    • 32. 发明申请
    • PROCESS FOR PRODUCING POLYTETRAFLUOROETHYLENE FINE POWDER
    • 生产聚四氟乙烯微粉的方法
    • US20140343239A1
    • 2014-11-20
    • US14449436
    • 2014-08-01
    • ASAHI GLASS COMPANY, LIMITED
    • Shinya HIGUCHIShigeki KobayashiHiroki Nagai
    • C08J3/16C08F114/26
    • C08J3/16C08F2/24C08F6/18C08F6/22C08F114/26C08L27/18
    • To provide a process for producing a PTFE fine powder having a high bulk density, whereby the concentration of non-coagulated PTFE in coagulation wastewater is low.Tetrafluoroethylene is emulsion-polymerized in the presence of an aqueous medium, at least one fluorinated emulsifier selected from the group consisting of a C4-7 fluorinated carboxylic acid having from 1 to 4 etheric oxygen atoms in its main chain, and its salts, and a radical polymerization initiator, to produce a polytetrafluoroethylene emulsion; the obtained polytetrafluoroethylene emulsion is adjusted to a polytetrafluoroethylene concentration of from 10 to 25 mass %, followed by coagulation and stirring at a coagulation temperature of from 5 to 18° C. to separate a wet-state polytetrafluoroethylene fine powder; and the obtained wet-state polytetrafluoroethylene fine powder is dried to produce a polytetrafluoroethylene fine powder.
    • 提供一种具有高堆积密度的PTFE细粉的制造方法,凝固废水中的非凝固PTFE的浓度低。 四氟乙烯在含水介质的存在下进行乳液聚合,至少一种选自由主链中具有1至4个醚性氧原子的C4-7氟化羧酸及其盐组成的组中的氟化乳化剂和 自由基聚合引发剂,生产聚四氟乙烯乳液; 将得到的聚四氟乙烯乳液调整为10〜25质量%的聚四氟乙烯浓度,在凝固温度为5〜18℃下进行凝固搅拌,分离湿式聚四氟乙烯细粉; 将得到的湿式聚四氟乙烯细粉末干燥,制成聚四氟乙烯细粉末。
    • 33. 发明授权
    • Processes for making silane, hydrophobated silica, silica masterbatch and rubber products
    • 制造硅烷,疏水二氧化硅,二氧化硅母粒和橡胶制品的方法
    • US08865799B2
    • 2014-10-21
    • US13747461
    • 2013-01-22
    • Industrias Negromex, S.A. de C.V.Cooper Tire & Rubber Company
    • Peter J. WallenChristopher J. HardimanHoward A. ColvinGregory C. BowmanJose Eduardo Rojas Reyna
    • C08K3/36C08J3/22C08J3/16C08J3/215C08K9/04C08K5/54
    • C08J3/22C01P2006/80C08J3/2053C08J3/215C08J3/223C08K5/54C08K9/06C09C1/3081Y10T428/2995C08L21/00
    • The present invention provides a process for making silica-filled rubber masterbatch using silica hydrophobated with a trimethoxy silane coupling agent that is soluble in an alcohol-water solution containing at least about 70 wt % water. One embodiment uses a mixture of trimethoxy silanes, one or more of which react with rubber to bond the silica to the rubber, and one or more of which do not react with rubber, but do hydrophobate the silica. Hydrophobated silica is mixed with latex polymer and incorporated into rubber during coagulation of the latex, which is preferably coagulated with calcium chloride. The present invention further provides a process for making the trimethoxy silane coupling agents. Preferred trimethoxy silane coupling agents include bis-(3-trimethoxysilylpropyl)-disulfide and bis-(3-trimethoxysilylpropyl)-tetrasulfide. Rubber products, particularly tires, compounded with the inventive silica masterbatch can be processed for a long time before scorching because the silica masterbatch provides a long scorch time.
    • 本发明提供一种使用二氧化硅疏水化的三甲氧基硅烷偶联剂制备二氧化硅填充橡胶母料的方法,所述三甲氧基硅烷偶联剂可溶于含有至少约70重量%水的醇 - 水溶液。 一个实施方案使用三甲氧基硅烷的混合物,其中一种或多种与橡胶反应以将二氧化硅结合到橡胶上,并且其中一种或多种不与橡胶反应,但是使二氧化硅疏水化。 将疏水性二氧化硅与胶乳聚合物混合,并在胶乳凝结期间并入橡胶中,其优选用氯化钙凝结。 本发明还提供了制备三甲氧基硅烷偶联剂的方法。 优选的三甲氧基硅烷偶联剂包括双 - (3-三甲氧基甲硅烷基丙基) - 二硫化物和双 - (3-三甲氧基甲硅烷基丙基) - 四硫化物。 与本发明的二氧化硅母料混合的橡胶制品,特别是轮胎,由于二氧化硅母料提供较长的焦烧时间,因此可在焦化之前长时间加工。