    • 2. 发明授权
    • Method for preparing dialkylnaphthalene
    • 制备二烷基萘的方法
    • US5365001A
    • 1994-11-15
    • US39067
    • 1993-04-08
    • Koji SumitaniKeizo ShimadaSeiji ItohKimihiko SatoRisuke SuzukiAkio Namatame
    • Koji SumitaniKeizo ShimadaSeiji ItohKimihiko SatoRisuke SuzukiAkio Namatame
    • B01J23/60B01J23/62C07C5/41C07C5/00C07C15/24
    • B01J23/62B01J23/60C07C5/41
    • A method for preparing a dialkylnaphthalene in one step by contacting an dialkylbenzene compound with a solid catalyst in a gas or liquid phase in the presence of hydrogen, using a catalyst having composition (I) or (II) below:(1)(M.sup.1).sub.a.(M.sup.2).sub.b.(SiO.sub.2.XAl.sub.2 O.sub.3).(Al.sub.2 O.sub.3).sub.c (I)(2) Mixture of II-(i) and II-(ii):(M.sup.3).sub.d.(Al.sub.2 O.sub.3) II-(i)(M.sup.4).sub.e.(SiO.sub.2.XAl.sub.2 O.sub.3) II-(ii)wherein M.sup.1 is a metal selected from the group consisting of metals belonging to group VIII of a periodic table and rhenium;M.sup.2 is a member selected from the group consisting of zinc, gallium, and oxides thereof;M.sup.3 is a metal belonging to group VIII of a periodic table;M.sup.4 is at least one alkali metal; anda, b, c, d, e, and X represent proportions, respectively.
    • PCT No.PCT / JP92 / 01006 Sec。 371日期:1993年4月8日 102(e)日期1993年4月8日PCT提交1992年8月6日PCT公布。 公开号WO93 / 02995 日本2月18日,1993年。一种通过使用具有下述组成(I)或(II)的催化剂在氢气存在下,在气相或液相中使二烷基苯化合物与固体催化剂接触的步骤中制备二烷基萘的方法。 :(1)(M1)a。(M2)b。(SiO2.XAl2O3)(Al2O3)c(I)(2)II-(i)和II-(ii)的混合物:(M3)d。 Al 2 O 3)II-(i)(M4)e。(SiO 2·XAl 2 O 3)II-(ii)其中M1是选自属于元素周期表第Ⅷ族的金属和铼的金属; M2是选自锌,镓及其氧化物的成员; M3是属于周期表第VIII族的金属; M4是至少一种碱金属; 和a,b,c,d,e和x分别表示比例。
    • 7. 发明授权
    • Aromatic polyamide composition and processes for preparing film and
fiber therefrom
    • 芳族聚酰胺组合物及其制备薄膜和纤维的方法
    • US4529763A
    • 1985-07-16
    • US482817
    • 1983-04-07
    • Yorikazu TamuraAkihiro AokiKeizo Shimada
    • Yorikazu TamuraAkihiro AokiKeizo Shimada
    • C08L77/00C08K3/16C08L77/10C08K5/20
    • C08K3/16C08K3/24C08K5/20
    • There is provided an aromatic polyamide composition, which comprises (a) a polyamide, the recurring structural units of which are substantially totally aromatic, (b) an organic amide solvent, and (c) one or more salts selected from chlorides and bromides of an alkali metal, an alkaline earth metal or ammonium. The amounts of the polyamide and the organic amide solvent are in the ranges of 30 to 50% and 70 to 50% by weight, respectively, based on the total weight of the polyamide and the organic amide solvent. The amount of the salt is defined by the formulae:in the case where 30.ltoreq.x.ltoreq.33.6, y.gtoreq.10, andin the case where 33.6 2.8x-84wherein "x" is the amount in % by weight of the polyamide based on the total weight of the polyamide and the organic amide solvent, and "y" is the amount in % by mole of the salt based on the polyamide. The polyamide composition is useful for melt-shaping films, fibers and other shaped articles.
    • 提供了一种芳族聚酰胺组合物,其包含(a)聚酰胺,其重复结构单元基本上是全芳族的,(b)有机酰胺溶剂,和(c)一种或多种选自氯化物和溴化物的盐 碱金属,碱土金属或铵。 基于聚酰胺和有机酰胺溶剂的总重量,聚酰胺和有机酰胺溶剂的量分别为30-50%和70-50wt%。 盐的量由下式定义:在30 / = 10的情况下,在33.6 2.8×-84 其中“x”是聚酰胺的重量百分比(以聚酰胺和有机酰胺溶剂的总重量计),“y”是以聚酰胺为基准的盐的摩尔%。 聚酰胺组合物可用于熔融成型薄膜,纤维和其它成型制品。