    • 2. 发明申请
    • Trough channel transistor and methods for making the same
    • 槽通道晶体管及其制作方法
    • US20120306005A1
    • 2012-12-06
    • US13136051
    • 2011-07-21
    • Kimihiro SatohJing ZhangYiming Huai
    • Kimihiro SatohJing ZhangYiming Huai
    • H01L29/78H01L21/336
    • H01L29/66795H01L29/7851
    • The present invention relates to transistor devices having a trough channel structure through which electrical current flows and methods for making the same. A transistor device having a semiconductor trough structure comprises a semiconductor substrate of a first conductivity type having a top surface; a semiconductor trough protruded from the top surface of the substrate along a first direction and having two top surfaces, two outer lateral surfaces, and an inner surface; a layer of isolation insulator disposed on the substrate and abutting the outer lateral surfaces of the semiconductor trough; a gate dielectric layer lining the inner surface and the top surfaces of the semiconductor trough; and a gate electrode disposed on top of the isolation insulator and extending over and filling the semiconductor trough with the gate dielectric layer interposed therebetween. The gate electrode extends along a second direction not parallel to the first direction provided in the semiconductor trough. Regions of the semiconductor trough not directly beneath the gate electrode have a second conductivity type opposite to the first conductivity type provided in the substrate.
    • 本发明涉及具有通过电流流过的槽槽结构的晶体管器件及其制造方法。 具有半导体槽结构的晶体管器件包括具有顶表面的第一导电类型的半导体衬底; 半导体槽沿着第一方向从基板的顶表面突出并具有两个顶表面,两个外侧表面和内表面; 隔离绝缘层,设置在所述基板上并邻接所述半导体槽的外侧表面; 栅极电介质层,衬在半导体槽的内表面和顶表面上; 以及栅电极,其设置在隔离绝缘体的顶部并且延伸并填充半导体槽,栅介电层插入其间。 栅电极沿着不平行于半导体槽中的第一方向的第二方向延伸。 不直接在栅电极下方的半导体槽的区域具有与设置在基板中的第一导电类型相反的第二导电类型。
    • 4. 发明授权
    • MRAM with sidewall protection and method of fabrication
    • MRAM具有侧壁保护和制造方法
    • US08796795B2
    • 2014-08-05
    • US13136454
    • 2011-08-01
    • Kimihiro SatohYiming HuaiJing ZhangEbrahim Abedifard
    • Kimihiro SatohYiming HuaiJing ZhangEbrahim Abedifard
    • H01L27/24H01L27/22H01L45/00
    • H01L27/222H01L27/2436H01L43/08H01L43/12H01L45/04H01L45/06H01L45/1233H01L45/1675
    • BEOL memory cells are described that include one or more sidewall protection layers on the memory device (including, for example, an MTJ element) deposited prior to interconnect via etching to prevent the formation of electrical shorts between layers. One embodiment uses a single layer sidewall protection sleeve that is deposited after the memory device has been patterned. The layer material is vertically etched down to expose the upper surface of the top electrode while leaving a residual layer of protective material surrounding the rest of the memory device. The material for the protection layer is selected to resist the etchant used to remove the first dielectric material from the via in the subsequent interconnect process. A second embodiment uses dual-layer sidewall protection in which the first layer covers the memory element is preferably an oxygen-free dielectric and the second layer protects the first layer during via etching.
    • 描述了BEOL存储器单元,其包括在经由蚀刻互连之前沉积的存储器件(包括例如MTJ元件)上的一个或多个侧壁保护层,以防止在层之间形成电短路。 一个实施例使用在存储器件已被图案化之后沉积的单层侧壁保护套管。 层材料被垂直地蚀刻以暴露顶部电极的上表面,同时留下围绕存储器件的其余部分的保护材料的残留层。 选择保护层的材料以抵抗用于在随后的互连过程中从通孔去除第一介电材料的蚀刻剂。 第二实施例使用双层侧壁保护,其中第一层覆盖存储元件优选是无氧电介质,并且第二层在通孔蚀刻期间保护第一层。
    • 5. 发明申请
    • MRAM Fabrication Method with Sidewall Cleaning
    • MRAM制造方法与侧壁清洁
    • US20130267042A1
    • 2013-10-10
    • US13443818
    • 2012-04-10
    • Kimihiro SatohYiming HuaiYuchen ZhouJing ZhangDong Ha JungEbrahim AbedifardRajiv Yadav RanjanParviz Keshtbod
    • Kimihiro SatohYiming HuaiYuchen ZhouJing ZhangDong Ha JungEbrahim AbedifardRajiv Yadav RanjanParviz Keshtbod
    • H01L21/02
    • H01L27/222H01L43/12
    • Fabrication methods for MRAM are described wherein any re-deposited metal on the sidewalls of the memory element pillars is cleaned before the interconnection process is begun. In embodiments the pillars are first fabricated, then a dielectric material is deposited on the pillars over the re-deposited metal on the sidewalls. The dielectric material substantially covers any exposed metal and therefore reduces sources of re-deposition during subsequent etching. Etching is then performed to remove the dielectric material from the top electrode and the sidewalls of the pillars down to at least the bottom edge of the barrier. The result is that the previously re-deposited metal that could result in an electrical short on the sidewalls of the barrier is removed. Various embodiments of the invention include ways of enhancing or optimizing the process. The bitline interconnection process proceeds after the sidewalls have been etched clean as described.
    • 描述了用于MRAM的制造方法,其中在互连过程开始之前清洁存储元件柱的侧壁上的任何重新沉积的金属。 在实施例中,首先制造柱,然后将介电材料沉积在侧壁上的再沉积金属上的柱上。 电介质材料基本上覆盖任何暴露的金属,因此在随后的蚀刻期间减少再沉积的来源。 然后进行蚀刻以将电介质材料从顶部电极和柱的侧壁向下移动到至少阻挡层的底部边缘。 结果是可能导致在屏障的侧壁上导致电短路的先前重新沉积的金属被去除。 本发明的各种实施方案包括增强或优化方法的方法。 如所描述的那样,在侧壁被蚀刻清洁之后,进行位线互连处理。
    • 6. 发明申请
    • Mram etching processes
    • 摩擦蚀刻工艺
    • US20130052752A1
    • 2013-02-28
    • US13199490
    • 2011-08-30
    • Kimihiro SatohYiming HuaiJing ZhangRajiv Yadav RanjanParviz KeshtbodRoger K. Malmhall
    • Kimihiro SatohYiming HuaiJing ZhangRajiv Yadav RanjanParviz KeshtbodRoger K. Malmhall
    • H01L21/8246
    • H01L43/12H01L29/00
    • Various embodiments of the invention relate to etching processes used in fabrication of MTJ cells in an MRAM device. The various embodiments can be used in combination with each other. The first embodiment adds a hard mask buffer layer between a hard mask and a top electrode. The second embodiment uses a multilayered etching hard mask. The third embodiment uses a multilayered top electrode structure including a first Cu layer under a second layer such as Ta. The fourth embodiment is a two-phase etching process used for the bottom electrode to remove re-deposited material while maintaining a more vertical sidewall etching profile. In the first phase the bottom electrode layer is removed using carbonaceous reactive ion etching until the endpoint. In the second phase an inert gas and/or oxygen plasma is used to remove the polymer that was deposited during the previous etching processes.
    • 本发明的各种实施例涉及用于制造MRAM装置中的MTJ电池的蚀刻工艺。 各种实施例可以彼此组合使用。 第一实施例在硬掩模和顶电极之间添加硬掩模缓冲层。 第二实施例使用多层蚀刻硬掩模。 第三实施例使用包括第二层如Ta之下的第一Cu层的多层顶电极结构。 第四实施例是用于底部电极去除再沉积材料同时保持更垂直侧壁蚀刻轮廓的两相蚀刻工艺。 在第一阶段中,使用碳质反应离子蚀刻去除底部电极层直到端点。 在第二阶段中,使用惰性气体和/或氧等离子体去除在先前蚀刻工艺期间沉积的聚合物。
    • 9. 发明申请
    • MTJ MRAM WITH STUD PATTERNING
    • MTJ MRAM与STUD PATTERNING
    • US20140042567A1
    • 2014-02-13
    • US13572197
    • 2012-08-10
    • Dong Ha JungKimihiro SatohJing ZhangYuchen ZhouYiming Huai
    • Dong Ha JungKimihiro SatohJing ZhangYuchen ZhouYiming Huai
    • H01L43/12H01L43/02
    • H01L43/12H01L43/08
    • Use of a multilayer etching mask that includes a stud mask and a removable spacer sleeve for MTJ etching to form a bottom electrode that is wider than the rest of the MTJ pillar is described. The first embodiment of the invention described includes a top electrode and a stud mask. In the second and third embodiments the stud mask is a conductive material and also serves as the top electrode. In embodiments after the stud mask is formed a spacer sleeve is formed around it to initially increase the masking width for a phase of etching. The spacer is removed for further etching, to create step structures that are progressively transferred down into the layers forming the MTJ pillar. In one embodiment the spacer sleeve is formed by net polymer deposition during an etching phase.
    • 描述了包括螺柱掩模和用于MTJ蚀刻以形成比MTJ柱的其余部分宽的底部电极的可移除间隔套的多层蚀刻掩模的使用。 所描述的本发明的第一实施例包括顶部电极和螺柱掩模。 在第二和第三实施例中,螺柱掩模是导电材料,并且还用作顶部电极。 在形成螺柱掩模之后的实施例中,在其周围形成间隔套,以最初增加蚀刻阶段的掩模宽度。 去除间隔物用于进一步蚀刻,以产生逐渐转移到形成MTJ柱的层中的阶梯结构。 在一个实施例中,间隔套筒是在蚀刻阶段期间通过净聚合物沉积形成的。
    • 10. 发明授权
    • MRAM fabrication method with sidewall cleaning
    • MRAM制造方法与侧壁清洁
    • US08574928B2
    • 2013-11-05
    • US13443818
    • 2012-04-10
    • Kimihiro SatohYiming HuaiYuchen ZhouJing ZhangDong Ha JungEbrahim AbedifardRajiv Yadav RanjanParviz Keshtbod
    • Kimihiro SatohYiming HuaiYuchen ZhouJing ZhangDong Ha JungEbrahim AbedifardRajiv Yadav RanjanParviz Keshtbod
    • H01L21/00
    • H01L27/222H01L43/12
    • Fabrication methods for MRAM are described wherein any re-deposited metal on the sidewalls of the memory element pillars is cleaned before the interconnection process is begun. In embodiments the pillars are first fabricated, then a dielectric material is deposited on the pillars over the re-deposited metal on the sidewalls. The dielectric material substantially covers any exposed metal and therefore reduces sources of re-deposition during subsequent etching. Etching is then performed to remove the dielectric material from the top electrode and the sidewalls of the pillars down to at least the bottom edge of the barrier. The result is that the previously re-deposited metal that could result in an electrical short on the sidewalls of the barrier is removed. Various embodiments of the invention include ways of enhancing or optimizing the process. The bitline interconnection process proceeds after the sidewalls have been etched clean as described.
    • 描述了用于MRAM的制造方法,其中在互连过程开始之前清洁存储元件柱的侧壁上的任何重新沉积的金属。 在实施例中,首先制造柱,然后将介电材料沉积在侧壁上的再沉积金属上的柱上。 电介质材料基本上覆盖任何暴露的金属,因此在随后的蚀刻期间减少再沉积的来源。 然后进行蚀刻以将电介质材料从顶部电极和柱的侧壁向下移动到至少阻挡层的底部边缘。 结果是可能导致在屏障的侧壁上导致电短路的先前重新沉积的金属被去除。 本发明的各种实施方案包括增强或优化方法的方法。 如所描述的那样,在侧壁被蚀刻清洁之后,进行位线互连处理。