    • Method for making tabular grain silver halide emulsion
    • 制备片状银卤化银乳剂的方法
    • US06673529B1
    • 2004-01-06
    • US10193341
    • 2002-07-11
    • Richard L. DaubendiekJon N. EikenberryBarbara J. FisherTimothy R. GerseyJoseph G. LighthouseDouglas L. Oehlbeck
    • Richard L. DaubendiekJon N. EikenberryBarbara J. FisherTimothy R. GerseyJoseph G. LighthouseDouglas L. Oehlbeck
    • G03C1005
    • G03C1/0051G03C2001/0055G03C2001/0058G03C2001/03511G03C2200/03
    • A process of preparing a high bromide tabular grain emulsion comprising a dispersion medium and silver halide grains including tabular grains having {111} major faces and an aspect ratio of at least 2, which contain greater than 50 mole percent bromide, based on silver, and which account for greater than 50 percent of total grain projected area, where such tabular grains have an average aspect ratio of at least 5, the process comprising (i) in a grain nucleation step creating in a dispersing medium tabular silver halide grain nuclei containing parallel twin planes and (ii) in a grain growth step subsequently growing the tabular grain nuclei into tabular grains in a silver halide reaction vessel by adding a silver ion source and a halide ion source to the reaction vessel and precipitating silver halide onto the tabular grain nuclei, wherein thiocyanate ion is introduced into the silver halide reaction vessel prior to the addition of at least the final 10 mole percent of the total silver added to the reaction vessel, and further wherein the introduced thiocyanate ion concentration is at most 0.4 mole %, based on the total silver added to the reaction vessel. Use of thiocyanate during grain precipitation result in increased aspect ratio without degrading morphological purity.
    • 一种制备高溴化物片状颗粒乳剂的方法,包括分散介质和卤化银颗粒,所述卤化银颗粒包括具有{111}主面和具有至少2的长宽比的片状颗粒,其含有基于银的大于50摩尔百分比的溴化物,以及 其占总颗粒投影面积的大于50%,其中这种片状颗粒具有至少5的平均纵横比,其方法包括(i)在分散介质中产生平均粒度的卤化银颗粒核的晶粒成核步骤 (ii)在晶粒生长步骤中,随后通过向反应容器中加入银离子源和卤离子源并将卤化银沉淀在片状晶粒核上,随后将片状晶粒核生长成卤化银反应容器中的片状颗粒 ,其中硫氰酸根离子在添加至少最终的10摩尔%的总银之前被引入到卤化银反应容器中 加入到反应容器中,进一步其中导入的硫氰酸根离子浓度至多为0.4摩尔%,基于添加到反应容器中的总银。 颗粒沉淀过程中硫氰酸盐的使用导致纵横比增加而不会降低形态纯度。