    • 10. 发明授权
    • Method for producing a glass thin film with controlloing an oxide vapor
of an additive
    • 用添加剂的氧化物蒸气调制玻璃薄膜的方法
    • US5503650A
    • 1996-04-02
    • US330602
    • 1994-10-28
    • Shinji IshikawaAkira UranoHaruhiko AikawaChizai HiroseHiroo KanamoriMasahide Saitoh
    • Shinji IshikawaAkira UranoHaruhiko AikawaChizai HiroseHiroo KanamoriMasahide Saitoh
    • C03B19/14C03C17/00C03C17/02C23C14/10C23C16/44C23C16/453C03B37/018
    • C03B19/1453C03B19/14C03B19/1415C03C17/001C03C17/02C23C14/10C23C16/44C23C16/453C03B2207/90
    • A method of producing an oxide glass thin film includes a process to obtain a transparent glass film, in which volatilization of additives in a porous film deposited is effectively suppressed and which can provide an oxide glass thin film having a desired arrangement of refractive index with a low optical loss. The method is for producing an oxide glass thin film, in which glass fine particles mainly containing SiO.sub.2 with additives are deposited on a substrate to form a porous thin film and then heated to form a transparent glass film. In the method, vapor of oxides of additive components is mixed in an atmosphere in which the porous thin film is heated to form the transparent glass film, whereby stopping the volatilization of the additives in the porous film deposited, preventing diffusion of the additives added to a core layer, and preventing the volatilization of glass transition temperature lowering components of additives (P.sub.2 O.sub.5, B.sub.2 O.sub.3, GeO.sub.2, etc.). By these, a desired arrangement of refractive index may be obtained, and an oxide glass thin film may be obtained while lowering the optical loss such as the optical scattering, which could be caused by bubbles in an unsintered portion.
    • 制造氧化物玻璃薄膜的方法包括获得透明玻璃膜的方法,其中有效地抑制了沉积的多孔膜中的添加剂的挥发,并且可以提供具有期望的折射率布置的氧化物玻璃薄膜 光损耗低。 该方法用于生产氧化物玻璃薄膜,其中主要含有SiO 2的玻璃微粒子添加剂沉积在基底上以形成多孔薄膜,然后加热形成透明玻璃膜。 在该方法中,添加成分的氧化物蒸气在多孔薄膜被加热的气氛中混合,形成透明玻璃膜,由此停止多孔膜中的添加剂的挥发,防止添加添加剂的扩散 核心层,并且防止添加剂(P 2 O 5,B 2 O 3,GeO 2等)的玻璃化转变温度降低成分的挥发。 通过这些,可以获得期望的折射率布置,并且可以在降低可能由未烧结部分中的气泡引起的光学散射等光损耗的同时获得氧化物玻璃薄膜。