    • BAINITICALLY HARDENED BRAKE DISK
    • 贝氏体固化后制动
    • WO9928641A2
    • 1999-06-10
    • PCT/DE9803507
    • 1998-11-26
    • ACTECH GMBH ADV CASTING TECHWENDT FLORIAN
    • WENDT FLORIAN
    • B22D19/16B23P13/00B23P15/18B60B27/00B60T1/06C21D1/20C21D5/02F16D20060101F16D65/00F16D65/12F16D
    • F16D65/12
    • The invention relates to a bainitically hardened brake disk comprising at least one ring-shaped cast disk (1) body with radially extending ring sections in contact with brake shoes (2). Said brake disk is mounted on the hub of a bicycle wheel (5) for braking purposes. In order to avoid noise emissions and vibrations, the inventive disk is made of cast iron, is highly tough and has a low weight. The aim is to avoid the disadvantages of combining disk brakes with an aluminium wheel hub. The inventive disk is characterised in that it has a thoroughly bainitically hardened body (1) made of cast iron with lamellar graphite (AGI), the brake disk is designed as a single piece and is linked to the wheel hub (5) through composite casting by forming a positive material fitting joint (15) in the area where the hub (5) is connected to the base (3) of the disk.
    • 本发明涉及一种贝氏体淬火制动盘与通过铸造环形圆盘状的垫圈本体(1)制造的至少一个,其具有沿径向向外,与制动蹄制动环部分接触(2),其被布置用于在轮毂制动与车轮合作(5)。 为了避免噪音排放和振动,本发明的目的是由具有高强度和轻重量铸铁制动盘。 特别地,与本发明的制动盘到轮毂的复合构造的缺点是从铝除去。 根据本发明的制动盘的特征在于,由铸铁制成与片状石墨(AGI),由此制动盘在一块,并通过复合铸造制动盘体(1)与所述轮毂制成的制动盘的连续贝氏体淬火的制动盘体(1)(5)以形成粘结 复合体(15)连接在轮毂(5)与制动盘脚(3)的连接区域。
    • 7. 发明申请
    • BAINITICALLY HARDENED BRAKE DISK
    • BAINITICALLY硬化制动盘
    • WO99028641A3
    • 1999-07-22
    • PCT/DE1998/003507
    • 1998-11-26
    • B22D19/16B23P13/00B23P15/18B60B27/00B60T1/06C21D1/20C21D5/02F16D20060101F16D65/00F16D65/12
    • F16D65/12
    • The invention relates to a bainitically hardened brake disk comprising at least one ring-shaped cast disk (1) body with radially extending ring sections in contact with brake shoes (2). Said brake disk is mounted on the hub of a bicycle wheel (5) for braking purposes. In order to avoid noise emissions and vibrations, the inventive disk is made of cast iron, is highly tough and has a low weight. The aim is to avoid the disadvantages of combining disk brakes with an aluminium wheel hub. The inventive disk is characterised in that it has a thoroughly bainitically hardened body (1) made of cast iron with lamellar graphite (AGI), the brake disk is designed as a single piece and is linked to the wheel hub (5) through composite casting by forming a positive material fitting joint (15) in the area where the hub (5) is connected to the base (3) of the disk.
    • 本发明涉及一种贝氏体淬火制动盘与通过铸造环形圆盘状的垫圈本体(1)制造的至少一个,其具有沿径向向外,与制动蹄制动环部分接触(2),其被布置用于在轮毂制动与车轮合作(5)。 为了避免声发射和振动,本发明的目标是一种由铸铁制成的制动盘,其具有高强度和低重量。 特别是,用本发明来消除具有由铝制成的轮毂的制动盘的复合结构的缺点。 根据本发明的制动盘的特征在于,由铸铁制成与片状石墨(AGI),由此制动盘在一块,并通过复合铸造制动盘体(1)与所述轮毂制成的制动盘的连续贝氏体淬火的制动盘体(1)(5)以形成粘结 在轮毂(5)与制动盘基座(3)的连接区域中的合成点(15)被连接。
    • 10. 发明申请
    • MALLEABLE IRON CONTAINING GRAPHITE NODULES
    • 含有石墨粉的易燃铁
    • WO00066795A1
    • 2000-11-09
    • PCT/US1999/009446
    • 1999-04-30
    • C21D5/00C21D5/02C22C33/08C22C37/10C21D5/04C21D5/06C22C37/00C22C38/56
    • C21D5/00C21D5/02C22C33/08C22C37/10
    • The invention is a malleable iron comprising about 250 to 400 nodules of graphite per square millimeter as observed in a photomicrograph at 100x, and a Brinell hardness of about 195 to 550 BHN. Preferably, the malleable iron further comprises sulfur and manganese wherein the manganese is present in an excess amount of at least 2 times the amount of sulfur plus 0,15 % and is formed by two separate quenching steps. The invention further comprises a method of preparing a malleable iron having a high nodule count comprising the steps of prenucleating a malleable iron casting at a temperature of about 600 to 900 DEG F for about 3 to 6 hours; austenitizing the prenucleated casting at about 1680 to 1740 DEG F for about 3 to 9 hours to form graphite nodules such that the malleable iron has about 250 to 400 nodules per mm ; and quenching the casting to form pearlite and a malleable iron made by this process.
    • 本发明是一种可延展的铁,其包括在100x的显微照相中观察到的每平方毫米约250至400个石墨结石,布氏硬度为约195至550 BHN。 优选地,可锻铸铁还包含硫和锰,其中锰以超过硫加上0.15%的量的至少2倍的过量存在并且通过两个单独的淬火步骤形成。 本发明还包括一种制备具有高结瘤计数的可延展的铁的方法,其包括以下步骤:在约600-900°F的温度下将可锻铸铁铸件预核约3至6小时; 在约1680至1740°F奥氏体化前核心铸件约3至9小时以形成石墨结核,使得可锻铸铁每mm 2具有约250至400个结核; 并将铸件淬火以形成珠光体和通过该方法制成的可锻铸铁。