    • 1. 发明授权
    • 고강도 목재 제조를 위한 목재 건조 및 고열처리 방법
    • KR102322516B1
    • 2021-11-04
    • KR1020210092841
    • 2021-07-15
    • B27K5/04B27K5/00B27K3/08B27K3/48
    • 본발명은소프트우드를건조및 고열처리하여하드우드와유사한강도를가지도록하여생산된목재의실용성이현저히향상되도록하는고강도목재제조를위한목재건조및 고열처리방법에관한것으로, 본목재건조및 고열처리방법은목재를선별하는목재선별단계(S1)와, 목재탑재전의건조챔버의하중을측정하는초기하중측정단계(S2)와, 상기건조챔버에선별된목재를탑재하고상기건조챔버의하중을측정하는탑재하중측정단계(S3)와, 하중연산으로상기건조챔버에탑재된목재의하중을계산하는목재하중계산단계(S4)와, 상기건조챔버에진공을형성하는진공형성단계(S5)와, 상기건조챔버의목재를예열하는목재예열단계(S6)와, 상기건조챔버의내부에과열증기를주입하여목재를건조및 고열처리하는과열증기고열처리단계(S7)와, 상기건조챔버의내부의목재의하중을측정하여함수율을연산하고유지하는함수율연산및 유지단계(S8)와, 상기건조챔버의내부의온도를일정한범위로하강시키는온도하강단계(S9)와, 상기건조챔버의내부의압력을하강시키는압력하강단계(S10)와, 상기건조챔버의목재를자연냉각시키면서숙성시키는자연냉각및 숙성단계(S11)를포함한다.
    • 4. 发明授权
    • 황토목재 제조방법
    • 如何制作赭石木材
    • KR101823826B1
    • 2018-01-30
    • KR1020170066249
    • 2017-05-29
    • (주) 대현목재
    • 남궁원
    • B27K3/02B27K3/08B27K3/16B27K5/04B27K5/00B27N1/02
    • 본발명은황토목재제조방법에관한것으로더욱상세하게는, 황토목재제조방법은황토를소금과혼합한혼합물을 0.1 ~ 5㎚크기의입자로제조하는제 1 공정, 상기제조한황토원료, 규소또는알루미늄으로이루어지는염알루미늄계열의무기질경화제및 물을혼합하여황토원액을제조하는제 2 공정, 목재를함침로에투입하는제 3 공정, 상기함침로에진공을가하여목재내부의수분및 불순물을제거하는제 4 공정, 상기함침로의저장탱크에황토원액을공급하는제 5 공정, 상기함침로의압력을가하여상기황토원액을목재조직내부로침투시키는제 6 공정, 상기가압을해제하고진공을가하여목재표면의잔재물및 과잉흡수된황토원액을회수하는제 7 공정, 상기황토원액을회수한목재를 8시간 ~ 7일동안 60 ~ 120℃의온도에서건조하는제 8 공정및 상기건조한목재의표면을샌딩처리하는제 9 공정으로이루어지는것을특징으로하는황토목재제조방법에관한것이다. 또한본 발명에따라제조된황토목재는산업적인측면에서황토의원가가저렴하여원재료인황토의구입이용이하며취급시안전하다는장점이있으며, 황토의점성적성질로목재내부의융착이용이하다는장점이있다. 또한환경적인측면에서황토를사용함으로써친환경적이며습도조절능력이뛰어나다는효과가있으며,목재와함께사용함으로써통기성및 축열성이높으며원적외선방사로인체건강에유익하며, 강력한항균력으로곰팡이서식을억제할수 있는효과가있다. 또한목재와황토무기질세라믹의혼합으로착화온도가높아화재발생을지연또는억제시키는역할을하며, 연소시불꽃이형성되지않아유독가스의발생을억제시키는효과가있다.
    • 本发明更具体地涉及用于生产木材赭石的方法,黄土木材制造方法包括在0.1〜5㎚,将上述制备的黄色土壤材料,硅或赭石粒径制备盐的混合物的第一步骤 下降混合的无机硬化剂的盐的第三步骤,和水铝为基础的由铝制成在第二处理中,在真空制备用于浸渍一个黄土原液木材至所述浸渍以除去木材内部的水分和杂质 第四步骤,第五步骤,第六步骤中,木材脱落的压力和真空,以落入压力在浸渍渗透到赭色原液到木材组织在贮存罐供给赭石原液至浸渍 第七步骤中,第八步骤和干燥木材的表面打磨至木材回收以60〜120℃的温度下干燥8-7小时赭石原液回收碎屑和多余的吸收表面的赭色原液 处理 其包括第九步骤赭石木材涉及制造相同的方法。 此外,在根据本发明制造的黄土木材具有作为安全时黄土便宜的成本在黄土的该等级性质稠合使用木材内部购买条款赭色生的,并在工业观点来看处理的优点的优点 有。 此外,通过使用从视图环境友好的环境点黄色土壤,且该调湿能力优异的效果,通过与木材一起使用具有较高的透气性和轴隐性和远红外线辐射对人体健康有益,这能抑制真菌栖息地很强的抗菌活性 这是有效的。 此外,抑制有毒气体的产生的效果,木材和延迟或抑制火灾的赭色无机陶瓷高动作的混合物的点火温度,且由于在燃烧过程中,火焰形成。
    • 6. 发明公开
    • 목재의 수지 주입성 개선을 위한 처리방법
    • 木材化学处理方法
    • KR1020160070222A
    • 2016-06-20
    • KR1020140175677
    • 2014-12-09
    • 전북대학교산학협력단
    • 박희준
    • B27K3/08B27K3/34
    • B27K3/34B27K3/06B27K3/083B27K3/10B27K3/14B27K3/18B27K3/20B27K3/28B27K3/50B27K5/02
    • 본발명은목재에수지를주입하는방법에관한것이다. 보다구체적으로, 본발명은목재를배할또는보링처리한후 방부또는난연수지를진공상태에서가압주입하는방법에관한것이다. 본발명에따른수지주입성개선방법은수지를목재내부에보다효율적으로균일하게주입할수 있어수지주입성을개선시켰다. 또한, 본발명의수지주입방법은건조과정중에할렬,크랙이나변형이없고건조시간도단축시킬수 있으므로고품질의수지주입목재(방부목재, 난연목재, 치수안정성개선목재등)를제공할수 있다. 또한, 본발명으로제조된방부/난연목재는기존의무처리목재나자상처리(인사이징)법에의해제조된목재에비해외관의손상이없는등 목재의미적외관을충분히살릴수 있다. 또한, 본발명으로제조된목재는무처리목재에비교하여서도휨강도나압축강도등이떨어지지않으며, 치수가크고무거운목조건축물의기둥이나보 등구조용부재의강도적감소없이중량을줄일수 있어운반, 가공및 시공등에서유리하게작용할수 있다.
    • 本发明涉及树脂注入木材的方法。 更具体地,本发明涉及在木材切割或镗孔后进行防腐或阻燃树脂的加压真空状态注入的方法。 根据本发明的树脂注射改进方法确保了树脂有效且均匀地注入木材并提高了树脂的注射性。 此外,根据本发明的树脂注射方法在干燥过程中不会发生裂开,开裂或变形,并且能够干燥时间减少,因此能够提供高品质的树脂注射的木材(防腐木材,火焰 易碎木材,尺寸稳定性提高的木材等)。 与根据现有技术的未经处理的木材或切割木材相比,用本发明制造的防腐/阻燃木材能够改善木材外观并消除对外部的损害。 此外,用本发明制造的木材具有与未处理木材相当的弯曲强度或压缩强度。 此外,本发明可以有效地用于运输,加工和施工中,因为可以在不降低强度的情况下减少诸如大型和重型木结构的柱和梁的结构构件的重量。
    • 7. 发明公开
    • 목재함침용 난연수지
    • 木材防火树脂
    • KR1020140023853A
    • 2014-02-27
    • KR1020130070037
    • 2013-06-19
    • 전북대학교산학협력단
    • 박희준
    • B27K3/52B27K3/08
    • B27K3/08B27K3/52
    • The present invention relates to a flame resisting resin for impregnating wood, which provides fire retardant as well as maintains the properties of natural wood by impregnating wood, and a method for manufacturing flame resisting wood manufactured using the same. In the method for manufacturing the flame resisting wood according to the present invention, the wood is impregnated with a water soluble flame retardant, thereby manufacturing the wood, which maintains a function of controlling temperature and humidity, one of big advantages of the natural wood, and keeps the scent of the wood, and meets the fire retardant standard(incombustibility, semi-non combustibility, fire retardant, and flame proof). Also, since the flame resisting resin is attached to the micropores such as inner cavity of cells and intercellular space of the wood after drying, the whitening event does not occurs and adhesive strength does not become weak, unlike phosphorous based polymer does not having carbon atom, if the flame resisting resin remains on the surface of the wood. And the flame resisting manufactured by the present invention also has significantly increased antimicrobial activity and dimensional stability. [Reference numerals] (S1) Step for transferring dried wood; (S2) Step for injecting a resin for impregnating wood into the wood; (S3) Step for impregnating the wood in the resin; (S4) Step for drying the wood
    • 本发明涉及一种用于浸渍木材的阻燃树脂,其提供阻燃剂以及通过浸渍木材来保持天然木材的性质,以及制造使用其的制造阻燃木材的方法。 在根据本发明的阻燃木材的制造方法中,木材用水溶性阻燃剂浸渍,从而制造木材,其保持控制温度和湿度的功能,天然木材的一大优点, 并保持木材的香味,符合阻燃标准(不燃性,半不燃,阻燃,防火)。 此外,由于阻燃树脂附着于细胞的内腔和干燥后的木材的细胞间隙等微细孔,与不含碳原子的磷基聚合物不同,不发生白化事件,粘合强度不变弱 如果阻燃树脂残留在木材的表面上。 并且本发明制造的阻燃性也具有显着增加的抗微生物活性和尺寸稳定性。 (附图标记)(S1)转移干木的步骤; (S2)将树脂浸渍到木材中的步骤; (S3)树脂浸渍木材的工序; (S4)干燥木材的步骤
    • 8. 发明公开
    • 목재의 치수안정성 및 난연성 향상 가공방법
    • 改进LUMBER的尺寸稳定性和耐火材料的方法
    • KR1020110128444A
    • 2011-11-30
    • KR1020100047897
    • 2010-05-24
    • 전북대학교산학협력단전일목재산업 주식회사
    • 오승원박희준김병진
    • B27K5/06B27K3/08B27K3/34
    • B27K3/08B27K3/38B27K2240/30
    • PURPOSE: Dimensional stability and flame retardant characteristic improvement processing method of timber are provided to improve the dimensional stability and the flame retardant characteristic of the timber using water solubility melamine resin having the concentration of 25-35% and water solubility flame retardant. CONSTITUTION: Mixture is formed by mixing water solubility melamine resin and water solubility flame retardant. The mixture is impregnated in timber by a vacuum press method. The water solubility melamine resin has the concentration of 25-35% in a state the water solubility melamine resin is attenuated by water. The water solubility flame retardant has the concentration of 25-35% in a state the water solubility melamine resin is attenuated by the water.
    • 目的:提供木材的尺寸稳定性和阻燃特性改进加工方法,以提高木材的尺寸稳定性和阻燃特性,使用浓度为25-35%的水溶性三聚氰胺树脂和水溶性阻燃剂。 构成:通过混合水溶性三聚氰胺树脂和水溶性阻燃剂形成混合物。 通过真空压制法将混合物浸渍在木材中。 在水溶性三聚氰胺树脂被水减弱的状态下,水溶性三聚氰胺树脂的浓度为25-35%。 在水溶性三聚氰胺树脂被水减弱的状态下,水溶性阻燃剂的浓度为25-35%。