    • REFRACTIVE INDEX GRATING MANUFACTURING PROCESS
    • 折射率指数制造工艺
    • WO2002073258A2
    • 2002-09-19
    • PCT/US2001/020280
    • 2001-06-26
    • 3M INNOVATIVE PROPERTIES COMPANY
    • GATICA, Anthony, W.DOWER, William, V.LEBLANC, Stephen, P.PEPIN, Ronald, P.GATES, Brian, J.CRONK, Bryon, J.COWHER, John, T.LABRAKE, Dwayne, L.NELSON, Brian, K.WALKER, Christopher, B.
    • G02B6/16
    • G02B6/02152B29C47/0021B29C47/02C03C25/106C03C25/12G02B6/245G02B6/3616G02B6/3636G03F7/001G03F7/24
    • A filament coating apparatus comprising a frame for releasably securing a filament, and a carriage mounted on the frame to oscillate between a first position and a second position. There is a first filament holding fixture mounted on the carriage and a second filament holding fixture also mounted on the carriage in axial alignment with the first filament holding fixture to secure a measured filament portion, preferably of an optical fiber, including a bare portion thereof, located inside a first boundary and a second boundary, between the first filament holding fixture and the second filament holding fixture. At least one spray head is attached to the frame at the first position with at least one radiation source attached to the frame at the second position. The measured filament portion moves between the spray head and the radiation source, during oscillation of the carriage between the first position and the second position to place the bare portion to receive a curable coating composition from the spray head, for application from the first boundary to the second boundary, and thereafter to cure the curable coating by exposure to radiation from the radiation source.
    • 一种灯丝涂覆设备,包括用于可释放地固定灯丝(20)的框架和安装在框架上以在第一位置和第二位置之间摆动的托架(354)。 安装在滑架上的第一灯丝固定夹具和第二灯丝保持夹具,其也安装在滑架上,与第一灯丝保持夹具轴向对准,以固定测量的细丝部分,优选地包括光纤的裸露部分, 位于第一边缘和第二边界之间,位于第一细丝保持固定装置和第二细丝保持固定装置之间。 至少一个喷头(322,326)在第一位置处附接到框架,其中至少一个辐射源(324,328)在第二位置处附接到框架。 测量的细丝部分在第一位置和第二位置之间的滑架摆动期间在喷头和辐射源(324,328)之间移动,以将裸露部分从喷头接收可固化的涂层组合物,以供应用 从第一边界到第二边界,然后通过暴露于来自辐射源的辐射固化可固化涂层。
    • 9. 发明申请
    • FILAMENT RECOATING APPARATUS AND METHOD
    • 纤维拾取装置和方法
    • WO2002072497A1
    • 2002-09-19
    • PCT/US2001/020405
    • 2001-06-26
    • 3M INNOVATIVE PROPERTIES COMPANY
    • NELSON, Brian, K.
    • C03C25/18
    • C03C25/18
    • A filament coating apparatus comprising a frame for releasably securing a filament, and a carriage mounted on the frame to oscillate between a first position and a second position. There is a first filament holding fixture mounted on the carriage and a second filament holding fixture also mounted on the carriage in axial alignment with the first filament holding fixture to secure a measured filament portion (250), preferably of an optical fiber, including a bare portion thereof, located inside a first boundary and a second boundary, between the first filament holding fixture and the second filament holding fixture. At least one extrusion coating fixture (334) is attached to the frame at the first position with at least one radiation source (336) attached to the frame at the second position. The measured filament portion moves between extrusion coating fixture (334) and the radiation source (336), during oscillation of the carriage between the first position and the second position to place the bare portion (250) to receive a curable coating composition from the to the second boundary, and thereafter to cure the curable coating by exposure to radiation from the radiation source (336).
    • 一种长丝涂覆装置,包括用于可释放地固定细丝的框架和安装在框架上的滑架,以在第一位置和第二位置之间摆动。 安装在滑架上的第一灯丝保持夹具和第二灯丝保持夹具也安装在滑架上,与第一灯丝保持夹具轴向对准,以固定测量的细丝部分(250),优选地包括光纤,包括裸露 位于第一光栅保持固定装置和第二灯丝固定装置之间的位于第一边界和第二边界内的部分。 至少一个挤压涂覆固定件(334)在第一位置处附接到框架,其中至少一个辐射源(336)在第二位置处附接到框架。 测量的细丝部分在挤压涂覆固定件(334)和辐射源(336)之间移动,在托架在第一位置和第二位置之间振荡期间,以将裸露部分(250)放置成接收可固化的涂料组合物 第二边界,然后通过暴露于来自辐射源(336)的辐射固化可固化涂层。
    • 10. 发明申请
    • METHOD OF MANUFACTURING TEMPERATURE RANGE ADJUSTED COATED OPTICAL FIBERS
    • 制造温度范围调节涂层光纤的方法
    • WO2002064525A1
    • 2002-08-22
    • PCT/US2002/003674
    • 2002-02-07
    • 3M INNOVATIVE PROPERTIES COMPANY
    • LYNCH, Thomas, M.NELSON, Brian, K.NOVACK, James, C.ONSTOTT, James, R.
    • C03C25/10
    • C03C25/12C03C25/1065Y10T428/2933
    • A method for manufacturing a coated optical fiber including the step of determining a desired temperature operating range of a coated optical fiber having at least one critical limit. The intercoating delamination stresses at the critical limit of said temperature range are determined. A zero-stress temperature region using the critical limit and the delamination stresses is then selected. An optical fiber is provided and the optical fiber is coated with a first polymer coating. The first polymer coating is exposed to a source of actinic radiation, wherein the source of actinic radiation generates heat. A second polymer coating including a photopolymerizable composition is applied to the optical fiber directly on the first polymer coating. The second polymer coating is cured, where at the time the second polymer coating is cured the first polymer coating is at the zero-stress temperature region.
    • 一种制造涂覆光纤的方法,包括确定具有至少一个临界极限的涂覆光纤的期望温度操作范围的步骤。 确定在所述温度范围的临界极限处的相互涂层分层应力。 然后选择使用临界极限和分层应力的零应力温度区域。 提供光纤并且光纤被第一聚合物涂层涂覆。 第一聚合物涂层暴露于光化辐射源,其中光化辐射源产生热量。 将包含可光聚合组合物的第二聚合物涂层直接施加到第一聚合物涂层上的光纤上。 固化第二聚合物涂层,其中在第二聚合物涂层固化时,第一聚合物涂层处于零应力温度区域。