    • 2. 发明授权
    • Treatment of an orifice plate with self-assembled monolayers
    • 用自组装单层处理孔板
    • US5598193A
    • 1997-01-28
    • US410624
    • 1995-03-24
    • David J. HalkoBarbara T. Halko
    • David J. HalkoBarbara T. Halko
    • B41J2/14B41J2/16B41J2/135
    • B41J2/1631B41J2/14B41J2/1606B41J2/162B41J2/1643B82Y30/00
    • Treatment of the inner and outer surfaces of an orifice plate for ink-jet pens with self-assembled monolayers is disclosed. The outer surface of a gold-plated orifice plate is treated with self-assembled monolayers to control the wettability of the surface in order to reduce the accumulation of residual ink. The inner surface is treated with self-assembled monolayers to improve and control drop ejection. Various monolayers can also be used on the inner surface allowing for greater flexibility in controlling the steady state firing rate and uniformity of drops from a pen. In addition, treatment of orifice plate surfaces with self-assembled monolayers inhibits corrosion and contamination of the plate while presenting a uniform surface for the ink. The self-assembled monolayers for use in the present invention include thiols, disulfides, and sulfinates, having terminal functional groups which determine the wettability of the surface. A chemical bond is formed between the gold on the orifice plate and the thiol, disulfide, or sulfinate group of the monolayer compounds. The terminal functional group of the monolayer compound is therefore oriented away from the surface of the orifice plate and renders the surface either wetting or nonwetting depending on whether the terminal group has hydrophobic or hydrophilic characteristics.
    • 公开了具有自组装单层的喷墨笔的孔板的内表面和外表面的处理。 用自组装单层处理镀金孔板的外表面以控制表面的润湿性,以减少残留油墨的积聚。 内表面用自组装单层处理,以改善和控制液滴喷射。 也可以在内表面上使用各种单层,从而允许更大的灵活性来控制稳态燃烧速率和从笔中的液滴的均匀性。 此外,用自组装单层处理孔板表面抑制板的腐蚀和污染,同时为油墨提供均匀的表面。 用于本发明的自组装单层包括具有确定表面润湿性的末端官能团的硫醇,二硫化物和亚硫酸盐。 孔板上的金和单层化合物的硫醇,二硫化物或亚磺酸盐之间形成化学键。 因此,单层化合物的末端官能团取向远离孔板的表面,并使表面润湿或不润湿,这取决于端基是否具有疏水性或亲水性。
    • 7. 发明授权
    • Treatment of an orifice plate with self-assembled monolayers
    • 用自组装单层处理孔板
    • US6102521A
    • 2000-08-15
    • US790744
    • 1997-01-27
    • David J. HalkoBarbara Tomlonovic Halko
    • David J. HalkoBarbara Tomlonovic Halko
    • B41J2/14B41J2/16
    • B41J2/1631B41J2/14B41J2/1606B41J2/162B41J2/1643B82Y30/00
    • Treatment of the inner and outer surfaces of an orifice plate for ink-jet pens with self-assembled monolayers is disclosed. The outer surface of a gold-plated orifice plate is treated with self-assembled monolayers to control wettability of the surface in order to reduce the accumulation of residual ink. The inner surface is treated with self-assembled monolayers to improve and control drop ejection. Various monolayers can also be used on the inner surface allowing for greater flexibility in controlling the steady state firing rate and uniformity of drops from a pen. In addition, treatment of orifice plate surfaces with self-assembled monolayers inhibits corrosion and contamination of the plate while presenting a uniform surface for the ink. The self-assembled monolayers for use in the present invention include thiols, disulfides, and sulfinates, having terminal functional groups which determine the wettability of the surface. A chemical bond is formed between the gold on the orifice plate and the thiol, disulfide, or sulfinate group of the monolayer compounds. The terminal functional group of the monolayer compound is therefore oriented away from the surface of the orifice plate and renders the surface either wetting or nonwetting depending on whether the term group has hydrophobic or hydrophilic characteristics.
    • 公开了具有自组装单层的喷墨笔的孔板的内表面和外表面的处理。 用自组装单层处理镀金孔板的外表面以控制表面的润湿性,以减少残留油墨的积聚。 内表面用自组装单层处理,以改善和控制液滴喷射。 也可以在内表面上使用各种单层,从而允许更大的灵活性来控制稳态燃烧速率和从笔中的液滴的均匀性。 此外,用自组装单层处理孔板表面抑制板的腐蚀和污染,同时为油墨提供均匀的表面。 用于本发明的自组装单层包括具有确定表面润湿性的末端官能团的硫醇,二硫化物和亚硫酸盐。 孔板上的金和单层化合物的硫醇,二硫化物或亚磺酸盐之间形成化学键。 因此,单层化合物的末端官能团取向远离孔板的表面,并使表面润湿或不润湿,这取决于术语基团是否具有疏水性或亲水性。
    • 8. 发明授权
    • Polyamines complexed to anionic dyes, thereby forming water-soluble
cationic dyes
    • 多胺与阴离子染料络合,从而形成水溶性阳离子染料
    • US5788753A
    • 1998-08-04
    • US738532
    • 1996-10-28
    • Norman E. PawlowskiDavid J. HalkoJoseph W. TsangKimberly L. Hockaday Dahm
    • Norman E. PawlowskiDavid J. HalkoJoseph W. TsangKimberly L. Hockaday Dahm
    • C09B69/04C09D11/00C09D11/02
    • C09D11/328C09B69/04
    • An ink-jet ink for ink-jet printers is provided, comprising: (a) an aqueous-based vehicle; and (b) an anionic dye complexed with a polyamine in an amount sufficient to form a pH-insensitive, water-soluble, dye:polyamine complex that acts like a cationic dye. Further, a method of converting the anionic dye to the cationic dye for formulating the ink-jet ink having a desired pH is provided. The method comprises adding a sufficient amount of the polyamine to form the dye:polyamine complex. The dye:polyamine complex is a complex of the dye and the polyamine polymer, which is cationic. Consequently, this complex behaves as a cationic dye. These ink-jet inks show remarkable waterfastness on a variety of common office papers and are pH-insensitive and even in some cases, completely pH-independent. These inks are thus stable over a wide pH range. In addition, the ink-jet inks exhibit superior ink-to-ink bleed when printed next to a drop of another color ink which contains an anionic polymer or carboxylated colorant and resist crusting or drying in ink-jet nozzles.
    • 提供一种用于喷墨打印机的喷墨油墨,包括:(a)水性载体; 和(b)与多胺络合的阴离子染料,其量足以形成像阳离子染料一样起作用的pH不敏感的水溶性染料:多胺络合物。 此外,提供了将阴离子染料转化为阳离子染料以配制具有所需pH的喷墨油墨的方法。 该方法包括加入足量的多胺以形成染料:多胺络合物。 染料:多胺络合物是染料和聚胺聚合物的复合物,其是阳离子的。 因此,这种复合物表现为阳离子染料。 这些喷墨墨水在各种常见的办公用纸上显示出显着的耐水性,并且pH不敏感,甚至在某些情况下,完全不依赖于pH。 因此,这些油墨在宽的pH范围内是稳定的。 此外,喷墨墨水在印刷在一滴含有阴离子聚合物或羧化着色剂的另一种彩色墨水上并且在喷墨喷嘴中抵抗结皮或干燥时表现出优异的墨到墨渗色。