    • 5. 发明申请
    • METHOD FOR FORMING ORGANIC THIN FILM
    • 形成有机薄膜的方法
    • US20090281238A1
    • 2009-11-12
    • US12312096
    • 2007-11-13
    • Tomoya HidakaYoshitaka FujitaNorifumi NakamotoKazuhisa KumazawaEiji Hoshi
    • Tomoya HidakaYoshitaka FujitaNorifumi NakamotoKazuhisa KumazawaEiji Hoshi
    • C09D5/00
    • C09D7/1233B05D1/185B05D7/24B05D2202/00B05D2203/35C03C17/30C03C2217/76C03C2218/113C08K5/01C08K5/04C08K5/05C08K5/5419C09D7/63C09K3/18
    • The object is to provide a method for forming an organic thin film which enables to form quickly a dense monomolecular film with less impurity. It is a method for forming an organic thin film which comprises:1) a step of preparing a hydroxyl group-containing solution by mixing the following (a), (b) and (c) so that the total amount of (A) and (B) in the hydroxyl group-containing solution becomes 0.1 wt % to 80 wt %, and conducting hydrolysis to generate a hydroxyl group-containing compound; a) an adjuvant for forming an organic thin film comprising a metal surfactant (A) having at least one or more hydrolysable group, and a compound (C) that can interact with the metal surfactant in an organic solvent b) a metal surfactant having at least one or more hydrolysable group (B), and c) water 2) a step of preparing a solution for forming an organic thin film by mixing an organic solvent and the hydroxyl group-containing solution obtained in the above step 1); and 3) a step of allowing the substrate to contact with the solution for forming an organic thin film obtained in the above step 2).
    • 本发明的目的是提供一种形成有机薄膜的方法,其能够快速形成具有较少杂质的致密单分子膜。 形成有机薄膜的方法包括:1)通过混合以下(a),(b)和(c)制备含羟基溶液的步骤,使得(A)和 含羟基溶液中的(B)成为0.1重量%〜80重量%,进行水解生成含羟基化合物; a)用于形成包含具有至少一个或多个可水解基团的金属表面活性剂(A)的有机薄膜的助剂和可在有机溶剂中与金​​属表面活性剂相互作用的化合物(C)b)具有 至少一个或多个可水解基团(B)和c)水2)通过混合有机溶剂和在上述步骤1)中获得的含羟基溶液来制备用于形成有机薄膜的溶液的步骤; 和3)允许基板与用于形成上述步骤2)中获得的有机薄膜的溶液接触的步骤。
    • 7. 发明授权
    • Lead-acid battery
    • 铅酸蓄电池
    • US07083876B2
    • 2006-08-01
    • US10096505
    • 2002-03-13
    • Kyoko HonboEiji HoshiYasushi MuranakaSeiji Takeuchi
    • Kyoko HonboEiji HoshiYasushi MuranakaSeiji Takeuchi
    • H01M4/02H01M4/88
    • H01M10/06H01M4/14H01M4/21H01M4/624H01M4/625H01M4/626H01M4/627H01M2004/027Y02E60/126Y02P70/54Y02T10/7016
    • A lead-acid battery superior in high-efficiency charging characteristic to conventional lead-acid batteries and a carbon material used in the lead-acid battery having excellent charge acceptability are disclosed. The lead-acid battery uses, as an additive to the anode active material, a simple substance and/or compound thereof, both having a catalysis for desulfurization or a catalyst for SOx oxidation by adding to, or loading on, a carbon material such as active carbon, carbon black, or the like. When the lead-acid battery with an anode containing carbon material is applied to electric cars, various hybrid cars, power storage systems, elevators, electromotive tools and power source systems such as uninterruptible power source, distributed power source and the like, all having high input and output requirements, stable control can be obtained.
    • 公开了一种铅酸蓄电池,该蓄电池具有优异的高效率充电特性,并且具有优异的充电可接受性,并且在铅酸蓄电池中使用的碳材料。 作为负极活性物质的添加剂,铅酸蓄电池使用具有脱硫催化作用的单体和/或其化合物,或者通过添加或/或 负载在碳材料如活性炭,炭黑等上。 当将具有碳材料的阳极的铅酸电池应用于电动汽车时,各种混合动力汽车,蓄电系统,电梯,电动工具以及诸如不间断电源,分布式电源等的电源系统都具有高 输入输出要求可以得到稳定的控制。