    • 3. 发明申请
    • RESIN COMPOSITION AND MOLDED ARTICLE
    • 树脂组合物和成型品
    • US20100324220A1
    • 2010-12-23
    • US12866164
    • 2009-02-03
    • Kiyotsuna ToyoharaJitsuo Oda
    • Kiyotsuna ToyoharaJitsuo Oda
    • C08L77/00C08L33/04
    • C08L67/02C08K3/34C08K5/0083C08K5/29C08L51/04C08L51/085C08L67/04C08L77/06C08L77/12C08L2666/18C08L2666/02
    • A resin composition comprising an aromatic polyester having a butylene terephthalate skeleton as the main constituent unit (component A), polylactic acid comprising poly(L-lactic acid) and poly(D-lactic acid) (component B), and a modifier (component C), wherein the resin composition has (i) a crystal melting peak of stereocomplex-phase polylactic acid at 190° C. or higher in differential scanning calorimeter measurement, (ii) a biomass ratio of not less than 50%, (iii) a notched Izod impact strength of 4 to 15 kJ/m2 and (iv) a flexural modulus of 2.5 to 6 GPa. The resin composition provides a molded article having excellent impact resistance and stiffness. The resin composition has a biomass ratio of not less than 50%. The resin composition has a low moisture absorptivity, hydrolysis resistance and high-speed moldability. The resin composition provides a molded article having excellent heat resistance.
    • 一种树脂组合物,其含有以对苯二甲酸丁二醇酯骨架为主要构成单元的芳香族聚酯(A成分),由聚(L-乳酸)和聚(D-乳酸)(B成分)构成的聚乳酸,和改性剂 C),其中所述树脂组合物具有(i)立体络合相聚乳酸在差示扫描量热计测量中在190℃以上的结晶熔融峰,(ii)生物质比不小于50%,(iii) 缺口伊佐德冲击强度为4〜15kJ / m 2,(iv)弯曲弹性模量为2.5〜6GPa。 树脂组合物提供具有优异的耐冲击性和刚度的模塑制品。 树脂组合物的生物质比不小于50%。 该树脂组合物具有低吸湿性,耐水解性和高速成型性。 树脂组合物提供耐热性优异的成型品。
    • 5. 发明申请
    • AROMATIC POLYCARBONATE RESIN COMPOSITION
    • 芳香聚碳酸酯树脂组合物
    • US20100222486A1
    • 2010-09-02
    • US12734196
    • 2008-10-15
    • Yuichi MatsunoFumitaka KondoKiyotsuna Toyohara
    • Yuichi MatsunoFumitaka KondoKiyotsuna Toyohara
    • C08K3/34C08L69/00
    • C08L67/04C08K3/34C08K5/29C08K5/521C08L69/00
    • The object of this invention is to provide a resin composition that contains a polymer obtained from biomass resources and constitutes molded articles excellent in heat resistance, mechanical properties and durable stability, this invention including a resin composition comprising (i) a resin component containing 95 to 5% by weight of an aromatic polycarbonate (component A) and 5 to 95% by weight of polylactic acid (component B), (ii) 0.001 to 10 parts by weight, per 100 parts by weight of the resin component, of a phosphoric ester metal salt (component C), and (iii) 0.01 to 5 parts by weight, per 100 parts by weight of the polylactic acid (component B), of a terminal blocker (component F), the stereo-complex crystal content (X) of the following expression (I) being 80% or more, X (%)={ΔHb/(ΔHa+ΔHb)}×100  (I) wherein ΔHa and ΔHb are a melting enthalpy (ΔHa) of a crystal melting point that appears at lower than 190° C. and a melting enthalpy (ΔHb) of a crystal melting point that appears at 190° C. or higher but less than 250° C., respectively, in a temperature-elevation process by a differential scanning calorimeter (DSC), and molded articles thereof.
    • 本发明的目的是提供一种含有由生物质资源获得的聚合物的树脂组合物,并且构成耐热性,机械性能和耐久稳定性优异的成型体,本发明包括树脂组合物,其包含(i)含有95〜 5重量%的芳族聚碳酸酯(组分A)和5至95重量%的聚乳酸(组分B),(ii)每100重量份树脂组分0.001至10重量份的磷酸 酯组分C)和(iii)每100重量份聚乳酸(组分B),末端阻断剂(组分F),立体络合物结晶含量(X)为0.01〜5重量份 (I)为80%以上,X(%)= {&Dgr; Hb /(&Dgr; Ha +&Dgr; Hb)}×100(I)其中&Dgr; Ha和&Dgr; Hb为熔融 焓(&Dgr; Ha)的晶体熔点低于190℃,熔融焓(&Dgr; Hb)为 通过差示扫描量热计(DSC)在升温过程中分别出现在190℃以上但小于250℃的晶体熔点,以及其成型体。
    • 9. 发明申请
    • FLAME RETARDANT RESIN COMPOSITION AND MOLDED ARTICLE THEREOF
    • 阻燃树脂组合物及其制品
    • US20110092623A1
    • 2011-04-21
    • US12994791
    • 2009-05-26
    • Katsuhiro YamanakaFumitaka KondoKiyotsuna Toyohara
    • Katsuhiro YamanakaFumitaka KondoKiyotsuna Toyohara
    • C08K5/5357
    • C08K5/5357C07F9/657181C08L67/04
    • A flame retardant resin composition which has high flame retardancy and excellent physical properties and comprises a resin obtained from a plant-derived raw material and a molded article thereof.The flame retardant resin composition comprises: (A) 100 parts by weight of a resin component (component A) which contains at least 50 wt % of a resin (component A-1) obtained from a plant-derived raw material; and (B) 1 to 100 parts by weight of an organic phosphorus compound (component B) represented by the following formula (1). (in the above formula, X1 and X2 are the same or different and each an aromatic substituted alkyl group represented by the following formula (2): ALAr)n  (2) in the above formula, AL is a branched or linear aliphatic hydrocarbon group having 1 to 5 carbon atoms, Ar is a phenyl group which may have a substituent, naphthyl group which may have a substituent or anthryl group which may have a substituent, n is an integer of 1 to 3, and Ar may be bonded to any carbon atom contained in AL.)
    • 阻燃性树脂组合物,其具有高阻燃性和优异的物理性质,并且含有由植物来源的原料得到的树脂及其成型体。 阻燃树脂组合物包含:(A)100重量份含有至少50重量%由植物来源的原料得到的树脂(A-1成分)的树脂成分(A成分) 和(B)1〜100重量份由下式(1)表示的有机磷化合物(B成分)。 (在上式中,X1和X2相同或不同,并且每个由下式(2)表示的芳族取代的烷基:上式中的n(2)中,AL是支链或 具有1至5个碳原子的直链脂族烃基,Ar是可以具有取代基的苯基,可以具有取代基的萘基或可以具有取代基的蒽基,n是1〜3的整数,Ar可以 结合到AL中包含的任何碳原子上。)
    • 10. 发明申请
    • POLYLACTIC ACID COMPOSITION
    • 聚氨酯组合物
    • US20100120991A1
    • 2010-05-13
    • US12593257
    • 2008-03-31
    • Kiyotsuna ToyoharaRyuji NonokawaKohei EndoShin To
    • Kiyotsuna ToyoharaRyuji NonokawaKohei EndoShin To
    • C08G63/06
    • C08G63/08B29K2995/006C08L67/04C08L2666/18
    • It is an object of the present invention to provide a composition comprising polylactic acid and having improved injection moldability and an injection molded product thereof.The object of the present invention is attained by a specific polylactic acid composition which meets the following requirements (a) to (g) at the same time: (a) it must have a weight average molecular weight of 70,000 to 700,000; (b) the total content of Sn atom, Ti atom, Al atom and Ca atom must be 3 to 20 ppm; (c) it must contain a P atom in an amount of 3 to 3,000 ppm; (d) the (total number of gram-atoms of Sn, Ti, Al and Ca)/(number of gram-atoms of P) value must be 0.01 to 5; (e) the content of a compound having a molecular weight of 150 or less must be not more than 0.2 wt %; (f) the COOH terminal group concentration must be not more than 30 equivalents/ton; and (g) the melt viscosity (P) at a melting temperature of 230° C. must satisfy the following expression (1): 10 Pa·s
    • 本发明的目的是提供一种包含聚乳酸并具有改进的注射成型性的组合物及其注模产品。 本发明的目的是通过同时满足以下要求(a)至(g)的特定聚乳酸组合物实现的:(a)其重均分子量必须为70,000至700,000; (b)Sn原子,Ti原子,Al原子和Ca原子的总含量必须为3〜20ppm, (c)必须含有3〜3000ppm的P原子; (d)(Sn,Ti,Al和Ca的克原子数)/(P的克原子数)值必须为0.01〜5; (e)分子量为150以下的化合物的含量必须为0.2重量%以下。 (f)COOH端基浓度必须不超过30当量/吨; 和(g)熔融温度为230℃时的熔融粘度(P)必须满足下式(1):10Pa·s