    • 2. 发明授权
    • 보수성 기층을 갖는 배수성·저소음 합성 도로포장 시공방법
    • 在含水层中排水和吸收吸收的复合材料的方法
    • KR100818489B1
    • 2008-04-01
    • KR1020060128145
    • 2006-12-14
    • 후암산업 주식회사송철영한국토지공사
    • 송철영
    • E01C7/18E01C7/26E01C11/22
    • E01C7/182E01C7/265E01C11/225
    • A construction method for a drainage and low-noise composite road pavement having a water retentive base layer is provided to promote the noise reduction of a pavement with drainage capacity, and to secure environment-friendly effect of a pavement and to improve durability with water holding capacity by forming a composite pavement with a double structure having drainage capacity and water holding capacity on a surface layer and an intermediate layer or a base layer. A construction method for a drainage and low-noise composite road pavement having a water retentive base layer comprises the steps of: manufacturing a porous open-graded asphalt composition for a base layer or an intermediate layer to secure a porosity of 21~30% by using single-graded aggregates having the maximum size of 40mm, 25mm, 19mm or 13mm(1); paving and tamping the porous open-graded asphalt composition(2); manufacturing water retentive cement paste to have the maximum absorption rate of 60~80% and the 7-day compressive strength of 0.5~18N/mm^2 by mixing water retentive materials(3); forming a water retentive pavement layer to have negative stiffness with the 7-day flexural strength of 1.0~3.9N/mm^2 and water retention power with the maximum water holding capacity of 4.0~8.0l/m^2 for a pavement having a thickness of 5cm by filling up gaps in the open-graded asphalt composition with the water retentive cement paste and curing, or, mixing 70~80 weight percent single-graded aggregates having the maximum size and 20~30 weight percent water retentive cement paste at a fixed temperature and paving directly on a pavement surface, and then curing(4); manufacturing a permeable or drainage asphalt composition having a porosity of 15~25% for a surface layer by using single-graded aggregates having the maximum size of 19mm, 13mm, 10mm or 8mm which are smaller than the maximum size of the aggregates used for the water retentive pavement layer and high-durable and high viscosity modified asphalt(5); and forming a drainage pavement layer to have drainage capacity by paving and tamping the permeable or drainage asphalt composition, wherein the water retentive pavement layer is constructed to have a 0.5~1cm-gap which is not filled with cement paste from the surface of the pavement to strength adhesive strength between the drainage pavement layer and the water retentive pavement layer.
    • 提供一种具有保水性基层的排水和低噪声复合路面施工方法,以促进具有排水能力的路面的噪声降低,并且确保路面的环境友好效果并且通过保水来提高耐久性 通过在表面层和中间层或基层上形成具有排水能力和保水能力的双重结构的复合路面的能力。 具有保水性基层的排水低噪声复合路面施工方法包括以下步骤:制造用于基层或中间层的多孔开放式沥青组合物,以确定21〜30%的孔隙率,由 使用最大尺寸为40mm,25mm,19mm或13mm(1)的单分级聚集体; 铺路和夯实多孔开放式沥青组合物(2); 通过混合保水材料(3),制备保水性水泥浆的最大吸收率为60〜80%,7天抗压强度为0.5〜18N / mm ^ 2。 形成保水路面层,具有负强度,7天弯曲强度为1.0〜3.9N / mm ^ 2,保水力最大,保水能力为4.0〜8.0l / m ^ 2,对于具有 通过用保水性水泥浆填充开放式沥青组合物的间隙并固化,或者将具有最大尺寸和20〜30重量%的保水性水泥浆的70〜80重量%的单级聚集体混合在一起,厚度为5cm 固定温度,直接铺在路面上,然后固化(4); 通过使用最大尺寸为19mm,13mm,10mm或8mm的单梯度聚集体制造表面层的孔隙率为15〜25%的可渗透或排水沥青组合物,其小于用于 保水路面层和高耐久性和高粘度改性沥青(5); 并且通过铺路和夯实可渗透或排出的沥青组合物形成排水路面层以具有排水能力,其中保水路面层被构造成具有距离路面表面没有填充水泥浆的0.5-1cm间隙 以强化排水路面层和保水路面层之间的粘合强度。
    • 5. 发明公开
    • 마그네슘계 고화재를 사용한 흙포장 조성물 및 이를 이용한 도로포장방법
    • 土壤覆盖组合物和使用这种方法铺设地基的方法
    • KR1020120119223A
    • 2012-10-31
    • KR1020110033328
    • 2011-04-11
    • 송철영
    • 송철영
    • E01C7/08E01C7/36E01C21/00C04B14/02
    • E01C7/08C04B14/02E01C7/085E01C7/36E01C21/00
    • PURPOSE: A soil paving composition using a magnesium-based solidifying agent and a paving method using the composition are provided to improve the strength and repair efficiency by employing waste refractory aggregate as a part of a soil material. CONSTITUTION: A soil paving composition using a magnesium-based solidifying agent comprises a main material, which includes 29-43 weight% of soil and 53-60 weight% of waste refractory aggregate, and a binding material, which includes 3-10 weight% of a magnesium-based solidifying agent and 0.15-0.5 weight% of a polymer admixture. [Reference numerals] (AA) Magnesia+soil+water; (BB) Reaction with water; (CC) Creation of magnesium hydroxide[Mg(OH)_2]; (DD) Pozzolanic reaction; (EE) Creation of a durable composition; (FF) Reaction with furnace slag, sulfate; (GG) Creation of magnesia ettringite
    • 目的:提供使用镁基固化剂的土壤铺路组合物和使用该组合物的铺路方法,以通过使用废耐火骨料作为土壤材料的一部分来提高强度和修复效率。 构成:使用镁基固化剂的土壤铺路组合物包括主要材料,其包括29-43重量%的土壤和53-60重量%的废弃耐火骨料,以及粘合材料,其包含3-10重量% 的镁基固化剂和0.15-0.5重量%的聚合物混合物。 (附图标记)(AA)氧化镁+土壤+水; (BB)与水反应; (CC)产生氢氧化镁[Mg(OH)_2]; (DD)火山灰反应; (EE)创建耐用的组合物; (FF)与炉渣,硫酸盐反应; (GG)产生氧化镁钙矾石
    • 7. 发明授权
    • 유색골재를 이용한 칼라 아스팔트 도로포장방법.
    • 使用彩色骨料铺路的方法
    • KR100584794B1
    • 2006-05-30
    • KR1020040022665
    • 2004-04-01
    • 안학현송철영
    • 안학현송철영
    • E01C7/08E01C7/35C04B16/04C04B26/26
    • 본 발명은 유색골재를 이용한 칼라 아스팔트 도로포장방법에 관한 것으로, 더욱 상세하게는 도로의 기능에 적합한 아스팔트 혼합물을 제조하여 시공하되, 상기 아스팔트 혼합물 제조시 또는 시공시에 유색골재를 사용하여 아스팔트 도로 포장의 칼라화를 실현하는 것이며, 결합재로서 검은색의 일반 도로포장용 아스팔트 또는 수지계 탈색 바인더 어느 것을 사용 하더라도 유색골재에 의한 다양한 칼라 아스팔트 포장이 가능할 뿐만 아니라, 탈색 등에 의해 칼라 도로의 기능이 상실되지 않도록 하는 것으로, 유색골재가 혼합된 혼합골재 또는 일반 골재 79.0∼95.0중량%, 결합재 4.0∼9.0중량%, 개질재 0.1∼3.0중량% 및 채움재 0.9∼9.0중량%로 되는 아스팔트 혼합물을 준비하는 단계와; 준비된 아스팔트 혼합물을 노면에 포설후 다짐 하거나 또는 아스팔트 혼합물 포설후 표면에 유색골재를 살포하여 다짐하는 단계와; 반강성 포장의 경우 포설 및 다짐된 아스팔트 혼합물의 공극에 시멘트 페이스트를 침투시켜 양생하는 단계와; 포장표면을 연마하는 단계를 포함하여 이루어지는 것을 특징으로 한다.
      유색골재, 아스팔트, 개질재, 시멘트 페이스트, 수지계 탈색 바인더
    • 8. 发明公开
    • 유색골재를 이용한 칼라 아스팔트 도로포장방법.
    • 使用彩色聚合物铺路的方法
    • KR1020050097585A
    • 2005-10-10
    • KR1020040022665
    • 2004-04-01
    • 안학현송철영
    • 안학현송철영
    • E01C7/08E01C7/35C04B16/04C04B26/26
    • E01C7/085C04B16/04C04B26/26E01C7/35
    • 본 발명은 유색골재를 이용한 칼라 아스팔트 도로포장방법에 관한 것으로, 더욱 상세하게는 도로의 기능에 적합한 아스팔트 혼합물을 제조하여 시공하되, 상기 아스팔트 혼합물 제조시 또는 시공시에 유색골재를 사용하여 아스팔트 도로 포장의 칼라화를 실현하는 것이며, 결합재로서 검은색의 일반 도로포장용 아스팔트 또는 수지계 탈색 바인더 어느 것을 사용 하더라도 유색골재에 의한 다양한 칼라 아스팔트 포장이 가능할 뿐만 아니라, 탈색 등에 의해 칼라 도로의 기능이 상실되지 않도록 하는 것으로, 유색골재가 혼합된 혼합골재 또는 일반 골재 79.0∼95.0중량%, 결합재 4.0∼9.0중량%, 개질재 0.1∼3.0중량% 및 채움재 0.9∼9.0중량%로 되는 아스팔트 혼합물을 준비하는 단계와; 준비된 아스팔트 혼합물을 노면에 포설후 다짐 하거나 또는 아스팔트 혼합물 포설후 표면에 유색골재를 살포하여 다짐하는 단계와; 반강성 포장의 경우 포설 및 다짐된 아스팔트 혼합물의 공극에 시멘트 페이스트를 침투시켜 양생하는 단계와; 포장표면을 연마하는 단계를 포함하여 이루어지는 것을 특징으로 한다.
    • 10. 发明授权
    • 탄성 투수 도로의 포장방법
    • 탄성투수도로의포장방법
    • KR100469582B1
    • 2005-02-02
    • KR1020020077753
    • 2002-12-09
    • 안학현송철영
    • 안학현송철영
    • E01C7/26
    • PURPOSE: A pavement method of an elastic permeable road is provided to prevent the lowering of durability or the damage of appearance, to secure the safety on walking or traveling and to improve eco-friendly and economical efficiencies by recycling waste resources. CONSTITUTION: The pavement method of an elastic permeable road comprises the steps of: preparing binder by mixing 50¯85 weight percent cement, 10¯30 weight percent blastfurnace slag and 5¯20 weight percent fine fly ash(S1); manufacturing permeable concrete by mixing 70.0¯91.9 weight percent aggregate, 0.1¯3.0 weight percent powdered waterproof materials and 3.0¯7.0 weight percent water with the mixed 5.0¯20.0 weight percent binder(S2); placing the manufactured permeable concrete on a base layer with the appointed thickness(S3); and placing permeable elastic materials composed of 66¯86 weight percent rubber chips, urethane chips or their admixture, 7¯17 weight percent resinous binder and 7¯17 weight percent silica sands on the constructed permeable concrete layer with the appointed thickness(S4).
    • 目的:提供弹性可渗透道路的铺设方法,以防止耐久性降低或外观损坏,确保行走或旅行的安全,并通过回收废物资源提高环保和经济效益。 组成:弹性可渗透路面的铺设方法包括以下步骤:通过混合50重量%〜85重量%的水泥,10重量%的30重量%高炉炉渣和5重量%的20重量%的细粉煤灰(S1)来制备粘结剂; 通过混合70.0和95.9重量百分比的骨料,0.1和3.0重量百分比的粉状防水材料和3.0重量百分比的7.0重量百分比的水与混合的5.0和20.0重量百分比的粘合剂(S2)制造可渗透混凝土; 将所制造的可渗透混凝土放置在具有指定厚度的基层上(S3); 并将具有66%重量百分比的橡胶碎片,聚氨酯碎片或它们的混合物,7%重量百分比的树脂粘结剂和7%重量百分比的硅砂组成的可渗透弹性材料放置在具有指定厚度(S4)的所构造的可渗透混凝土层上。