    • 1. 发明申请
    • METHOD FOR PRODUCING SHEET METAL PART AND A FORMING TOOL
    • 用于生产薄片金属部件和成形工具的方法
    • US20120192611A1
    • 2012-08-02
    • US13361672
    • 2012-01-30
    • Christian HielscherOtto Buschsieweke
    • Christian HielscherOtto Buschsieweke
    • B21B15/00B21D37/10B21D37/16
    • B21D35/006B21D22/02
    • In a method for producing a sheet metal part, a sheet metal blank is rolled to have at least two regions of different material thickness to define a thick region and a thin region, with a thickness profile of the sheet metal blank extending in substantial symmetric relationship to a central plane of the sheet metal blank. The sheet metal blank is inserted into a forming tool having a punch and a die and a punch-proximal side of the sheet metal blank is contacted with a pressing cam formed on the punch. The sheet metal blank is formed into the sheet metal part by pressing the punch against the die and thereby forming an embossment by a die cam provided on the die on a die-proximal side of the sheet metal part.
    • 在制造钣金件的方法中,将金属板坯材轧制成具有不同材料厚度的至少两个区域以限定厚的区域和薄区域,其中金属片坯料的厚度分布呈基本对称关系 到金属板坯的中心平面。 将金属板坯插入到具有冲头和模具的成形工具中,并且金属板坯料的冲头近侧侧与形成在冲头上的按压凸轮接触。 通过将冲头压靠在模具上而将金属板坯件形成为金属板坯件,从而通过设置在模具上的模具凸轮在金属板零件的模具近侧形成压纹。
    • 9. 发明申请
    • METHOD OF MAKING A SHAPED METAL PART FOR A MOTOR VEHICLE COMPONENT
    • 制造汽车部件的形状金属部件的方法
    • US20120023748A1
    • 2012-02-02
    • US13007065
    • 2011-01-14
    • MARTIN POHLOtto BuschsiewekeStefan Adelbert
    • MARTIN POHLOtto BuschsiewekeStefan Adelbert
    • B21D53/88H05B6/10B21D37/16
    • C21D1/25C21D1/32C21D8/02C21D8/04C21D9/48C22C1/02Y10T29/49622
    • In a method of making a shaped metal part for a motor vehicle component, a blank is made from a steel alloy containing, in weight percent: carbon (C) 0.18% to 0.3%, silicon (Si) 0.1% to 0.7%, manganese (Mn) 1.0% to 2.5%, phosphorus (P) maximal 0.025%, chromium (Cr) 0.1 to 0.8%, molybdenum (Mo) 0.1 to 0.5%, sulfur (S) maximal 0.01%, titanium (Ti) 0.02% to 0.05%, boron (B) 0.002% to 0.005%, aluminum (Al) 0.01% to 0.06%, balance iron and impurities resulting from smelting, The blank is heated to a temperature between 900° C. and 950° C., and formed in a press tool into a formed part which is quenched and tempered while still being in the press tool. At least one region of the formed part is then annealed to become soft by a heating operation within a time interval of less than 30 seconds to thereby provide the region with higher ductility.
    • 在制造机动车用部件的成形金属部件的方法中,坯料由钢合金制成,所述钢合金含有重量百分比:碳(C)0.18%〜0.3%,硅(Si)0.1%〜0.7%,锰 (Mn)1.0%〜2.5%,磷(P)最大0.025%,铬(Cr)0.1〜0.8%,钼(Mo)0.1〜0.5%,硫(S)最大0.01%,钛(Ti)0.02% 0.05%,硼(B)0.002%〜0.005%,铝(Al)0.01〜0.06%,铁和杂质产生的杂质,将坯料加热至900〜950℃, 在冲压工具中形成为在仍处于压制工具中的淬火和回火的成形部件。 然后通过在小于30秒的时间间隔内的加热操作将成形部件的至少一个区域退火以变软,从而为该区域提供更高的延展性。