    • 2. 发明授权
    • Method for producing coated steel sheet
    • 涂层钢板的制造方法
    • US08709550B2
    • 2014-04-29
    • US10502670
    • 2003-01-24
    • Yuka KomoriMasaki KawanoKazumichi SashiAkio Fujita
    • Yuka KomoriMasaki KawanoKazumichi SashiAkio Fujita
    • B05D5/06
    • C23C22/74B05D3/0209B05D7/14B05D2202/10C21D8/0284C21D8/0484C21D8/1233C21D8/1283H01F1/14725H01F1/18
    • In a process for manufacturing a coated steel sheet such as a coated electromagnetic steel sheet using a water-based coating liquid containing an organic resin, to perform steps subsequent to an annealing step continuously at high speed without causing appearance defects such as coating unevenness; to provide an electromagnetic steel sheet having an insulating film thereon, in which properties of the film are satisfactory, superior weldability and punchability can be obtained without deteriorating the space factor, and the satisfactory film properties can be maintained even if the electromagnetic steel sheet having the insulating film thereon is temper-rolled. A coating liquid is applied onto an untreated steel sheet. The applied liquid is heated on the side close to the steel sheet in such a manner that the time elapsed until the steel sheet temperature is increased to 100° C. after the application is completed is 10 seconds or less, thereby drying the coating liquid. The steel sheet temperature is further increased to a predetermined temperature, thereby forming a coating film. When insulating films for electromagnetic steel sheets are formed, the coating liquid preferably further contains a water based inorganic component.
    • 在使用含有有机树脂的水性涂布液的涂布电磁钢板的涂布钢板的制造方法中,高速连续地进行退火工序后的工序,不会引起涂布不均匀等的外观缺陷; 为了提供一种其上具有绝缘膜的电磁钢板,其中膜的性能令人满意,可以获得优异的焊接性和冲压性,而不会使空间因素变差,并且即使电磁钢板具有 对其上的绝缘膜进行回火。 将涂布液施加到未处理的钢板上。 所施加的液体在靠近钢板的一侧被加热,使得在施加完成之后直到钢板温度升高到100℃的时间为10秒以下,从而使涂布液干燥。 钢板温度进一步提高到预定温度,从而形成涂膜。 当形成用于电磁钢板的绝缘膜时,涂布液优选还含有水基无机组分。
    • 3. 发明申请
    • Method for producing coated steel sheet
    • 涂层钢板的制造方法
    • US20050064107A1
    • 2005-03-24
    • US10502670
    • 2003-01-24
    • Yuka KomoriMasaki KawanoKazumichi SashiAkio Fujita
    • Yuka KomoriMasaki KawanoKazumichi SashiAkio Fujita
    • B05D3/02B05D7/14C21D8/02C21D8/04C21D8/12C23C22/74H01F1/147H01F1/18
    • C23C22/74B05D3/0209B05D7/14B05D2202/10C21D8/0284C21D8/0484C21D8/1233C21D8/1283H01F1/14725H01F1/18
    • In a process for manufacturing a coated steel sheet such as a coated electromagnetic steel sheet using a water-based coating liquid containing an organic resin, to perform steps subsequent to an annealing step continuously at high speed without causing appearance defects such as coating unevenness; to provide an electromagnetic steel sheet having an insulating film thereon, in which properties of the film are satisfactory, superior weldability and punchability can be obtained without deteriorating the space factor, and the satisfactory film properties can be maintained even if the electromagnetic steel sheet having the insulating film thereon is temper-rolled. A coating liquid is applied onto an untreated steel sheet. The applied liquid is heated on the side close to the steel sheet in such a manner that the time elapsed until the steel sheet temperature is increased to 100° C. after the application is completed is 10 seconds or less, thereby drying the coating liquid. The steel sheet temperature is further increased to a predetermined temperature, thereby forming a coating film. When insulating films for electromagnetic steel sheets are formed, the coating liquid preferably further contains a water based inorganic component.
    • 在使用含有有机树脂的水性涂布液的涂布电磁钢板的涂布钢板的制造方法中,高速连续地进行退火工序后的工序,不会引起涂布不均匀等的外观缺陷; 为了提供一种其上具有绝缘膜的电磁钢板,其中膜的性能令人满意,可以获得优异的焊接性和冲压性,而不会使空间因素变差,并且即使具有 对其上的绝缘膜进行回火。 将涂布液施加到未处理的钢板上。 所施加的液体在靠近钢板的一侧被加热,使得在施加完成之后直到钢板温度升高到100℃的时间为10秒以下,从而使涂布液干燥。 钢板温度进一步提高到预定温度,从而形成涂膜。 当形成用于电磁钢板的绝缘膜时,涂布液优选还含有水基无机组分。