    • Process for making a polyurethane foam
    • 制造聚氨酯泡沫的方法
    • US08658709B2
    • 2014-02-25
    • US12294066
    • 2007-02-22
    • Philip BerthelsRaf ElenLuc Van Essche
    • Philip BerthelsRaf ElenLuc Van Essche
    • C08G18/00
    • C08G18/4833C08G18/6677C08G2101/0008C08G2101/005C08G2101/0075C08G2101/0083C08G2350/00
    • Process for preparing a polyurethane foam, according to the free rise process, the foam having a free rise density of 5-40 kg/m3, comprising reacting at an index of 40-80 a polyisocyanate composition consisting of diphenylmethane diisocyanate and of homologues of diphenylmethane diisocyanate, said homologues having an isocyanate functionality of 3 or more, and wherein the polyisocyanate composition has an average isocyanate functionality of 2.10-2.40 and a 2,4′-diphenylmethane diisocyanate content of 6-45% by weight with the proviso that the relationship between this functionality (F) and content (C) is: −123F+287≦C≦−123F+311, and a polyoxyethylene polyoxypropylene polyol (polyol b1) having an oxyethylene content of 5-30% by weight, a nominal functionality of 2-4 and an average equivalent weight of 1000-3000, and comprising using 5-20 parts by weight, per 100 parts by weight of polyol b1, of water as blowing agent, an effective amount of a catalyst enhancing urethane formation, and an effective amount of a surfactant.Foams are claimed as well. The foams show good sound absorption and/or sound insulation.
    • 制备聚氨酯泡沫的方法,根据自由升高方法,泡沫的自由升高密度为5-40kg / m 3,包括以40-80的指数反应由二苯基甲烷二异氰酸酯和二苯基甲烷的同系物组成的多异氰酸酯组合物 二异氰酸酯,所述同系物的异氰酸酯官能度为3以上,其中多异氰酸酯组合物的平均异氰酸酯官能度为2.10-2.40,2,4'-二苯基甲烷二异氰酸酯含量为6-45重量%,条件是 在该功能性(F)和含量(C)之间为:-123F + 287 @ C @ -123F + 311,和氧化乙烯含量为5-30重量%的聚氧乙烯聚氧丙烯多元醇(多元醇b1),标称官能度 2-4,平均当量为1000-3000,并且包括使用5-20重量份,相对于100重量份的多元醇b1,水作为发泡剂,有效量的催化剂增强聚氨酯形成,和 有效量的表面活性剂。 泡沫也被要求。 泡沫显示出良好的吸声和/或隔音效果。