    • 2. 发明申请
    • POLYAMIDE-66-MONOFILAMENTS FOR PRECISION FABRICS
    • 尼龙单丝66 FOR PRECISION FABRICS
    • WO1996024711A1
    • 1996-08-15
    • PCT/CH1996000042
    • 1996-02-05
    • RHONE-POULENC VISCOSUISSE S.A.KURT, MaxSCHAFFNER, Paul
    • RHONE-POULENC VISCOSUISSE S.A.
    • D01F06/60
    • D01F6/60Y10T428/2913Y10T428/2969
    • The invention concerns a polyamide-66-monofilament with improved initial modulus and with a titre of dtex 4f1-150f1. The strength of the monofilaments is at least 60 cN/tex for an extension of less than 25 % and the specific LASE, in relation to the initial titre at 2 % is at least 7.5cN/tex, at 5 % at least 18cN/tex and at 10 % at least 40 cN/tex, and the dry relaxation is less than 25 %. The result is an improvement of about 40 % in the LASE at 2 % and an improvement of about 35 % in the wet relaxation compared to standard polyamide (PA 66) monofilament. The precision fabric manufactured from the monofilaments disclosed is particularly suitable for direct use in direct printing onto non-woven fabrics and hollow articles.
    • 本发明公开了具有改进的初始模量,并且具有分特4f1-150f1的线密度的聚酰胺66单丝。 是单丝的强度至少60厘牛顿/特以小于25%的伸长率和特定的LASE,基于所述Ausgangstiter以至少为7.5cN /特克斯的2%,以至少18厘牛顿/特的5%和至少40 10% CN /特,以及干松弛小于25%。 这导致改进的约40%LASE为2%,并与标准的聚酰胺(PA 66)单丝约35%的湿松弛改善。 由本发明的单丝制成的织物精度是优选直接适用于Direktfliesen-使用和中空体的压力。
    • 3. 发明申请
    • PROCESS FOR PRODUCING A HIGH-STRENGTH, HIGH-SHRINKAGE POLYAMIDE 66 FILAMENT YARN
    • 用于生产高强度,具有高收缩的尼龙66长丝纱线
    • WO1997008371A1
    • 1997-03-06
    • PCT/CH1996000288
    • 1996-08-20
    • RHONE-POULENC VISCOSUISSE S.A.FISCHER, KlausLINZ, HansBERGER, Luzius
    • RHONE-POULENC VISCOSUISSE S.A.
    • D02J01/22
    • D02J1/228Y10T428/2913Y10T428/2969
    • In a process for producing a high-strength, high-shrinkage polyamide 66 filament yarn for industrial fabrics, especially air-bag fabrics, by the multi-stage stretching of polyamide 66 LOY filament (1) with a relative viscosity RV of at least 40 by means of at least three heatable sets of stretching rollers (2, 3, 4) with the immediate winding of the stretched yarn (5) on a cylindrical core (6), the temperature of the last set (4) of stretching rollers before winding is set to between 70 and 160 DEG C before winding, with a relaxation ratio of 4 to 10 %, and the winding tension is set to under 0.2 cN/dtex. The polyamide 66 filament yarn has a strength of at least 60 cN/tex, an expansion of 10-25 % and a heat-shrinkage of 7-11 % (160 DEG C) and is eminently suitable for making air-bag fabrics. The yarn is wound on a package tube (cross-wound package) at at least 6 kg.
    • 一种生产高强度,对于工业织物高收缩尼龙-6,6长丝,特别是对气囊织物,通过多级聚酰胺66 LOY长丝的拉伸过程(1)具有至少40(相对粘度RV由至少三个可加热的拉伸辊组件2的装置 ,3,4)和直接卷绕拉伸丝(5)上的圆筒形导纱器(6)中,在松弛率为4-10%,最后的拉伸辊组件的温度(4),卷绕,70℃和160°之间之前 C,和卷绕张力小于0.2厘牛顿/分特组。 该聚酰胺66细丝纱线具有至少60厘牛顿/ tex的强度,10-25%的伸长率和7-11%(160℃)的热收缩率,优选地适合于气囊织物的制造。 纱线被卷绕具有至少6千克的筒管(乳酪)的。
    • 4. 发明申请
    • UNCOATED AIRBAG FABRIC
    • 安全气囊无涂层布
    • WO1996005985A1
    • 1996-02-29
    • PCT/CH1995000180
    • 1995-08-15
    • RHONE-POULENC VISCOSUISSE S.A.BERGEN, EberhardLALONDE, RemiLANG, Bruno
    • RHONE-POULENC VISCOSUISSE S.A.
    • B60R21/16
    • B60R21/235D03D1/02Y10T428/1362Y10T442/3024
    • An uncoated airbag fabric is made of a plain or rib weave of polyamide filament yarn with 1.5 to 7 dtex fibril titre, 50 to 80 cN/tex strength, 15 to 30 % extensibility, less than 3 l/dm /min air permeability, less than 2 % residual shrinkage when boiled and more than 110 N tear-grow resistance in warp and woof. In a process for producing this uncoated airbag fabric, a polyamide filament with less than 6 % hot air shrinkage and more than 0.20 cN/tex minimum resistance to shrinking is used. The fabric is treated in a closed container at a temperature from 80 to 160 DEG C and a relative atmospheric humidity from 90 to 100 %, is dried on a stretching frame and fixed or treated by a generally known calendering or sanforising process.
    • 它将分特由聚酰胺长丝纱的平纹或防裂织的未涂布的气囊织物具有1.5至7原纤维,50〜80厘牛顿/ tex的强度和15至30%的伸长率,具有小于3 1的透气度 /分米<2> /分,残余沸腾收缩率<2%和在经纱的撕裂传播强度和纬纱>为110N权利。 在未涂覆气囊织物的制备方法,用的热空气收缩<6%和最小收缩力> 0点20分的聚酰胺长丝,使用CN / tex的作为起始原料。 将织物在密闭容器中在80℃至160℃,90至100%的相对湿度处理,并在拉幅机上干燥和固定或处理与公知的压延或Sanforisierverfahren。
    • 7. 发明申请
    • PROCESS FOR SUBSEQUENT CONDENSATION OF POLYCONDENSATES, IN PARTICULAR OF POLYAMIDE 6.6
    • 方法缩聚物的aftercondensing,特别是聚酰胺6.6
    • WO1997024389A1
    • 1997-07-10
    • PCT/CH1995000307
    • 1995-12-27
    • RHONE-POULENC VISCOSUISSE S.A.BERGER, LuziusSTEHR, HansZEMP, Niklaus
    • RHONE-POULENC VISCOSUISSE S.A.
    • C08G69/28
    • C08G69/46C08G69/28C08G69/48C08J3/00C08J5/00C08J2377/00
    • The invention relates to a process for one-stage subsequent condensation of polycondensates, in particular of polyamide 6.6 granules in a fluidised bed reactor (1). During said process, a partial stream of a carrier gas, where nitrogen (N2) is used as the carrier gas, is removed at a temperature of 20-230 DEG C from the main stream and is conveyed in such a manner through a gas washing column (15) charged with water that the partial stream of conditioned carrier gas is returned with a point of condensation of 10-80 DEG C (100 % of relative humidity) into the main stream of the carrier gas. During the cooling phase of the granules, return of the partial stream of carrier gas is stopped. After cooling, the granules are removed and used directly in other applications. Said process achieves the designated viscosity and also a precisely defined level of humidity in the polymer, which level is important for further processing.
    • 在一种用于在流化床反应器中的缩聚物的单步后缩合,尤其是尼龙-6,6粒料的方法(1)载气中的20-230℃的温度下使用氮的部分流(N 2)作为从主流动,并通过截取的载体气体C 与引导,使得经调节的载气用10-80℃(相对湿度100%)露点部分流被返回到载气的主流水喂养的气体洗涤塔(15)。 在颗粒中的冷却阶段中,载气的部分流的供给被关闭。 冷却后,可以将颗粒排出并进一步直接使用。 用本发明的方法不仅所需的粘度,而且还用于进一步处理在聚合物中精确限定的水分被实现的一个重要。