    • 77. 发明授权
    • Partially crosslinked plastics materials of propylene copolymers
    • 丙烯共聚物的部分交联塑料材料
    • US5371144A
    • 1994-12-06
    • US025861
    • 1993-03-03
    • Sibylle BrosiusHarald SchwagerSusanne HahnBernd L. Marczinke
    • Sibylle BrosiusHarald SchwagerSusanne HahnBernd L. Marczinke
    • C08F8/42C08F255/00C08F8/00
    • C08F8/42C08F255/00
    • Partially crosslinked plastics materials having a melt flow index of from 0.1 to 100 g/10 min at 230.degree. C. and under a weight of 2.16 kg, containinga) a polymer of from 25 to 97% by weight of a propylene copolymer (I) which contains from 0.1 to 15% by weight of polymerized C.sub.2 -C.sub.10 -alk-1-enes and of from 3 to 75% by weight of a further propylene copolymer (II) which contains from 15 to 80% by weight of polymerized C.sub.2 -C.sub.10 -alk-1-enes andb) an organosilane compound of the following formula (I)A.sub.4-n SiR.sub.n (I)where the radicals A are identical or different and are each an acrylate or methacrylate or vinyl, the radicals R are identical or different and are each C.sub.1 -C.sub.8 -alkoxy or C.sub.1 -C.sub.8 -acetoxy and n is 1, 2 or 3,are obtainable by reacting the polymer a) with the organosilane compound b) in the presence of a free radical initiator and a condensation catalyst at from 180 to 280.degree. C. and from 1 to 100 bar and in the course of average residence times of the reaction mixture of from 0.2 to 10 minutes.The novel plastics materials have in particular improved processibility and thermoformability, a lower sealing temperature and better white fracture behavior.
    • 在230℃和2.16kg重量下熔体流动指数为0.1-100g / 10min的部分交联塑料材料,其包含a)25至97重量%的丙烯共聚物(I ),其含有0.1至15重量%的聚合的C 2 -C 10 - 烷-1-烯和3至75重量%的另外的丙烯共聚物(II),其含有15至80重量%的聚合的C 2 -C 10 - 烷-1-烯和b)下式(I)的有机硅烷化合物,其中基团A相同或不同,各自为丙烯酸酯或甲基丙烯酸酯或乙烯基,其中基团R是相同的 或不同的,并且各自为C 1 -C 8 - 烷氧基或C 1 -C 8 - 乙酰氧基且n为1,2或3,可通过使聚合物a)与有机硅烷化合物b)在自由基引发剂和缩合物 催化剂为180-280℃和1-100巴,反应混合物的平均停留时间为0.2-10分钟 ute。 新颖的塑料材料具有特别改进的加工性和热成型性,较低的密封温度和更好的白色断裂性能。
    • 79. 发明授权
    • Modified polyolefin polymer, its manufacturing method and resin
composition containing it
    • 改性聚烯烃聚合物,其制造方法和含有它的树脂组合物
    • US5294673A
    • 1994-03-15
    • US778144
    • 1991-12-26
    • Yoshikuni DeguchiKazuya Yonezawa
    • Yoshikuni DeguchiKazuya Yonezawa
    • C08F8/30C08F110/06C08F210/00C08F255/00C08F277/00C08F279/02C08F269/00
    • C08F277/00C08F210/00C08F255/00C08F279/02C08F8/30C08F110/06
    • The present invention provides a modified polyolefin type polymer having one structural unit having a glycidyl group represented by the following general formula (I) per 2-1,000 repeating units of olefin: ##STR1## (In the formula, Ar represents an aromatic hydrocarbon group 6-23 in carbon number having at least one glycidyloxy group, and R represents hydrogen atom or methyl group.), its manufacturing method and a resin composition containing the aforementioned modified polyolefin polymer. The polyolefin type polymer of the present invention is excellent not only in mechanical properties, heat resistance and resistance to oil, but also in dyeability, adhesiveness, antistatic property. It enables blending and conversion into alloys for its outstanding affinity with other resins.
    • PCT No.PCT / JP91 / 00552 Sec。 371 1991年12月26日第 102(e)日期1991年12月26日PCT 1991年4月24日PCT PCT。 出版物WO91 / 17192 日本公开日1991年11月14日。本发明提供一种具有一个结构单元的改性聚烯烃类聚合物,其具有每2-1,000个烯烃重复单元由以下通式(I)表示的缩水甘油基:(*化学结构*)(I )(式中,Ar表示碳数为6〜23的芳香族烃基,具有至少一个缩水甘油基氧基,R表示氢原子或甲基),其制造方法和含有上述改性聚烯烃聚合物的树脂组合物。 本发明的聚烯烃类聚合物不仅具有机械性能,耐热性和耐油性,而且在染色性,粘合性,抗静电性方面也是优异的。 它能够与其他树脂具有突出的亲和力,使其能够共混和转化成合金。