    • 1. 发明专利
    • Printing wire
    • 印刷线
    • JPS6164458A
    • 1986-04-02
    • JP18780784
    • 1984-09-07
    • Toshiba CorpToshiba Tungaloy Co Ltd
    • FUJIWARA TETSUOUZAWA SUMIYOSUZUKI ISAOENDO AKIRA
    • C23C16/30B22F7/04B41J2/25C22C29/02C22C29/06
    • B22F7/04B41J2/25C22C29/02C22C29/067
    • PURPOSE:To obtain a light wt. printing wire having excellent abrasion resistance and high toughness, by providing an alloy layer based on nickel or cobalt to the surface of a wire main body based on a hard alloy powder containing titanium carbide. CONSTITUTION:A printing wire has a wire main body, which comprises a hard sintered alloy based on a hard alloy powder containing titanium carbide and containing at least one component selected from nickel and cobalt as a bonding phase, and an alloy layer, which is formed on the surface of the wire main body and based on nickel to which nickel phosphide or nickel boride was precipitated. or an alloy layer based on cobalt to which cobalt phosphide or cobalt boride was precipitated. The hard alloy powder containing titanium carbide contributes to the enhancement of the hardness and abrasion resistance of the printing wire. The bonding layer comprising at least one component selected from nickel and cobalt brings trouble to the wettability with the hard alloy powder or the particle growth of said alloy powder and contributes to a sintering property. The alloy layer, which is formed to the surface of the wire main body, comprising the hard sintered alloy imparts high toughness without bringing about the lowering in hardness.
    • 目的:获得重量轻 基于含有碳化钛的硬质合金粉末,通过向线主体的表面提供基于镍或钴的合金层,具有优异的耐磨性和高韧性的印刷线。 构成:印刷线具有线主体,其包括基于含有碳化钛并含有至少一种选自镍和钴的成分作为结合相的硬质合金粉末的硬质烧结合金和形成的合金层 在导线主体的表面上并且基于沉积有磷化镍或硼化镍的镍。 或基于钴的合金层沉积钴磷化钴或钴硼化物。 含有碳化钛的硬质合金粉末有助于提高印刷线的硬度和耐磨性。 包含至少一种选自镍和钴的组分的粘合层会使硬质合金粉末的润湿性或所述合金粉末的颗粒生长带来麻烦,并且有助于烧结性能。 形成在线主体表面的合金层包括硬质烧结合金,赋予高韧性,而不会降低硬度。
    • 3. 发明专利
    • DATA RECORDING MEDIUM
    • JPH0449089A
    • 1992-02-18
    • JP15765590
    • 1990-06-18
    • TOSHIBA CORP
    • TADA KAORUFUJIWARA TETSUOARAI SHINJI
    • B41M5/26G11B7/24G11B7/243
    • PURPOSE:To obtain a data recording medium enhanced in the S/N ratio of reproduction, subjected to high speed recording erasure, susceptible to high density data recording, having long life and capable of being prepared by a simple manufacturing process by providing a recording layer formed from a crystalline alloy changing in phase between an alpha-phase and sigma-phase. CONSTITUTION:A medium has a substrate 1 and the recording layer 2 provided thereon and, for example, the substrate 1 is constituted of glass or an org. resin. The recording layer 2 constituted of a material changing in phase between an alpha-phase and sigma-phase. As an alloy capable of generating this phase change, there is a crystalline alloy containing at least one element selected from Cr, Mn, V, Ni, Si and Cu and substantially composed of the reminder of Fe. This alloy is inexpensive and an inexpensive data recording medium can be obtained by using said alloy as the recording layer.
    • 9. 发明专利
    • Production of shape memory alloy element
    • 形状记忆合金元素的生产
    • JPS61127892A
    • 1986-06-16
    • JP24861884
    • 1984-11-27
    • Toshiba Corp
    • YAMAMOTO MASAOFUJIWARA TETSUO
    • C25D7/00H01H37/32
    • H01H37/323
    • PURPOSE:To prolong the endurance life by putting an electrically conductive metallic layer on the surface of a shape memory alloy substrate and joining them together at a specified temp. so as to increase the adhesion of the metallic layer to the substrate. CONSTITUTION:A layer of an electrically conductive metal such as Cu or Ni is put on pat of the surface of a substrate of a shape memory alloy such as NiTi at one or more positions. The thickness of the metallic layer is =400 deg.C in vacuum or in an inert or reducing gas to obtain a shape memory alloy element. The electrically conductive layer is not stripped by repeated shape restoring action, and the element maintains its stable characteristics for a long time.
    • 目的:通过将导电金属层放置在形状记忆合金基板的表面上并在指定温度下将它们连接在一起来延长寿命。 以增加金属层对基材的粘附性。 构成:在一个或多个位置上,诸如NiTi等形状记忆合金的基板表面放置一层诸如Cu或Ni的导电金属。 金属层的厚度是基板的最小厚度的约5%。 它们在真空中或在惰性或还原性气体中在> = 400℃下连接在一起,以获得形状记忆合金元素。 通过重复的形状恢复动作,不会剥离导电层,并且该元件长时间保持其稳定的特性。
    • 10. 发明专利
    • Color picture tube
    • 彩色图像管
    • JPS6142838A
    • 1986-03-01
    • JP16441184
    • 1984-08-06
    • Toshiba Corp
    • INABA MICHIHIKOFUJIWARA TETSUOKANTO MASAHARUOTAKE YASUHISA
    • C22C19/03C22C38/00C22C38/04C22C38/08C23C8/10H01J9/14H01J29/02H01J29/07
    • H01J29/07H01J2229/0733H01J2229/0783
    • PURPOSE:To increase the quality of images by using a material prepared by adding Mn to an Fe-Ni alloy to form the shadow mask, the frame and the inner shield and specifying the thermal expansion coefficient and the 0.2% proof stress of the material. CONSTITUTION:A material composed of Fe, 25-50wt% Ni and 0.8-10wt% Mn is used to form a shadow mask 6, a supporting frame 7 and an inner shield 9 interrupting the influence of earth magnetism, which are installed near the fluorescent screen 5 of a color picture tube. The thermal expansion coefficient of the material is adjusted to 20-80X10 and its 0.2% proof stress is adjusted to be at least 22kg/mm. . Besides, the surface of the material consists of a black oxide film with a spinel structure represented by the formula NixMnYFe3-X-Y. Accordingly, improved image quality can be realized by preventing color shift or similar phenomenon by inhibiting thermal strain. Furthermore, improved manufacture yield can be achieved by facilitating press formation performed at room temperature.
    • 目的:通过使用通过在Fe-Ni合金中添加Mn形成阴影掩模,框架和内部屏蔽并指定材料的热膨胀系数和0.2%屈服应力的材料来提高图像质量。 构成:由Fe,25-50wt%Ni和0.8-10wt%Mn组成的材料用于形成荫罩6,支撑框架7和中断地球磁力影响的内屏蔽9,它们安装在荧光灯附近 屏幕5的彩色显像管。 材料的热膨胀系数调整为20-80×10 -7,其0.2%的弹性应力调整至少为22kg / mm 2。 此外,材料的表面由具有由式NixMnYFe3-X-Y表示的尖晶石结构的黑色氧化物膜组成。 因此,可以通过抑制热应变来防止色移或类似现象来实现改进的图像质量。 此外,通过促进在室温下进行的压制成型,可以提高制造产率。