    • 1. 发明授权
    • Method for preparing a vinyl polymer-polyolefine composite
    • 乙烯基聚合物 - 聚烯烃复合材料的制备方法
    • US5312872A
    • 1994-05-17
    • US103886
    • 1993-08-06
    • Torvald VestbergIsmo Lehtiniemi
    • Torvald VestbergIsmo Lehtiniemi
    • C08F255/00C08F2/18C08F255/02B32B27/30C08J3/02
    • C08F255/02
    • A method for preparing a polyolefine-vinyl composite, in which method about 10-200 weight fractions of vinyl monomer and about 0.01-4.0 weight fractions of a free radical polymerization initiator, based on 100 weight fractions of vinyl monomer, are impregnated in 100 weight fractions of polyolefine particles by slowly mixing these at a temperature of about 20.degree.-100.degree. C. while continuously or discontinuously adding about 1-60% by weight of water, based on the total weight of the vinyl monomer and the polyolefine, during the maintenance of the particle structure of the polyolefine, is disclosed. A water suspension is prepared by adding water and stabilizing agents to the above-mentioned mixture after a completed impregnation. The total quantity of water is about 80-1000 weight fractions, based on 100 weight fractions of polyolefine+vinyl monomer. The temperature of the water suspension is then increased for polymerizing the vinyl monomer.
    • 一种制备聚烯烃 - 乙烯基复合材料的方法,其中基于100重量份乙烯基单体约10-200重量份的乙烯基单体和约0.01-4.0重量份的自由基聚合引发剂以100重量份 通过在约20℃-100℃的温度下缓慢混合它们,同时连续地或不连续地加入约1-60重量%的水,基于乙烯基单体和聚烯烃的总重量,聚烯烃微粒的分数 公开了维持聚烯烃的颗粒结构。 在完全浸渍之后,通过向上述混合物中加入水和稳定剂来制备水悬浮液。 基于100重量份的聚烯烃+乙烯基单体,水的总量为约80-1000重量份。 然后增加水悬浮液的温度以使乙烯基单体聚合。
    • 4. 发明授权
    • Method for preparing a vinyl polymer-polyolefine composite
    • 乙烯基聚合物 - 聚烯烃复合材料的制备方法
    • US5300578A
    • 1994-04-05
    • US9772
    • 1993-01-27
    • Torvald VestbergIsmo Lehtiniemi
    • Torvald VestbergIsmo Lehtiniemi
    • C08F2/00C08F2/18C08F2/44C08F255/02C08F2/20C08F255/04
    • C08F255/02
    • A method for preparing a polyolefine--vinyl polymer composite, wherein about 10-200 parts by weight of vinyl monomer and about 0.01-4.0 parts by weight of a free radical polymerization initiator, based on 100 parts by weight of vinyl monomer, are impregnated in 100 parts of weight of polyolefine particles by slowly mixing these at a temperature of about 20.degree.-130.degree. C. while maintaining the particle structure of the polyolefine. After 50-99% of the amount of the monomer has been absorbed into the polyolefine particles, a water suspension is prepared by adding to the above-mentioned mixture about 80-1000 parts by weight water, based on 100 parts of weight of polyolefine+vinyl monomer, as well as a stabilizing agent. The temperature of the water suspension is then increased for polymerizing the vinyl monomer.
    • 一种制备聚烯烃 - 乙烯基聚合物复合材料的方法,其中基于100重量份的乙烯基单体将约10-200重量份的乙烯基单体和约0.01-4.0重量份的自由基聚合引发剂浸渍在 通过在保持聚烯烃的颗粒结构的同时在约20摄氏度至130摄氏度的温度下缓慢混合它们100重量份的聚烯烃微粒。 在50-99%的单体量被吸收到聚烯烃颗粒中之后,通过向上述混合物中加入约80-1000重量份的水,基于100重量份的聚烯烃+ 乙烯基单体,以及稳定剂。 然后增加水悬浮液的温度以使乙烯基单体聚合。