热词
    • 14. 发明授权
    • Heat resistant low shrink polyester resins
    • 耐热低收缩聚酯树脂
    • US4348499A
    • 1982-09-07
    • US182284
    • 1980-08-28
    • Donald L. Nelson
    • Donald L. Nelson
    • C08G63/553C08G63/52C08L67/06
    • C08G63/553
    • Polyester resins are produced from unsaturated dicarboxylic anhydrides which are modified with a C.sub.10 hydrocarbon concentrate. They are superior to the known resins made by the hydrolysis method containing the hydrocarbon concentrate in that the dicarboxylic anhydrides used in the preparation of the resins are hydrolyzed with an amount of water always less than the amount of maleic anhydride and/or hydrocarbon on a molar basis. After the hydrocarbon addition reaction of the in situ generated acid, the reaction is heated to 140.degree. C. to 185.degree. C. in order to generate cyclopentadiene or similar C.sub.5 hydrocarbons and form endomethylene tetrahydrophthalic anhydride (carbic anhydride) or other similar Diels-Alder products from the remaining unreacted maleic anhydride and hydrocarbon, generally prior to the addition of other resin forming chemical intermediates e.g. polyols.
    • 聚酯树脂由用C10烃精矿改性的不饱和二羧酸酐制成。 它们优于通过含有烃浓缩物的水解方法制备的已知树脂,因为用于制备树脂的二羧酸酐水解总量小于马来酸酐和/或摩尔数量的水 基础。 在原位产生酸的烃加成反应后,将反应物加热至140℃至185℃,以产生环戊二烯或类似的C5烃,并形成内亚甲基四氢邻苯二甲酸酐(碳酸酐)或其它类似的狄尔斯 - 阿尔德 通常在添加形成其它树脂的化学中间体之前,剩余的未反应的马来酸酐和烃的产物 多元醇。
    • 15. 发明授权
    • High temperature polymers
    • 高温聚合物
    • US4188473A
    • 1980-02-12
    • US869337
    • 1978-01-13
    • Donald L. Nelson
    • Donald L. Nelson
    • C07C43/263C08G65/00
    • C07C43/263
    • Polymeric materials and their thermoset, resinous products prepared by the polymerization of a mixture containing at least two different monomeric structures selected from the group having the general formula ##STR1## wherein each A represents a chalcogen independently selected from the group oxygen and sulfur; R.sub.1 represents a member selected from the group hydrogen, --CH.sub.2 (OCH.sub.2).sub.y OCH.sub.2 --R.sub.3 ; each R.sub.2 represents a member independently selected from the group consisting of R.sub.1, halogen and an alkyl group of 1 to 10 carbon atoms; R.sub.3 represents a member selected from the group consisting of H, methyl, ethyl and propyl; each m represents an independently selected integer from 1 to 2; n represents an integer from 0 to 60 and y represents an integer from 0 to 3 in the presence of an acid catalyst at a temperature of from between about 140.degree. and about 165.degree. C. for from several minutes to several hours. The thermoset resinous products are obtained by further heating the aforedescribed polymeric materials at a temperature of from about 170.degree. C. to about 260.degree. C. for from several minutes to several hours.The polymeric materials are low melting solids which are useful as laminating, molding, film-forming materials which can be cured or thermoset by heat.
    • 聚合材料及其热固性树脂产品通过聚合包含至少两种不同单体结构的混合物制备,所述混合物选自通式为:其中每个A代表独立地选自以下的硫族元素: 组氧和硫; R1表示选自氢,-CH2(OCH2)yOCH2-R3; 每个R 2表示独立地选自由R 1,卤素和1至10个碳原子的烷基组成的组的成员; R3表示选自H,甲基,乙基和丙基的成员; 每个m表示1至2的独立选择的整数; n表示0〜60的整数,y表示0〜3的整数,在酸催化剂存在下,温度为约140〜165℃,反应时间为数分钟〜数小时。 通过在约170℃至约260℃的温度下将上述聚合物材料进一步加热数分钟至数小时来获得热固性树脂产品。 聚合物材料是低熔点固体,其可用作层压,成型,可通过加热固化或热固化的成膜材料。