会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明专利
    • METHOD AND APPARATUS FOR PRODUCING Ti BY Ca REDUCTION
    • 通过Ca还原生产Ti的方法和装置
    • JP2006124813A
    • 2006-05-18
    • JP2004317842
    • 2004-11-01
    • Sumitomo Titanium CorpToho Titanium Co Ltd住友チタニウム株式会社東邦チタニウム株式会社
    • HORI MASAHIKOOGASAWARA TADASHIYAMAGUCHI MAKOTOUENISHI TORUYAMAGUCHI MASANORIONO YUICHIKOSEMURA SUSUMUNISHIMURA EIJI
    • C25C3/28C22B5/04C22B34/12
    • C25C3/02C22B34/1268C22B34/1272C22B34/129C25C3/28C25C7/007
    • PROBLEM TO BE SOLVED: To provide a method and an apparatus for cost effectively produce high-purity metal Ti with high efficiency without using a costly reducing agent. SOLUTION: The method for producing the Ti includes a Ti generation process of holding a molten salt 3a which contains CaCl 2 and in which Ca is dissolved within a reaction chamber 1, and supplying TiCl 4 to generate the Ti, an electrolysis process of holding the molten salt 3b containing CaCl 2 within an electrolytic cell 2, and generating the Ca on a cathode side by electrolysis, and a Ca transport process of depositing and sticking the generated Ca in the electrolytic cell on a continuum 5 constituted movably in the state of immersing a part thereof into the molten salt within the reaction chamber and the electrolytic cell, transporting the same into the reaction chamber, and dissolving the same to the molten salt, wherein the generated Ti is extracted outside the reaction chamber together with the molten salt and after the Ti is separated, the molten salt is transported into the electrolytic cell, and thereby the continuous production of the Ti is made possible. The method can be suitably implemented by the apparatus. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种在不使用昂贵的还原剂的情况下高效地生产高纯度金属Ti的方法和装置。 解决方案:制备Ti的方法包括:将产生CaCl 2的熔融盐3a保持在反应室1中并将Ca溶解在反应室1内并提供TiCl 4 以产生Ti,在电解槽2内保持含有CaCl 2的熔融盐3b的电解过程,并且通过电解在阴极侧产生Ca,并且将Ca 将生成的Ca在电解槽中沉积并粘附在连续体5上的运送过程,该连续体5以将其一部分浸入反应室和电解槽内的熔融盐中并将其输送到反应室中并溶解 与熔融盐相同,其中所产生的Ti与熔融盐一起被抽出到反应室外部,并且在Ti分离之后,熔融盐被输送到电解槽中,从而可以连续生产Ti 乐。 该方法可以通过该装置适当地实现。 版权所有(C)2006,JPO&NCIPI
    • 3. 发明专利
    • Method and device for producing metallic titanium
    • 用于生产金属钛的方法和装置
    • JP2005194554A
    • 2005-07-21
    • JP2004000449
    • 2004-01-05
    • Foundation For The Promotion Of Industrial ScienceToho Titanium Co Ltd東邦チタニウム株式会社財団法人生産技術研究奨励会
    • OKABE TORUONO YUICHI
    • C22B34/12C22B5/04C22B9/10C25C3/28
    • PROBLEM TO BE SOLVED: To provide a method for producing metallic titanium capable of inexpensively producing metallic titanium of high purity with satisfactory current efficiency and production efficiency, and further capable of corresponding to the serialization of production steps.
      SOLUTION: A molded body or a sintered compact obtained by adding a reaction assistant to titanium oxide is reduced by electrons released at the time when active metal is dissolved in molten salt, thus metallic titanium can be rapidly and uniformly reduced to the inside of the molded body. Further, since the active metal is held to a limited region in a part of a molten salt bath, the contact of the produced metal titanium with the active metal in which impurities are concentrated does not occur. In this way, the metallic titanium of high purity can be produced.
      COPYRIGHT: (C)2005,JPO&NCIPI
    • 解决的问题:提供一种能够以良好的电效率和生产效率廉价地制造高纯度的金属钛的金属钛的制造方法,并且还能够对应于生产步骤的序列化。 解决方案:通过在氧化钛中加入反应助剂获得的成型体或烧结体在活性金属溶解在熔融盐中时释放的电子减少,金属钛可以迅速均匀地还原到内部 的成型体。 此外,由于在熔融盐浴的一部分中将活性金属保持在有限的区域,所以不会发生生成的金属钛与杂质浓缩的活性金属的接触。 以这种方式,可以生产高纯度的金属钛。 版权所有(C)2005,JPO&NCIPI
    • 8. 发明专利
    • Method and apparatus for producing metal calcium
    • 用于生产金属钙的方法和装置
    • JP2009287045A
    • 2009-12-10
    • JP2008137794
    • 2008-05-27
    • Toho Titanium Co Ltd東邦チタニウム株式会社
    • YAMAGUCHI MASANORIONO YUICHIYAMANAKA OSAMU
    • C25C3/02C25C7/04C25C7/08
    • PROBLEM TO BE SOLVED: To provide a method and apparatus for efficiently producing high purity metal calcium by a molten salt electrolysis. SOLUTION: The method of producing metal calcium by filling molten calcium chloride into an electrolytic cell as an electrolytic bath and imparting voltage to an anode and a cathode which are immersed and arranged in the electrolytic cell to carry out the molten salt electrolysis includes a step of: keeping the electrolytic bath of a part including the cathode in the electrolytic bath to a temperature equal to or above the melting point of the metal calcium to form the molten metal calcium (thereafter called "electrolytic step"); and a step of: cooling the electrolytic bath of the part including the cathode to a temperature equal to or below the melting point of metal calcium to deposit metal calcium (thereafter called "cooling step") and is provided with the electrolytic cell where the electrolytic bath is filled and the anode and the cathode which are immersed and arranged in the electrolytic bath, wherein the cathode and the anode are respectively arranged inside of a cathode partition wall and an anode partition wall respectively surrounding the cathode and the anode. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种通过熔融盐电解有效生产高纯度金属钙的方法和装置。 解决方案:通过将熔融氯化钙填充到电解槽中并将其施加于电解池中并进行熔融盐电解的阳极和阴极赋予电压来产生金属钙的方法包括: 将包含阴极的部分的电解浴保持在电解浴中的步骤为等于或高于金属钙的熔点的温度,形成熔融金属钙(此后称为“电解步骤”); 以及将包含阴极的部分的电解槽冷却至等于或低于金属钙的熔点以沉积金属钙的温度(此后称为“冷却步骤”)的步骤,并且设置有电解槽,其中电解 将阴极和阳极分别设置在分别围绕阴极和阳极的阴极分隔壁和阳极分隔壁的内部,阴极和阴极被浸没并排列在电解槽中。 版权所有(C)2010,JPO&INPIT
    • 9. 发明专利
    • Method of producing metal calcium and molten salt electrolytic apparatus
    • 生产金属钙和钼酸盐电解质设备的方法
    • JP2009144176A
    • 2009-07-02
    • JP2007319325
    • 2007-12-11
    • Toho Titanium Co Ltd東邦チタニウム株式会社
    • YAMAGUCHI MASANORIONO YUICHIYAMANAKA OSAMU
    • C25C3/02C25C7/00C25C7/04
    • PROBLEM TO BE SOLVED: To provide a method and an apparatus for efficiently producing metal calcium by a molten salt electrolysis.
      SOLUTION: In the method of producing metal calcium by filling calcium chloride molten salt in an electrolytic bath and arranging so as to dip an anode and a cathode to carry out the molten salt electrolysis, metal calcium is deposited on the cathode in a solid state by cooling the cathode to a temperature equal to or below the melting point of the metal calcium in the molten salt electrolysis and after molten salt electrolysis, the deposited solid metal calcium is recovered by heating to be melted. The molten salt electrolytic apparatus is used for the manufacturing method and is composed of an electrolytic bath, the cathode, the anode and a partition wall dipped and arranged between the cathode and the anode and the cathode has a flow passage formed to pass a heating medium or a cooling medium to heat or cool the cathode itself.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种通过熔盐电解有效地生产金属钙的方法和装置。 解决方案:在通过在电解槽中填充氯化钙熔盐并排列以使阳极和阴极浸入以进行熔融盐电解的方法制备金属钙的方法中,金属钙沉积在阴极上 通过在熔盐电解中将阴极冷却至等于或低于金属钙的熔点的温度,并且在熔融盐电解之后,通过加热回收沉积的固体金属钙以使其熔融。 熔盐电解设备用于制造方法,并且由电解浴,阴极,阳极和浸渍并布置在阴极和阳极之间的分隔壁组成,阴极具有形成为使热介质通过的流路 或用于加热或冷却阴极本身的冷却介质。 版权所有(C)2009,JPO&INPIT