    • 9. 发明授权
    • Method for making punches using multi-layer ceramic technology
    • 使用多层陶瓷技术制作冲孔的方法
    • US06352014B1
    • 2002-03-05
    • US09464510
    • 1999-12-15
    • David B. GolandDavid C. LongJohn U. KnickerbockerSubhash L. Shinde
    • David B. GolandDavid C. LongJohn U. KnickerbockerSubhash L. Shinde
    • B26F114
    • B26F1/14B23P15/24B26F2210/08H05K1/0306H05K3/005Y10T83/9423
    • A method for making small punches by employing multi-layer ceramic (MLC) technology includes the steps of preparing a sublaminate matrix of a high or low sintering temperature material, drilling holes in the sublaminate using a mask as a guide, filling the holes with punch material paste by a solupor process, laminating the sublaminate to a base plate or as a freestanding substrate, firing a laminate at an appropriate sintering temperature and removing the matrix material by a chemical or mechanical method. In accordance with the present invention, a large number of small punches are made in parallel to precise dimensions of two to ten mils in diameter and approximately 100 mils in length. This method allows that a punch plate array can also be used to simultaneously punch an array of vias in a greensheet and eliminates the additional step of loading individual punches into a punch plate, offering cost and time savings.
    • 通过采用多层陶瓷(MLC)技术制造小冲孔的方法包括以下步骤:制备高或低烧结温度材料的层压基质,使用掩模作为导向孔在该层压板上钻孔,用冲孔 通过溶剂法处理材料糊料,将层压材料层压到基板或独立的基材上,在适当的烧结温度下焙烧层压材料,并通过化学或机械方法除去基体材料。 根据本发明,大量的小冲头与直径为2至10密耳,长度为大约100密耳的精确尺寸并联制成。 该方法允许冲压板阵列也可以用于同时冲切毛坯中的通孔阵列,并且消除了将单个冲头加载到冲压板中的额外步骤,从而节约了成本和时间。