    • 4. 发明授权
    • PET yarns with improved loop tensile properties
    • 具有改善环路拉伸性能的PET纱线
    • US08025969B2
    • 2011-09-27
    • US12289118
    • 2008-10-21
    • Heping ZhangCraig Valentine
    • Heping ZhangCraig Valentine
    • D02G3/00D03D15/00
    • D01F6/62D01D5/16D02G3/447D21F1/0027D21F1/0054Y10T428/2913Y10T428/2933Y10T428/298Y10T442/3146Y10T442/608
    • Poly(ethylene terephthalate) monofilaments having improved loop strength and toughness as well as improved tensile strength and tensile toughness. The yarns can have a loop toughness of at least 2 gf/den, a loop tenacity of at least 7 gf/den, a tensile toughness of at least 0.9 gf/den, a tensile tenacity of at least 4 gf/den, and a DSC crystallinity of at least 35%. A process for the production of poly(ethylene terephthalate) monofilaments includes melt extrusion, orientation of the extrudates by stretching, and further stretching as well as heat treating the stretched monofilaments. Industrial fabrics, especially fabrics for paper machine clothing, can be made of such monofilaments as load bearing yarns that resist loop failure and that resist fabric creep at high temperature and high load.
    • 具有改善的环路强度和韧性以及改进的拉伸强度和拉伸韧性的聚对苯二甲酸乙二醇酯单丝。 纱线的回弹韧性至少为2gf / den,环韧度至少为7gf / den,拉伸韧度至少为0.9gf / den,拉伸强度至少为4gf /,,以及 DSC结晶度至少为35%。 聚(对苯二甲酸乙二醇酯)单丝的制造方法包括熔融挤出,挤出物的拉伸取向,进一步拉伸以及热处理拉伸的单丝。 工业织物,特别是造纸机服装的织物,可以由耐受环路故障的承重纱线和耐高温高负载下的织物蠕变的单丝制成。
    • 7. 发明申请
    • TOUGHENED MONOFILAMENTS
    • 加强单一伪装
    • US20080182938A1
    • 2008-07-31
    • US11627082
    • 2007-01-25
    • Heping ZhangCraig Valentine
    • Heping ZhangCraig Valentine
    • C08L77/00
    • D01F6/90
    • A method of forming a monofilament or a technical fiber for use in a press felt of a papermaking machine including the steps of selecting polyamide 66, selecting polyamide 6/66, blending and forming a monofilaments. An amount of polyamide selected by weight of approximately 60-95% of a total weight. An amount of polyamide 6/66 copolymer is selected by weight in an amount of approximately 5% to 40% of the total weight. The polyamide 66 and polyamide 6/66 copolymer are blended, thereby defining a blended material. The monofilament or technical fiber is formed from the blended material.
    • 一种形成用于造纸机的压榨毛毯的单丝或工业纤维的方法,包括选择聚酰胺66,选择聚酰胺6/66,共混和形成单丝的步骤。 一定量的聚酰胺选自重量的总重量的约60-95%。 聚酰胺6/66共聚物的量以总重量的约5%至40%的量选择。 混合聚酰胺66和聚酰胺6/66共聚物,从而限定混合材料。 单丝或技术纤维由混合材料形成。