会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明公开
    • 가구용 패널
    • 家具面板
    • KR1020000024375A
    • 2000-05-06
    • KR1020000006304
    • 2000-02-10
    • 정지한
    • 정지한
    • B27K5/04
    • B27K3/34B27K3/0207B27K3/12B27K3/14
    • PURPOSE: A method of manufacturing panel for furniture is provided to prevent environmental pollution by using perilla oil or bean juice etc. instead of chemicals in the surface treatment of a panel and to give smooth and natural gloss to the panel, thereby providing traditional and antique beauty. CONSTITUTION: A method of manufacturing panel for furniture includes the steps of preprocessing(10) the surface of a panel by abrasing or forming patterns, applying bean juice on the surface of the panel by brush or cotton sheet and drying the bean juice such as soy beans for hardening the surface to prevent deformation of the pattern formed in the preprocessing and to prevent the permeation of the oil to be applied later, and applying vegetable oil such as perilla oil on the surface of the panel by brush or cotton sheet and drying the surface for emitting water out of the panel to prevent the deformation of the panel due to the humidity, wherein the glossy of the panel is very natural and continued for a long time by rubbing with the surface.
    • 目的:提供一种制造家具面板的方法,以防止在面板表面处理中使用紫苏油或豆汁等代替化学品对环境造成污染,并给面板提供光滑自然的光泽,从而提供传统和古董 美丽。 构成:制造家具面板的方法包括以下步骤:通过磨损或形成图案对面板的表面进行预处理(10),通过刷子或棉花片将豆汁施加在面板的表面上并干燥豆汁如大豆 用于使表面硬化以防止在预处理中形成的图案变形并防止稍后施用的油渗透,并通过刷子或棉布片将诸如紫苏油的植物油施用在面板的表面上并干燥 表面用于将水从面板中排出以防止由于湿度而导致的面板的变形,其中面板的光泽是非常自然的并且通过与表面摩擦而持续很长时间。
    • 2. 发明公开
    • 목재의 수지 주입성 개선을 위한 처리방법
    • 木材化学处理方法
    • KR1020160070222A
    • 2016-06-20
    • KR1020140175677
    • 2014-12-09
    • 전북대학교산학협력단
    • 박희준
    • B27K3/08B27K3/34
    • B27K3/34B27K3/06B27K3/083B27K3/10B27K3/14B27K3/18B27K3/20B27K3/28B27K3/50B27K5/02
    • 본발명은목재에수지를주입하는방법에관한것이다. 보다구체적으로, 본발명은목재를배할또는보링처리한후 방부또는난연수지를진공상태에서가압주입하는방법에관한것이다. 본발명에따른수지주입성개선방법은수지를목재내부에보다효율적으로균일하게주입할수 있어수지주입성을개선시켰다. 또한, 본발명의수지주입방법은건조과정중에할렬,크랙이나변형이없고건조시간도단축시킬수 있으므로고품질의수지주입목재(방부목재, 난연목재, 치수안정성개선목재등)를제공할수 있다. 또한, 본발명으로제조된방부/난연목재는기존의무처리목재나자상처리(인사이징)법에의해제조된목재에비해외관의손상이없는등 목재의미적외관을충분히살릴수 있다. 또한, 본발명으로제조된목재는무처리목재에비교하여서도휨강도나압축강도등이떨어지지않으며, 치수가크고무거운목조건축물의기둥이나보 등구조용부재의강도적감소없이중량을줄일수 있어운반, 가공및 시공등에서유리하게작용할수 있다.
    • 本发明涉及树脂注入木材的方法。 更具体地,本发明涉及在木材切割或镗孔后进行防腐或阻燃树脂的加压真空状态注入的方法。 根据本发明的树脂注射改进方法确保了树脂有效且均匀地注入木材并提高了树脂的注射性。 此外,根据本发明的树脂注射方法在干燥过程中不会发生裂开,开裂或变形,并且能够干燥时间减少,因此能够提供高品质的树脂注射的木材(防腐木材,火焰 易碎木材,尺寸稳定性提高的木材等)。 与根据现有技术的未经处理的木材或切割木材相比,用本发明制造的防腐/阻燃木材能够改善木材外观并消除对外部的损害。 此外,用本发明制造的木材具有与未处理木材相当的弯曲强度或压缩强度。 此外,本发明可以有效地用于运输,加工和施工中,因为可以在不降低强度的情况下减少诸如大型和重型木结构的柱和梁的结构构件的重量。
    • 5. 发明授权
    • 염색 천연 무늬목 제조 방법 및 그 제조 방법으로 제조된 염색 천연 무늬목
    • DYED VENEER及其制造方法
    • KR100848044B1
    • 2008-07-23
    • KR1020080015291
    • 2008-02-20
    • (주) 혜성무늬목
    • 신호열
    • B27K5/02B27K3/34
    • B27K5/02B27K3/14B27K5/001B27K5/007
    • A dyed natural veneer manufacturing method and a dyed veneer produced by the same are provided to unify the tones of the dyed veneer made of the same species of trees, at low cost through a simple process and to use the veneer with the unified tone and the veneer with the natural tone selectively. A dyed natural veneer manufacturing method comprises the steps of: dispersing oil dyes having the single color, in an oil solvent and applying the mixture to a thin film(101); laminating the film on the veneer of 0.1~0.5mm which is not decolorized(102); and making tones of the front and rear surfaces of the veneer different by gradually dyeing the veneer with dyes in the thickness of 10~70% of the veneer while keeping temperature of 160~190°C and pressure of 5~30Kg/cm^3 by a heat press(103).
    • 提供了一种染色的天然单板制造方法和由其制造的染色单板,以通过简单的工艺以低成本统一由相同种类的树木制成的染色单板的色调,并且使用具有统一色调的单板和 单板选择性自然。 染色天然胶合板制造方法包括以下步骤:将具有单一颜色的油性染料分散在油溶剂中并将混合物施加到薄膜(101)上; 将薄膜层压在0.1〜0.5mm不脱色的薄板上(102); 并且通过在保持温度为160〜190℃,压力为5〜30Kg / cm 3的薄板的10〜70%的厚度内逐渐染色单板,使单板的前后表面的色调不同 通过热压机(103)。
    • 7. 发明公开
    • 옻칠 기술 기반의 가구 표면 마감 방법
    • 基于变压器的家具表面处理方法
    • KR1020120136915A
    • 2012-12-20
    • KR1020110056122
    • 2011-06-10
    • 한양대학교 산학협력단주식회사 장수산업
    • 남경숙
    • B27K5/00A47B96/20
    • B27K5/00A47B96/20B27K3/0271B27K3/0292B27K3/04B27K3/06B27K3/083B27K3/10B27K3/14B27K3/163B27K3/166
    • PURPOSE: A method of finishing a surface of a furniture using lacquer is provided to obtain antibacterial, antiseptic and sterilizing effect by the function of an urushiol which is a main component of the lacquer. CONSTITUTION: A method of finishing a surface of a furniture using lacquer comprises: a step(S100) of polishing the surface of a wood frame which forms the body of furniture by an abrasive with a first roughness; a step(S105) of coating the wood frame with urethane paint several times; a step(S105) of polishing the surface of the wood frame by an abrasive with a second roughness which is higher than the first roughness; and a step(S140) of lacquer-painting the wood frame. [Reference numerals] (AA) Start; (BB) End; (S100) Polishing surface of wood frame; (S105) Primary spreading urethane paint on wood frame; (S110, S120, S130) Drying urethane paint and polishing wood frame by abrasive; (S115) Secondary spreading urethane paint on wood frame; (S125) Tertiary spreading urethane paint on wood frame; (S135) Controlling moisture of surface of wood frame to 60%; (S140) Primary varnishing wood frame with lacquer; (S145, S155) Drying and controlling surface of wood frame to 60%; (S150) Secondary varnishing wood frame with lacquer; (S160) Tertiary spreading urethane paint on wood frame
    • 目的:提供使用漆完成家具表面的方法,以通过作为漆的主要成分的漆酚的功能获得抗菌,防腐和杀菌作用。 构成:使用漆完成家具表面的方法包括:通过具有第一粗糙度的磨料研磨形成家具主体的木框架的表面的步骤(S100); 用氨基甲酸酯涂料涂布木框架数次的步骤(S105) 通过具有高于第一粗糙度的第二粗糙度的磨料研磨木质框架的表面的步骤(S105) 以及对木框架进行漆漆的步骤(S140)。 (附图标记)(AA)开始; (BB)结束; (S100)木框抛光面; (S105)木架上主要涂布氨基甲酸酯漆; (S110,S120,S130)干燥聚氨酯涂料,研磨磨木架; (S115)木架上二次铺展的聚氨酯漆; (S125)木框架上第三层聚氨酯涂料; (S135)控制木框表面的水分达到60%; (S140)主要上漆木框架与漆; (S145,S155)木框干燥控制面达到60%; (S150)二次上漆木框与漆; (S160)木框架上三层铺展聚氨酯漆