    • METHOD FOR COATING AN ARCHITECTURAL TEXTILE WITH AT LEAST ONE LAYER OF A SILICONE ELASTOMER USING AN AQUEOUS SILICONE EMULSION AND AN ARCHITECTURAL TEXTILE WITH SUCH A COATING
    • 使用水性硅胶乳液和具有这种涂层的建筑纺织品的至少一层硅胶弹性体涂覆建筑纺织品的方法
    • WO03106759A9
    • 2005-04-07
    • PCT/FR0350012
    • 2003-06-17
    • FERRARI S TISSAGE & ENDUCT SAMARTIN GERALDINEPERILLON JEAN-LUC
    • MARTIN GERALDINEPERILLON JEAN-LUC
    • C03C25/40D06M15/643D06M15/693D06M15/70D06N3/12C08J3/03C09D183/04
    • D06M15/693C03C25/1095D06M15/643D06N3/128Y10T442/30
    • The invention relates to the production of silicone membranes for architectural use, by means of coating an architectural textile with a silicone, in particular, but not exclusively on a glass fabric. The aim of the invention is a method in which the deposition on the architectural textile may be easily and rapidly achieved with a coating rate of less than 40 g/m . Said aim is achieved whereby said method comprises the following steps: deposition on said architectural textile of at least one layer of an emulsion of polyorganosiloxane (POS), which may be cross-linked to give an elastomer by polyaddition and comprising: (A) a POS with =SiVinyl groups, (B) a POS with =SiH groups, (C) a special adherence promoter (polyvinyl alcohol) or POS(OH), (D) a catalyst, (E) at least one surface active agent, (F) optionally a POS resin with =SiVinyl groups, (G) optionally a cross-linking inhibitor, (H) optionally a pH stabilising agent,(I) optionally a formulation additive, (J) optionally a charge and (K) water, with the condition that 0.05 (C) 4 % by weight of the silicone phase, followed by cross-linking such that the weight proportion of the coating as a proportion of the dry weight of the architectural textile is less than 0.2 and preferably between 0.05 and 0.11.
    • 本发明涉及通过用硅树脂涂覆建筑织物,特别是但不限于玻璃织物来制造用于建筑用途的硅氧烷膜。 本发明的目的是可以以小于40g / m 2的涂布速率容易且快速地实现建筑织物上的沉积。 所述目的是实现的,其中所述方法包括以下步骤:在所述建筑织物上沉积至少一层聚有机硅氧烷(POS)的乳液,其可以被交联以通过加聚得到弹性体,并且包括:(A) POS具有= SiV基,(B)具有= SiH基的POS,(C)特殊粘附促进剂(聚乙烯醇)或POS(OH),(D)催化剂,(E)至少一种表面活性剂, F)任选地具有= SiVinyl基的POS树脂,(G)任选的交联抑制剂,(H)任选的pH稳定剂,(I)任选的制剂添加剂,(J)任选的电荷和(K) 其条件是硅氧烷相的重量比为0.05%(C) 4%,然后进行交联,使得涂层的重量比例为 建筑纺织品的干重小于0.2,优选为0.05至0.11。