    • 1. 发明授权
    • Apparatus for recovering flatness of web material
    • 用于回收纤维网材料的平整度的装置
    • US6065955A
    • 2000-05-23
    • US221845
    • 1998-12-29
    • Daisuke FujikuraNaoaki Suzuki
    • Daisuke FujikuraNaoaki Suzuki
    • B29C71/02B29B13/02B29C35/08B29C53/18B29L7/00B29C35/10
    • B29C53/18B29B13/023B29C2035/0822B29C35/0805B29K2067/00
    • The present invention provides a method for recovering flatness of a web material which comprises heating a side edge portion of the web material at a temperature in a range from a glass transition temperature minus 40.degree. C. to a melting point of the web material for a period of from 1 to 600 seconds, and an apparatus for recovering flatness of a web material which comprises a plurality of conveying rollers for conveying the web material and a side edge portion heating means which surrounds and heats the side edge portion of the web material traveling through conveying rollers. According to the method and apparatus, the side edge portion(s) elongated by the previous heat treatment is recovered to a state similar to the central portion by reheating to correct the side edge portion(s), and thereby, flatness of the web material can be improved.
    • 本发明提供一种回收纤维网材料的平整度的方法,该方法包括将幅材材料的侧边缘部分在玻璃化转变温度为-40℃的温度范围内加热至网状材料的熔点 时间为1至600秒,以及用于回收幅材材料的平整度的装置,其包括用于输送幅材材料的多个输送辊和围绕并加热幅材材料行进的侧边缘部分的侧边缘部分加热装置 通过输送辊。 根据该方法和装置,通过再加热将通过先前的热处理延伸的侧边缘部分恢复到与中心部分相似的状态,以校正侧边缘部分,从而使幅材材料的平整度 可以改进。
    • 3. 发明授权
    • Method for recovering flatness of web material and apparatus therefor
    • 用于回收网材料的平整度的方法及其装置
    • US5879606A
    • 1999-03-09
    • US598216
    • 1996-02-07
    • Daisuke FujikuraNaoaki Suzuki
    • Daisuke FujikuraNaoaki Suzuki
    • B29C71/02B29B13/02B29C35/08B29C53/18B29L7/00B29C61/00
    • B29C53/18B29B13/023B29C2035/0822B29C35/0805B29K2067/00
    • The present invention provides a method for recovering flatness of a web material which comprises heating a side edge portion of the web material at a temperature in a range from a glass transition temperature minus 40.degree. C. to a melting point of the web material for a period of from 1 to 600 seconds, and an apparatus for recovering flatness of a web material which comprises a plurality of conveying rollers for conveying the web material and a side edge portion heating means which surrounds and heats the side edge portion of the web material traveling through conveying rollers. According to the method and apparatus, the side edge portion(s) elongated by the previous heat treatment is recovered to a state similar to the central portion by reheating to correct the side edge portion(s), and thereby, flatness of the web material can be improved.
    • 本发明提供一种回收纤维网材料的平整度的方法,该方法包括将幅材材料的侧边缘部分在玻璃化转变温度为-40℃的温度范围内加热至网状材料的熔点 时间为1至600秒,以及用于回收幅材材料的平整度的装置,其包括用于输送幅材材料的多个输送辊和围绕并加热幅材材料行进的侧边缘部分的侧边缘部分加热装置 通过输送辊。 根据该方法和装置,通过再加热将通过先前的热处理延伸的侧边缘部分恢复到与中心部分相似的状态,以校正侧边缘部分,从而使幅材材料的平整度 可以改进。
    • 6. 发明授权
    • Method of preforming heat treatment on a wound roll film
    • 对卷绕的卷膜进行热处理的方法
    • US5634789A
    • 1997-06-03
    • US365364
    • 1994-12-28
    • Takashi NawanoDaisuke FujikuraOsamu Nagayama
    • Takashi NawanoDaisuke FujikuraOsamu Nagayama
    • B29C35/04B29C71/02G03C1/795G03C1/76
    • B29C71/02G03C1/795B29C2071/022B29C35/045B29K2067/00
    • Knurling is applied to both side edge portions of a high-molecular film and then the film is wound up. A packing agent is applied to the knurled portions to enclose air at the time of winding in spaces between wound film layers and the film is put into an annealing isothermal chamber while contact between the wound film layers is prevented by the air. Preferably, the high-molecular film is made to pass through a heating zone just before the winding so that the high-molecular film after heated is wound up. More preferably, the winding core used for winding is a hollow porous winding core and high-temperature pressurized air is blown out onto the film through the hollow porous cylindrical surface. In a method of performing heat treatment on a wound roll film in which annealing treatment is performed on a roll film obtained by winding a high-molecular film, comprising the steps of: enclosing a winding portion of a device in a box; keeping the inside of the box at a high temperature equal to that of an annealing chamber; heating the high-molecular film to a temperature equal to the temperature of the inside of the box just before winding and then winding the high-molecular film; and conveying the high-molecular film into an isothermal chamber for annealing treatment.
    • 将滚花应用于高分子膜的两侧缘部分,然后将膜卷起。 将包装剂施加到滚花部分,以在缠绕膜卷层之间的空间中包围空气,并且将薄膜放入退火等温室中,同时通过空气防止卷绕膜层之间的接触。 优选地,使高分子膜在卷绕之前通过加热区,使得加热后的高分子膜被卷起。 更优选地,用于卷绕的卷芯是中空多孔卷芯,并且高温加压空气通过中空多孔圆柱形表面吹出到膜上。 在对通过卷绕高分子膜获得的辊膜进行退火处理的卷绕辊膜上进行热处理的方法中,包括以下步骤:将装置的卷绕部分封闭在盒中; 将箱体内部保持在与退火室相同的高温下; 在卷绕之前将高分子膜加热到等于盒内部温度的温度,然后卷绕高分子膜; 并将高分子膜输送到用于退火处理的等温室中。