    • 6. 发明申请
    • PHENOLIC FOAM
    • 酚醛泡沫
    • US20110124257A1
    • 2011-05-26
    • US11991533
    • 2006-09-08
    • Vincent CoppockRuud ZeggelaarHiroo TakahashiToshiyuki Kato
    • Vincent CoppockRuud ZeggelaarHiroo TakahashiToshiyuki Kato
    • C08J9/06C08K3/26C08K5/12B32B5/18
    • C08J9/145C08J9/0066C08J9/149C08J2203/14C08J2203/142C08J2361/06C08J2361/10C08L71/08Y10T428/249953Y10T442/647
    • A phenolic foam is made by foaming and curing a formable phenolic resin composition that comprises a phenolic resin, a blowing agent, an acid catalyst and an inorganic filler. The blowing agent comprises a blend of chlorinated aliphatic hydrocarbon containing 2 to 5 carbon atoms and an aliphatic hydrocarbon containing from 3 to 6 carbon atoms mixed in a ratio of 60/40 to 95/5 parts by weight. The inorganic filler is at least one selected from a metal hydroxide, a metal oxide, a metal carbonate and metal powder. The phenolic foam has a pH of 5 or more and a water uptake less than 1 kg/m2. A phenolic foam with a higher pH value compared with conventional phenolic foam reduces corrosion risk when in contact with metallic materials. The phenolic foam maintains excellent long-term stable thermal insulation performance, low water uptake and fire resistance performance and by using the said blowing agent, does not harm the environment as an ozone or global warming depleting material.
    • 通过发泡和固化包含酚醛树脂,发泡剂,酸催化剂和无机填料的可成形酚醛树脂组合物来制备酚醛泡沫。 发泡剂包含含有2至5个碳原子的氯代脂族烃和含有3-6个碳原子的脂族烃的混合物,其混合比例为60/40至95/5重量份。 无机填料是选自金属氢氧化物,金属氧化物,金属碳酸盐和金属粉末中的至少一种。 酚醛泡沫体的pH为5以上,吸水量小于1kg / m 2。 与常规酚醛泡沫相比,具有较高pH值的酚醛泡沫体在与金属材料接触时可降低腐蚀风险。 酚醛泡沫塑料具有优异的长期稳定的隔热性能,低吸水性和耐火性能,并且通过使用所述发泡剂,不会对臭氧或全球变暖消耗材料造成危害。
    • 7. 发明申请
    • Natural Fibre Thermoset Composite Product and Method For Manufacturing the Same
    • 天然纤维热固性复合材料及其制造方法
    • US20090130377A1
    • 2009-05-21
    • US12063911
    • 2006-08-10
    • Dasarathi SamantaAnukul SamantaMahadeb SamantaBasudev Samanta
    • Dasarathi SamantaAnukul SamantaMahadeb SamantaBasudev Samanta
    • B32B5/02
    • C08J5/045C08J2361/10C08J2361/24C08J2361/28Y10T156/1052Y10T428/24124
    • A natural fibre thermoset composite product of high tensile strength, high compressive strength, high cross breaking point, high water absorption properties and a method for producing the same. The product comprises bamboo and jute fibre, resins, fillers and additives wherein bamboo and jute are present in the ratio of 1:99 to 99:1 as reinforcement material. The method of manufacture of natural fibre thermoset composite product of high tensile strength, high compressive strength, high cross breaking point, high water absorption properties comprises forming slurry with resin solution, fillers and optional additives; impregnation of bamboo and jute provided in a ratio of 1:99 to 99:1 as reinforcement material into the slurry; drying said impregnated bamboo and jute composite in oven at temperature of 100° C. to 200° C.; cutting said impregnated and dried bamboo and jute composite into required size; said impregnated dried cut pieces of bamboo and jute composite multilayered according to require thickness and pressed in the hydraulic press at a pressure 1 to 3 tons per square inches for a definite period at a defined temperature. The composite product is adapted to be used as floor board, paneling sheet, roofing material and the like.
    • 高抗拉强度,高抗压强度,高断裂点,高吸水性的天然纤维热固性复合材料及其制造方法。 该产品包括竹和黄麻纤维,树脂,填料和添加剂,其中竹和黄麻以1:99至99:1的比例作为增强材料存在。 高抗拉强度,高抗压强度,高断裂点,高吸水性的天然纤维热固性复合材料的制造方法包括用树脂溶液,填料和任选的添加剂形成浆料; 以1:99至99:1的比例提供竹和黄麻作为增强材料浸入浆料中; 在100℃至200℃的温度下烘干所述浸渍的竹和黄麻复合物。 将浸渍和干燥的竹和黄麻复合材料切割成所需尺寸; 所述浸渍的竹和黄麻复合材料的干燥切片根据要求的厚度多层化,并且在液压机中以1至3吨/平方英寸的压力在一定的温度下固定一段时间。 复合产品适用于地板,镶板,屋顶材料等。