    • 15. 发明申请
    • POLYESTER FIBER AND METHOD FOR MANUFACTURING SAME
    • 聚酯纤维及其制造方法
    • WO2012091524A2
    • 2012-07-05
    • PCT/KR2011010399
    • 2011-12-30
    • KOLON INCKIM YOUNG-JOAN BYOUNG-WOOKLEE SANG-MOKLEE YOUNG-SOOKIM GI-WOONG
    • KIM YOUNG-JOAN BYOUNG-WOOKLEE SANG-MOKLEE YOUNG-SOOKIM GI-WOONG
    • D01F1/10B60R21/16D01D5/08D01F6/62D02J1/22D03D1/02
    • D02G3/446B60R21/235D01D5/16D01F1/10D01F6/62D03D1/02D10B2331/04D10B2505/124Y10T428/249921
    • The present invention relates to a polyester fiber for use in airbag fabric, and more particularly, to a polyester fiber, to a method for manufacturing same, and to airbag fabric manufactured from the polyester fiber, wherein the polyester fiber is characterized in that the content of one or more organic fillers selected from a group consisting of TiO2, SiO2 and BaSO4 is 200 ppm or lower, elongation at break is 15% or higher, dry heat shrinkage is 3% or higher, and the sum of the elongation at break and dry heat shrinkage is 20% or higher. The polyester fiber of the present invention has significantly low stiffness and superior mechanical properties to ensure the physical properties of high strength, high elongation, and high shrinkage. Thus, the polyester fiber of the present invention, when used for airbag fabric, may significantly lower stiffness, improve toughness, tear strength, edge comb resistance, etc., provide air seal performance, be easily embedded in a vehicle, provide shape stability and air sealing effects, and minimize the shocks applied to a seat occupant in order to safely protect the seat occupant.
    • 本发明涉及一种用于气囊织物的聚酯纤维,更具体地说,涉及一种聚酯纤维及其制造方法,以及由聚酯纤维制成的气囊织物,其特征在于,所述聚酯纤维的含量 的一种或多种选自TiO 2,SiO 2和BaSO 4的有机填料为200ppm以下,断裂伸长率为15%以上,干热收缩率为3%以上,断裂伸长率和 干热收缩率为20%以上。 本发明的聚酯纤维具有显着低的刚度和优异的机械性能,以确保高强度,高伸长率和高收缩率的物理性能。 因此,本发明的聚酯纤维用于气囊织物时,可显着降低刚度,提高韧性,撕裂强度,边缘梳理性等,提供空气密封性能,易于嵌入车辆,提供形状稳定性和 空气密封效果,并尽量减少施加到座椅乘客的冲击,以安全地保护座椅乘客。
    • 16. 发明申请
    • METHOD FOR MANUFACTURING A POLYESTER YARN
    • 制造聚酯纱线的方法
    • WO2013025062A3
    • 2013-06-13
    • PCT/KR2012006525
    • 2012-08-16
    • KOLON INCKIM YOUNG-JOAN BYOUNG-WOOKLEE SANG-MOKLEE YOUNG-SOOKIM GI-WOONG
    • KIM YOUNG-JOAN BYOUNG-WOOKLEE SANG-MOKLEE YOUNG-SOOKIM GI-WOONG
    • D01F6/62D01D5/08D02J1/22D03D15/00
    • B60R21/231C08G63/183C08G63/80D01D5/098D01F6/84D02J1/22D03D1/02D03D15/00D10B2331/04Y10T442/30
    • The present invention relates to a polyester yarn usable in an air bag fabric, and more specifically, to a method for manufacturing a polyester yarn, an air bag yarn manufactured therefrom, and an air bag fabric including the same, wherein the method comprises the steps of: mixing a specific dicarboxylic acid composition and glycol in a predetermined range, and performing an ester reaction; performing a polycondensation reaction for an oligomer created by said ester reaction; performing solid state polymerization for a polymer created by said polycondensation reaction; and performing melt spinning for a polyester chip created by said solid state polymerization, and performing stretching. The polyester yarn manufactured by the present invention has low modulus, high strength, and further, high contraction. In addition, the polyester yarn of the present invention obtains an excellent mechanical property with remarkably low stiffness, thereby providing a superior storage effect, shape stabilization, and an air blocking effect when used for an air bag fabric.
    • 本发明涉及一种可用于气囊织物中的聚酯纱线,更具体地说,涉及一种聚酯纱线的制造方法,由其制造的气囊纱线以及包括该聚酯纱线的气囊织物,其中该方法包括步骤 :将特定的二羧酸组合物与二醇在规定的范围内混合,进行酯反应; 对由所述酯反应产生的低聚物进行缩聚反应; 对由所述缩聚反应产生的聚合物进行固态聚合; 并对由所述固态聚合产生的聚酯切片进行熔融纺丝,并进行拉伸。 由本发明制造的聚酯纱具有低模量,高强度和进一步高收缩率。 此外,本发明的聚酯纱线具有优异的机械性能,刚度显着低,因此当用于气囊织物时提供优异的储存效果,形状稳定性和空气阻塞效果。