    • Method of Producing a Material of Oxide Superconductor, Method of Producing an Oxide Superconducting Wire, and Superconducting Apparatus
    • 生产氧化物超导体的材料的方法,生产氧化物超导线的方法和超导装置
    • US20080020936A1
    • 2008-01-24
    • US11579583
    • 2006-01-30
    • Naoki Ayai
    • Naoki Ayai
    • H01L39/24
    • H01L39/248C01G1/00C01G1/02C01G3/006C04B35/4525C04B35/6267C04B35/6268C04B2235/3208C04B2235/3213C04B2235/443C04B2235/6567C04B2235/661H01L39/2477Y10T29/49014
    • A method of producing a material of an oxide superconductor comprises the following steps: (a) in a solution, ionizing a material containing an atom for constituting the oxide superconductor, (b) by removing a solvent by spraying the solution in a first atmosphere, producing a material powder containing the atom for constituting the oxide superconductor, and (c) cooling the material powder in a second atmosphere into which a cooling gas is introduced. In this method, the concentration of carbon dioxide in the second atmosphere is lower than that in the first atmosphere, which contains the removed solvent component. The concentration of nitrogen oxide in the second atmosphere is lower than that in the first atmosphere, which contains the removed solvent component. The concentration of water vapor in the second atmosphere is lower than that in the first atmosphere, which contains the removed solvent component. These specifications enable the method to increase the density and purity of the oxide superconductor.
    • 制造氧化物超导体的材料的方法包括以下步骤:(a)在溶液中电离含有用于构成氧化物超导体的原子的材料,(b)通过在第一气氛中喷雾溶液除去溶剂, 制造含有构成氧化物超导体的原子的材料粉末,以及(c)在引入冷却气体的第二气氛中冷却材料粉末。 在该方法中,第二气氛中的二氧化碳浓度低于含有除去的溶剂成分的第一气氛中的二氧化碳浓度。 第二气氛中的氮氧化物浓度低于含有去除的溶剂成分的第一气氛中的浓度。 第二气氛中的水蒸气浓度低于含有去除的溶剂成分的第一气氛中的浓度。 这些规范使得该方法能够增加氧化物超导体的密度和纯度。