会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 3. 发明授权
    • Phosphor and treatment method for the same
    • 磷光体和处理方法相同
    • US07468145B2
    • 2008-12-23
    • US10528589
    • 2003-10-07
    • Takehiro ZukawaMasatoshi KitagawaMasaharu TerauchiJunko Asayama
    • Takehiro ZukawaMasatoshi KitagawaMasaharu TerauchiJunko Asayama
    • C09K11/08
    • C09K11/7734H01J61/44H01J2211/42Y10T428/2991Y10T428/2993
    • The present invention aims at realizing a PDP and a mercury-free fluorescent lamp feasible to maintain excellent luminescent characteristics over long periods by suppressing time-lapse changes in luminescent characteristics of a phosphor that is excited by vacuum ultraviolet light to thereby emit light. To accomplish this object, the oxide phosphor of the invention comprises individual particles, each of which has a region at and near the surface thereof modified, and the elemental composition of the surface region is in a more oxidized state than that of the internal region of the particles. Alternatively, the surface region has more halogen or chalcogen in the elemental composition. In the phosphor treatment method of the invention, the surface region of individual phosphor particles is selectively modified by (i) forming a highly reactive gas atmosphere by exciting gas which contains reactive gas, and (ii) exposing the phosphor to the gas atmosphere.
    • 本发明旨在实现通过抑制由真空紫外光激发的荧光体的发光特性的延时变化从而发光的方法,实现长时间保持优异发光特性的PDP和无汞荧光灯。 为了实现这个目的,本发明的氧化物荧光体包括单个颗粒,每个颗粒在其表面处和附近的区域都被修饰,并且表面区域的元素组成比内部区域的 颗粒。 或者,表面区域在元素组合物中具有更多的卤素或硫族元素。 在本发明的荧光体处理方法中,通过(i)通过激发含有反应性气体的气体形成高反应性气体气氛,并且(ii)将荧光体暴露于气体气氛,来选择性地修饰单个荧光体颗粒的表面区域。
    • 4. 发明申请
    • Light-Emitting Device
    • 发光装置
    • US20080203893A1
    • 2008-08-28
    • US11910832
    • 2006-04-06
    • Masahiro SakaiSeigo ShiraishiTakehiro ZukawaKojiro OkuyamaJunichi HibinoKazuhiko Sugimoto
    • Masahiro SakaiSeigo ShiraishiTakehiro ZukawaKojiro OkuyamaJunichi HibinoKazuhiko Sugimoto
    • H01J1/62H01J17/49
    • C09K11/7734H01J1/63H01J11/12H01J11/42H01J61/44
    • The present invention is a light-emitting device which is provided with a phosphor layer containing a blue phosphor, wherein the phosphor layer includes an aluminate phosphor, as the blue phosphor, that contains Ba, Sr, Eu, Mg, Al and O as constituting elements at an atom-number ratio Ba:Sr:Eu:Mg:Al:O=p:q:r:1:w:17 wherein 0.70≦p≦0.95, 0≦q≦0.15, 0.05≦r≦0.20, p+q+r≧1, and 9.8≦w≦10.5 are satisfied, and a value of a linear coupling function s represented by a formula: s=−11622+2043.07La+199.24L1−116.91L2 is 1 or less, when a lattice constant is La(Å), an interatomic distance between Al(2) and O(5) is L1(Å), and an interatomic distance between Al(1) and O(4) is L2(Å), which are obtained by an X-ray crystal structure analysis assuming that the aluminate phosphor belongs to a space group P63/mmc.
    • 本发明是一种发光装置,其具有含有蓝色荧光体的荧光体层,其中,荧光体层含有作为蓝色荧光体的铝酸盐荧光体,其含有Ba,Sr,Eu,Mg,Al,O作为构成 元素原子数比Ba:Sr:Eu:Mg:Al:O = p:q:r:1:w:17其中0.70 <= p <= 0.95,0 <= q <= 0.15,0.05 < 满足r <= 0.20,p + q + r> = 1和9.8 <= w <= 10.5,并且由公式表示的线性耦合函数s的值:<?in-line-formula description =“In -line公式“end =”lead“?> s = -11622 + 2043.07L 199.24L -116.91L <2> 在线公式描述=“在线公式”end =“tail”?>为1以下,当晶格常数为L(a)时,Al(2)之间的原子间距离 )和O(5)是L 1(A),Al(1)和O(4)之间的原子间距离是L 2(),它们是 通过假设铝酸盐荧光体属于空间群P6 3
    • 8. 发明申请
    • PLASMA DISPLAY PANEL
    • 等离子显示面板
    • US20120326598A1
    • 2012-12-27
    • US13202896
    • 2011-03-15
    • Jun HashimotoTakehiro ZukawaTakuji TsujitaTakayuki Shimamura
    • Jun HashimotoTakehiro ZukawaTakuji TsujitaTakayuki Shimamura
    • H01J17/49
    • H01J11/12H01J11/40
    • PDP (1) includes front plate (2) and rear plate (10). Front plate (2) has protective layer (9). Rear plate (10) has phosphor layers (15). Protective layer (9) includes a first metal oxide and a second metal oxide. In X-ray diffraction analysis, a peak of a base layer lies between a first peak of the first metal oxide and a second peak of the second metal oxide. The first and second metal oxides are two selected from the group consisting of MgO, CaO, SrO, and BaO. The concentration of calcium contained in the base layer ranges from not less than 1 atomic % to not greater than 5 atomic %. In X-ray diffraction analysis, the metal oxide exhibits one peak that lies between the minimum and the maximum of diffraction angles of single substances of the selected metal oxides in a specific plane direction (111).
    • PDP(1)包括前板(2)和后板(10)。 前板(2)具有保护层(9)。 后板(10)具有荧光体层(15)。 保护层(9)包括第一金属氧化物和第二金属氧化物。 在X射线衍射分析中,基层的峰位于第一金属氧化物的第一峰和第二金属氧化物的第二峰之间。 第一和第二金属氧化物选自MgO,CaO,SrO和BaO。 基质层中所含的钙浓度为1原子%以上5原子%以下。 在X射线衍射分析中,金属氧化物表现出一个位于特定平面方向上选择的金属氧化物的单一物质的最小和最大衍射角的峰(111)。