    • Alumina sintered body and process for producing the same
    • Aluminiumoxidsinterkörper和Verfahren zu seiner Herstellung
    • EP0976697A1
    • 2000-02-02
    • EP99114634.1
    • 1999-07-26
    • Sumitomo Chemical Company, Limited
    • Watanabe, HisashiUchida, Yoshio
    • C04B35/111A61L27/00H01L21/68
    • A61L27/105C04B35/111H01L21/6838
    • A process for producing a polycrystalline alumina sintered body which comprises the steps of:

      subjecting alumina powder to ultrasonic irradiation, mechanical stirring not using a grinding medium, or ultrasonic irradiation and mechanical stirring not using a grinding medium, resulting in slurry dispersed in a solvent;
      drying and forming said slurry to produce a green body; and then
      sintering said green body in an air atmosphere at a temperature in the range of 1400 °C to 1800 °C;
      wherein said alumina powder having a purity of 99.99 wt% or more comprises a polyhedral particle having substantially no fractured surface, and comprises α alumina particles having polyhedral shape; a D/H ratio of from 0.5 or more to 3.0 or less; the number-average particle size of from 0.1 µ m or more to 1.0 µm or less; a D90/D10 ratio of 7 or less.
    • 一种多晶氧化铝烧结体的制造方法,其特征在于,包括以下步骤:使氧化铝粉末进行超声波照射,不使用研磨介质的机械搅拌,或者不使用研磨介质的超声波照射和机械搅拌,使浆料分散在溶剂中; 干燥和形成所述浆料以产生生坯; 然后在空气气氛中在1400〜1800℃的温度范围内烧结生坯; 其中纯度为99.99重量%以上的所述氧化铝粉末包含基本上没有断裂表面的多面体颗粒,并且包含具有多面体形状的α氧化铝颗粒; 0.5以上3.0以下的D / H比; 数均粒径为0.1μm以上至1.0μm以下; D90 / D10的比例为7以下。