热词
    • 2. 发明授权
    • Expanded material and laminate
    • 膨胀材料和层压板
    • US6110578A
    • 2000-08-29
    • US482111
    • 2000-01-13
    • Yasutoshi KakizawaToshiki Shikata
    • Yasutoshi KakizawaToshiki Shikata
    • C08J9/00B32B3/26
    • C08J9/00C08J2367/02
    • The present invention provides a biodegradable expanded material having excellent expandability, moldability, impact resistance, heat resistance and storage stability. The present invention also provides a process for the preparation of the foregoing expanded material. The present invention further provides a laminate of a non-expanded material layer and an expanded material layer prepared from the foregoing expanded material which exhibits excellent impact resistance and heat resistance and an excellent transparency in the non-expanded material even after heat treatment so that a pattern printed on the inner side of the non-expanded material layer can be clearly viewed from the outside. A novel expanded material is provided made of a hydroxycarboxylic acid based polyester having a weight-average molecular weight of from 20,000 to 400,000 comprising as structural units a structural unit derived from hydroxycarboxylic acid, a structural unit derived from molecular weight increasing agent and/or a structural unit derived from polymerization catalyst deactivator.
    • 本发明提供具有优异的可膨胀性,成型性,耐冲击性,耐热性和储存稳定性的生物降解性发泡材料。 本发明还提供了制备上述膨胀材料的方法。 本发明还提供一种非发泡材料层和由上述膨胀材料制成的发泡材料层的叠层体,即使在热处理后也显示出优异的抗冲击性和耐热性,并且非发泡材料的透明度优异, 可以从外部清楚地看到印刷在非发泡材料层的内侧上的图案。 提供一种新型膨胀材料,其由重均分子量为20,000至400,000的羟基羧酸基聚酯制成,其包含衍生自羟基羧酸的结构单元作为结构单元,衍生自分子量增加剂的结构单元和/或 衍生自聚合催化剂失活剂的结构单元。
    • 5. 发明授权
    • Process for the preparation of lactic acid-based polyester
    • 制备乳酸基聚酯的方法
    • US5686540A
    • 1997-11-11
    • US722599
    • 1996-09-27
    • Yasutoshi Kakizawa
    • Yasutoshi Kakizawa
    • C08L67/02C08L67/04C08F20/00
    • C08L67/02C08L67/04
    • The present invention provides a process for the preparation of a biodegradable lactic acid-based polyester composition excellent in thermal stability, storage stability, flexibility, heat resistance, mechanical and physical properties and moldability which comprises kneading a lactic acid-based polyester and a polyester consisting of dicarboxylic acid component(s) and diol component(s) with a chelating agent, an acidic phosphoric acid ester, a molecular weight increasing agent, etc., and then devolatizing the kneaded mixture. The present invention also provides a molding process of the foregoing lactic acid-based polyester composition. A novel process for the preparation of a lactic acid-based polyester composition is provided, which comprises melt-kneading a lactic acid-based polyester (A), a polyester (B) consisting of dicarboxylic acid component(s) and diol component(s) and a chelating agent and/or acidic phosphoric acid ester (C) in an amount such that the weight ratio (A)/(B is from 99/1 to 10/90 and the proportion of (C) is 0.001 to 5 parts by weight based on 100 parts by weight of the sum of (A) and (B). A novel process for molding a lactic acid-based polyester composition is also provided, which comprises kneading a lactic acid-based polyester (A) and a polyester (B) consisting of dicarboxylic acid component(s) and diol component(s) with a chelating agent and/or acidic phosphoric acid ester (C), and then molding the material.
    • 本发明提供一种制备热稳定性,保存稳定性,柔软性,耐热性,机械和物理性能以及成型性优异的生物降解性乳酸类聚酯组合物的方法,其包括将乳酸类聚酯与含有 的二羧酸组分和二醇组分与螯合剂,酸性磷酸酯,分子量增加剂等混合,然后使捏合的混合物脱水。 本发明还提供了上述乳酸类聚酯组合物的成型方法。 提供了一种制备乳酸基聚酯组合物的新方法,其包括将乳酸基聚酯(A),由二羧酸组分和二醇组分(B)组成的聚酯(B) )和螯合剂和/或酸性磷酸酯(C),其量使得重量比(A)/(B为99/1〜10/90,(C)的比例为0.001〜5份 (A)和(B)之和的100重量份,还提供了一种新型的乳酸类聚酯组合物的成型方法,其包括将乳酸类聚酯(A)和 由二羧酸组分和二醇组分与螯合剂和/或酸性磷酸酯(C)组成的聚酯(B),然后模塑该材料。
    • 6. 发明授权
    • Process for the continuous production of biodegradable polyester polymer
    • 连续生产可生物降解聚酯聚合物的方法
    • US5484882A
    • 1996-01-16
    • US272191
    • 1994-07-08
    • Morio TakadaYasutoshi Kakizawa
    • Morio TakadaYasutoshi Kakizawa
    • C08G63/08C08G63/78C08L101/16C08F6/00
    • C08G63/08Y02P20/582
    • The present invention provides a process for the continuous production of a biodegradable polyester polymer with an excellent quality useful in the field of medicine, coating material and packaging material by eliminating difficulty in uniform agitation and heat removal caused by the rise in the viscosity of reactants in the production of a high molecular biodegradable polyester polymer by ring-opening polymerization. In some detail, the present invention provides a process for the continuous production of a biodegradable polyester polymer having a melt viscosity of not more than 500,000 poise and a weight-average molecular weight of not less than 10,000, which comprises continuously supplying monomers or polymers selected from the group consisting of intermolecularly cyclized ester of hydroxycarboxylic acid, lactone, and polymer having hydroxyl group and/or ester bond into a continuous reaction apparatus equipped with a static mixer where the reactants are subjected to continuous polymerization reaction at a polymerization temperature of 125.degree. to 270.degree. C., a maximum system reaction pressure of 2 to 15 Kg/cm.sup.2 and a conversion (one pass) of not less than 85% in the presence or absence of solvent without coming into contact with oxygen and water in the atmosphere, and then subjected to devolatilization to remove and recover residual monomers and solvent for reuse.
    • 本发明提供了通过消除由于反应物的粘度升高引起的均匀搅拌和除热的困难而连续生产具有优异品质的可生物降解的聚酯聚合物的方法,其用于医药,涂料和包装材料领域 通过开环聚合生产高分子生物降解聚酯聚合物。 更详细地说,本发明提供了连续制备熔体粘度不超过500,000泊,重均分子量不小于10,000的可生物降解聚酯聚合物的方法,该方法包括连续供应选择的单体或聚合物 由羟基羧酸的分子内环化的酯,具有羟基和/或酯键的聚合物组成的组中,连接反应装置,该反应装置配备有在125℃的聚合温度下使反应物进行连续聚合反应的静态混合器 在270℃,最大系统反应压力为2至15Kg / cm 2,并且在存在或不存在溶剂的情况下转化率(一次通过)不低于85%,而不与大气中的氧气和水接触, 然后进行脱挥发分以除去和回收残留的单体和溶剂以便重复使用。
    • 8. 发明授权
    • Process for the preparation of lactic acid-based polyester
    • 制备乳酸基聚酯的方法
    • US5844066A
    • 1998-12-01
    • US712994
    • 1996-09-10
    • Yasutoshi Kakizawa
    • Yasutoshi Kakizawa
    • C08K5/00C08G63/06C08G63/60C08G63/88C08G63/90C08G63/91C08L67/00C08L67/04C08L101/16C08G63/08C08F20/00
    • C08G63/60C08G63/912
    • The present invention provides a process for the preparation of a lactic acid-based polyester having an excellent moldability, storage stability and biodegradability which has a less residual lactide left therein and is less susceptible to decomposition of lactic acid-based polyester and attachment of sublimed lactide to the molding apparatus, etc. at the devolatilization step and molding step after the polymerization reaction of lactic acid-based polyester. In the present invention, an organic chelating agent is added to a lactic acid-based polyester to deactivate the esterification catalyst used in the preparation of the lactic acid-based polyester, making it possible to inhibit the decomposition of lactic acid-based polyester at the devolatilizing process and molding process after polymerization reaction. Accordingly, a process for the preparation of a lactic acid-based polyester useful as a packaging material such as film and sheet having a high molecular weight, a high heat resistance, good mechanical properties and excellent moldability, storage stability and biodegradability can be provided.
    • 本发明提供一种制备具有优异的成型性,保存稳定性和生物降解性的乳酸类聚酯的方法,其残留的残留丙交酯残留在乳酸基聚酯中并不易分解,并且升华的丙交酯的附着 在乳酸类聚酯的聚合反应之后的脱挥发分步骤和成型步骤中的成型装置等。 在本发明中,向乳酸类聚酯中添加有机螯合剂使乳酸类聚酯的制造中所使用的酯化催化剂失活,能够抑制乳酸类聚酯的分解 脱挥发分过程和聚合反应后的成型工艺。 因此,可以提供一种制备用作具有高分子量,高耐热性,良好机械性能和优异的成型性,保存稳定性和生物降解性的包装材料如薄膜和片材的乳酸基聚酯的方法。