22C1/10B23K35/30C22C19/05C22C19/07C22C32/00
    • C22C19/058B23K35/304C22C19/053
    • A nickel-base wear and corrosion resistant alloy is provided containing by weight about 20% to 35% Cr, about 1% to 8% Si, about 1.7% to 3.5% C, 0 to 15% W and the balance essentially at least about 40% nickel, the amount of carbon present in said composition being stoichiometrically related to the chromium content to provide carbides based on the formula M.sub.7 C.sub.3, wherein M comprises essentially chromium, the amount of chromium in said M.sub.7 C.sub.3 compound ranging from about 65% to less than about 100% of the total chromium in said composition, the melting point of said alloy being less than about 1350.degree. C. The alloy has particular use in welding consumables for hard facing, for valve seats, for wear resistant sleeves and bushings (castings) and other uses.
    • 提供镍基耐磨损和耐腐蚀合金,其包含重量约20%至35%的Cr,约1%至8%的Si,约1.7%至3.5%的C,0至15%的W,余量基本上至少约为 40%的镍,所述组合物中存在的碳的量在化学计量上与铬含量相关,以提供基于式M7C3的碳化物,其中M基本上包含铬,所述M7C3化合物中的铬的量为约65%至小于 所述组合物中的总铬的约100%,所述合金的熔点小于约1350℃。该合金特别用于硬面,用于阀座的耐磨套和衬套(铸件)的焊接材料中。 和其他用途。
    • 8. 发明授权
    • Solder braze alloy
    • 焊锡钎焊合金
    • US06367683B1
    • 2002-04-09
    • US09462577
    • 2000-03-09
    • Ino J. RassErich LugscheiderFrank Hillen
    • Ino J. RassErich LugscheiderFrank Hillen
    • C22C1800
    • B23K35/26B23K35/262B23K35/264B23K35/268B23K35/282B23K35/3006
    • The invention, which permits active solder braze technology to be used in a more versatile manner, relates to a solder braze alloy and to a method for joining workpieces by soldering by means of a solder braze alloy. The novel alloy is characterized in that it comprises 1-10% by weight of an element or a mixture of elements of subgroup IVa and/or Va of the Periodic Table of the Elements and 0.1-20 wt% of an element or a mixture of elements of the group of the rare earths and the remainder consists of zinc, lead, tin, bismuth or indium or a mixture predominantly of two or more of the elements zinc, lead, tin, bismuth and indium and optionally of the elements silver, copper, gallium, antimony, nickel, manganese, chromium, cobalt possibly of customary impurities. The alloy according to the invention can be processed an a solder even in oxygen-containing atmospheres, for example in air, has a relatively low processing temperature and exhibits good wetting even of inherently poorly wettable surfaces such as, for example, ceramic surfaces In a development of the invention the solder braze alloy can be processed without a flux.
    • 允许活性焊料钎焊技术以更通用的方式使用的本发明涉及钎焊钎焊合金以及通过钎焊钎焊合金焊接来连接工件的方法。 该新型合金的特征在于它包含1-10重量%元素的元素或元素周期表的亚Ⅳa族元素和/或Ⅴa元素的混合物,和0.1-20重量%的元素或 稀土元素,其余部分由锌,铅,锡,铋或铟组成,或主要由锌,铅,锡,铋和铟中的两种或多种元素组成的混合物,以及任选的元素银,铜 ,镓,锑,镍,锰,铬,钴可能是常规杂质。 即使在含氧气氛中,例如在空气中,也可以将本发明的合金作为焊料加工,具有相对低的加工温度,并且即使是固有的可润湿性差的表面,例如陶瓷表面也显示良好的润湿。 本发明的开发钎焊钎焊合金可以无助焊剂加工。