    • 1. 发明授权
    • Coating composition and film system therefrom
    • 涂料组合物和薄膜体系
    • US07807743B2
    • 2010-10-05
    • US11534352
    • 2006-09-22
    • Marvin L GreenDonald H. CampbellJohn E. BoisseauBruce Oermann
    • Marvin L GreenDonald H. CampbellJohn E. BoisseauBruce Oermann
    • C09B67/00
    • C08J7/18C08J2377/12
    • A coating composition is used to form a clearcoat layer of a film system including a basecoat layer and the clearcoat layer. The coating composition includes a carbamate functional polymer, a cross-linking agent reactive with the carbamate functional polymer, and an acid functional polymer substantially non-reactive with the carbamate functional polymer and the cross-linking agent. The acid functional polymer has an acid value of at least 50 mg KOH/g and contributes to an increased resistance to acid etch of the clearcoat layer. The acid functional polymer also contributes to an increased intercoat adhesion of the basecoat layer and the clearcoat layer thereby decreasing a possibility of separation/delamination of the basecoat layer and the clearcoat layer.
    • 涂料组合物用于形成包括底涂层和透明涂层的膜系统的透明涂层。 涂料组合物包括氨基甲酸酯官能聚合物,与氨基甲酸酯官能聚合物反应的交联剂和与氨基甲酸酯官能聚合物和交联剂基本上不反应的酸官能聚合物。 酸官能聚合物具有至少50mg KOH / g的酸值,并且有助于增加对透明涂层的酸蚀刻的耐受性。 酸官能聚合物还有助于增加底涂层和透明涂层的层间粘附性,从而降低了底涂层和透明涂层的分离/分层的可能性。
    • 4. 发明授权
    • Plasticizing component and a curable coating composition including the same
    • 增塑组分和包含其的可固化涂料组合物
    • US07772304B2
    • 2010-08-10
    • US11560932
    • 2006-11-17
    • Walter H. OhrbomJohn E. Boisseau
    • Walter H. OhrbomJohn E. Boisseau
    • C08K5/3492C07D251/30
    • C09D133/066C09D133/14
    • A curable coating composition includes a plasticizing component. The plasticizing component includes an isocyanurate core and at least one low surface tension group pending from the isocyanurate core. The low surface tension group may be a) a fatty chain includes at least 6 carbon atoms, b) a silicon-containing group having at least 1 silicon atom, c) a fluorocarbon, and combinations thereof. The low surface tension group may have cross-linkable functional groups pending therefrom. In addition to the plasticizing component, the curable coating composition further includes a resin component and a crosslinking agent that is reactive with the resin component. The curable coating composition including the plasticizing component is capable of forming a cured film that has resistance to both cracking and etching that, to date, has not been achieved with known plasticizing components.
    • 可固化涂料组合物包括增塑组分。 增塑组分包括异氰脲酸酯芯和至少一种从异氰脲酸酯芯悬浮的低表面张力组。 低表面张力基团可以是a)脂肪链包含至少6个碳原子,b)具有至少1个硅原子的含硅基团,c)碳氟化合物及其组合。 低表面张力组可能具有可交联的官能团。 除了增塑组分之外,可固化涂料组合物还包括树脂组分和与树脂组分反应的交联剂。 包含增塑组分的可固化涂料组合物能够形成耐开裂和蚀刻的固化膜,迄今为止,已知的增塑组分尚未实现。
    • 5. 发明申请
    • PLASTICIZING COMPONENT AND A CURABLE COATING COMPOSITION INCLUDING THE SAME
    • 塑化组分和可固化的涂料组合物,包括它们
    • US20080119592A1
    • 2008-05-22
    • US11560932
    • 2006-11-17
    • Walter H. OhrbomJohn E. Boisseau
    • Walter H. OhrbomJohn E. Boisseau
    • C08K5/3492C07D251/30
    • C09D133/066C09D133/14
    • A curable coating composition includes a plasticizing component. The plasticizing component includes an isocyanurate core and at least one low surface tension group pending from the isocyanurate core. The low surface tension group may be a) a fatty chain includes at least 6 carbon atoms, b) a silicon-containing group having at least 1 silicon atom, c) a fluorocarbon, and combinations thereof. The low surface tension group may have cross-linkable functional groups pending therefrom. In addition to the plasticizing component, the curable coating composition further includes a resin component and a crosslinking agent that is reactive with the resin component. The curable coating composition including the plasticizing component is capable of forming a cured film that has resistance to both cracking and etching that, to date, has not been achieved with known plasticizing components.
    • 可固化涂料组合物包括增塑组分。 增塑组分包括异氰脲酸酯芯和至少一种从异氰脲酸酯芯悬浮的低表面张力组。 低表面张力基团可以是a)脂肪链包含至少6个碳原子,b)具有至少1个硅原子的含硅基团,c)碳氟化合物及其组合。 低表面张力组可能具有可交联的官能团。 除了增塑组分之外,可固化涂料组合物还包括树脂组分和与树脂组分反应的交联剂。 包含增塑组分的可固化涂料组合物能够形成耐开裂和蚀刻的固化膜,迄今为止,已知的增塑组分尚未实现。