    • Positive electrode for lithium battery and lithium battery
    • 锂电池和锂电池正极
    • US06221529B1
    • 2001-04-24
    • US08972485
    • 1997-11-18
    • Hideo Yasuda
    • Hideo Yasuda
    • H01M452
    • H01M10/052H01M4/131H01M4/525H01M10/0525
    • A positive electrode for a lithium battery wherein nickel oxyhydroxide is held in an electro-conductive three-dimensional porous material or a sintered nickel substrate and a lithium battery using it. When the three-dimensional porous material is used, the electric contact of the active material and the current collector is good, also the contact state of nickel oxyhydroxide particles, which are active materials, each other is good, further, the contact resistance among the particles is low, and also the diffusion of the lithium ion, which is the rate-determining step of the reaction, becomes easy among the particles. Furthermore, in a positive electrode for a lithium battery wherein lithium is intercalated into nickel oxyhydroxide by discharging and lithium is disintercalated from nickel oxyhydroxide by charging, the positive electrode contains at least one kind selected from the group of cobalt oxyhydroxide, metallic cobalt, cobalt oxide, tricobalt tetroxide, lithium cobaltate, and proton-containing cobalt dioxide.
    • 一种用于锂电池的正极,其中将氢氧化正镍保持在导电三维多孔材料或烧结镍基底和使用它的锂电池中。 当使用三维多孔材料时,活性物质和集电体的电接触性良好,作为活性物质的氢氧化镍粒子的接触状态也良好,此外, 颗粒低,并且作为反应的速率决定步骤的锂离子的扩散在颗粒中变得容易。 此外,在通过放电将锂插入氢氧化正镍并通过充电从镍氢氧化镍中脱去锂的锂电池用正极中,正极含有选自羟基氧化钴,金属钴,氧化钴 ,四氧化四钴,钴酸锂和含质子的二氧化钴。
    • 18. 发明授权
    • Nickel electrode for akaline storage cell and manufacturing method of the same
    • 用于碱性蓄电池的镍电极及其制造方法
    • US06171728B2
    • 2001-01-09
    • US09110861
    • 1998-07-07
    • Yoshitaka BabaMotoo TadokoroTakayuki Yano
    • Yoshitaka BabaMotoo TadokoroTakayuki Yano
    • H01M452
    • H01M4/52H01M4/32Y10T29/49115
    • A nickel electrode for an alkaline storage cell manufactured by the steps of precipitating cobalt hydroxide on the surface of a first nickel active material essentially composed of nickel hydroxide, subjecting the first nickel active material to heat treatment under the presence of an alkaline solution and oxygen to that the cobalt hydroxide precipitated on the first nickel active material is disordered to its crystal structure and is formed in a higher order cobalt compound containing alkaline cation, and mixing the first nickel active material subjected to the alkali heat treatment with a second nickel hydroxide active material essentially composed of nickel hydroxide without forming any conductive substance of lower in dissolubility to the alkaline solution.
    • 一种碱性蓄电池用镍电极,其特征在于,在基本上由氢氧化镍构成的第一镍活性物质的表面析出氢氧化钴,在碱溶液和氧气的存在下进行第一镍活性物质的热处理, 沉淀在第一镍活性材料上的氢氧化钴无定形为其晶体结构,并且形成为含有碱性阳离子的较高级的钴化合物,并将进行碱热处理的第一镍活性材料与第二氢氧化镍活性物质 基本上由氢氧化镍组成,而不形成对碱性溶液具有较低溶解度的任何导电物质。