    • 2. 发明公开
    • 피지엔-피지티계 압전 세라믹 조성물 및 그 제조방법
    • PZN-PZT压电陶瓷及其制造方法
    • KR1020130090696A
    • 2013-08-14
    • KR1020120012020
    • 2012-02-06
    • 경원산업 주식회사
    • 김경원정현진정광현김관수김수찬
    • C04B35/491C04B35/495C04B35/64H01L41/187
    • C04B35/491C04B35/4521C04B35/495C04B35/64C04B2235/3227C04B2235/3244C04B2235/3251C04B2235/3298H01L41/1876
    • PURPOSE: A PZN-PZT piezoelectric ceramic composition is provided to have a high mechanical quality factor (Qm) of a piezoelectric ceramic with maintaining a high dielectric constant (K33), an electromechanical coupling coefficient (kp) and a piezo-electric constant (d33) by including a specific additives like CuO to the optimal range. CONSTITUTION: A PZN-PZT piezoelectric ceramic composition is indicated as the chemical formula: 0.2 Pb (Zn1/3Nb2/3)O3-0.8 Pb (Zr,Ti)O3+xBiMnO3+yLaMnO3+zCuO; and the x+y is 0.5-1.5wt%, based on the total weight of the composition and the z is 0.1-0.5wt%. A manufacture method of 0.2 Pb (Zn1/3Nb2/3)O3-0.8 Pb (Zr,Ti)O3 piezoelectric ceramic composition comprises the following steps. 0.2 Pb (Zn1/3Nb2/3)O3-0.8 Pb (Zr,Ti)O3 is mixed, pulverized and calcinated at 800-850°C. The calcinated 0.2 Pb (Zn1/3Nb2/3)O3-0.8 Pb (Zr,Ti)O3 compound is reground. BiMnO3 and LaMnO3 are mixed, pulverized and calcinated at 700°C and at 1000°C. The calcinated BiMnO3 compound and the calcinated LaMnO3 compound are reground. One or more of the BiMnO3, the LaMnO3 and the CuO is mixed with the 0.2 Pb (Zn1/3Nb2/3)O3-0.8 Pb (Zr,Ti)O3 compound and pulverized. The mixed compound of the 0.2 Pb (Zn1/3Nb2/3)O3-0.8 Pb (Zr,Ti)O3 is sintered at 880-920°C after molded with the high pressure.
    • 目的:提供PZN-PZT压电陶瓷组合物,以具有保持高介电常数(K33),机电耦合系数(kp)和压电常数(d33)的压电陶瓷的高机械品质因数(Qm) )通过将特定的添加剂如CuO包含在最佳范围内。 构成:PZN-PZT压电陶瓷组合物以化学式表示:0.2 Pb(Zn1 / 3Nb2 / 3)O3-0.8 Pb(Zr,Ti)O3 + xBiMnO3 + yLaMnO3 + zCuO; 并且x + y为0.5-1.5重量%,基于组合物的总重量,z为0.1-0.5重量%。 0.2 Pb(Zn1 / 3Nb2 / 3)O3-0.8 Pb(Zr,Ti)O3压电陶瓷组合物的制造方法包括以下步骤。 将0.2 Pb(Zn1 / 3Nb2 / 3)O3-0.8 Pb(Zr,Ti)O3在800-850℃下混合,粉碎和煅烧。 煅烧后的0.2 Pb(Zn1 / 3Nb2 / 3)O3-0.8 Pb(Zr,Ti)O3化合物重掺杂。 将BiMnO 3和LaMnO 3在700℃和1000℃下混合,粉碎和煅烧。 煅烧的BiMnO3化合物和煅烧的LaMnO 3化合物是重掺杂的。 将一种或多种BiMnO3,LaMnO3和CuO与0.2 Pb(Zn1 / 3Nb2 / 3)O3-0.8 Pb(Zr,Ti)O3化合物混合并粉碎。 0.2 Pb(Zn1 / 3Nb2 / 3)O3-0.8 Pb(Zr,Ti)O3的混合化合物在高压成型后在880-920℃下烧结。
    • 3. 发明公开
    • 압전 밸브
    • 压电阀
    • KR1020120135724A
    • 2012-12-17
    • KR1020110054599
    • 2011-06-07
    • 경원산업 주식회사
    • 김홍희한용환
    • F16K31/02
    • PURPOSE: A piezoelectric valve is provided to increase generation force and the bending displacement of a piezoelectric actuator by extending one surface in the opposite side to a surface where the displacement occurs to support the piezoelectric actuator. CONSTITUTION: A piezoelectric valve comprises a housing(10), a piezoelectric actuator(20), and a pressing part(30). The housing comprises a hole and a flow path. Air flows in or out through the hole and is moved through the flow path. One end of the piezoelectric actuator is fixed in the housing by a fixing member and the other end thereof is supported by the housing. The pressing part presses the other end of the piezoelectric actuator at a constant pressure.
    • 目的:提供一种压电阀,以通过将相反侧的一个表面延伸到发生位移的表面以支撑压电致动器来增加压电致动器的发电力和弯曲位移。 构成:压电阀包括壳体(10),压电致动器(20)和按压部分(30)。 壳体包括孔和流路。 空气通过孔流入或流出,并通过流路移动。 压电致动器的一端通过固定构件固定在壳体中,另一端由壳体支撑。 按压部分以恒定的压力按压压电致动器的另一端。
    • 7. 发明公开
    • 열가소성 물질을 이용한 나선형 압전 액츄에이터의제조방법 및 그로부터 제조된 나선형 압전 액츄에이터 및초소형 초음파 모터
    • 使用热塑性挤压和螺旋压电致动器制造螺旋压电致动器的方法和制造的微型超声波电机
    • KR1020090016060A
    • 2009-02-13
    • KR1020070080422
    • 2007-08-10
    • 재단법인서울대학교산학협력재단경원산업 주식회사
    • 김현이이경우이성미
    • H01L41/16H01L41/18B06B1/06
    • H01L41/1876C04B35/491H01L41/0906H01L41/43
    • A method for manufacturing a spiral piezoelectric actuator using a thermoplastic material and the spiral piezoelectric actuator, and a micromini ultrasonic motor are provided to obtain a sufficient piezoelectric characteristic by performing the sintering using the thermoplastic property after making one feedrod composed of a piezoelectric element and an inert compound and extruding the feedrod through co-extrusion method. The pulverized PZN-PZT powder sintered at low temperature is made by mixing PZN made of Pb, Zn, and Nb and PZT made of Pb, Zn, and (Ti) with a predetermined ratio(S1). A piezoelectric element is made by adding polymer to the PZN-PZT powder(S2). A compound is made by adding the polymer after mixing the PZN-PZT power with Ag(S3). After forming the feedrod with a square pillar of the piezoelectric actuator composed of two-layer plate shape by co-extruding the piezoelectric element and the compound, the feedrod is cut(S4). The feedrod with a predetermined size is processed with a spiral shape in a furnace(S5). The spiral piezoelectric actuator composed of a piezoelectric layer and a compound layer is formed by performing the sintering at high temperature while combusting the polymer by heating the spiral feedrod at high temperature(S6).
    • 提供一种制造使用热塑性材料的螺旋压电致动器和螺旋压电致动器的方法以及微型超声波马达,通过在由一个压电元件和一个压电元件构成的一个馈线之后进行使用热塑性的烧结来获得足够的压电特性 惰性化合物,并通过共挤出法挤出进料。 通过将由Pb,Zn和Nb制成的PZN和由Pb,Zn和(Ti)制成的PZT以预定的比例(S1)混合制成在低温下烧结的粉碎的PZN-PZT粉末。 通过向PZN-PZT粉末(S2)中加入聚合物制成压电元件。 通过在将PZN-PZT功率与Ag(S3)混合后添加聚合物来制备化合物。 在通过共挤出压电元件和化合物的方式将由双层板形式构成的压电致动器的方柱形成饲料之后,进料被切割(S4)。 具有预定尺寸的饲料在炉中以螺旋形状加工(S5)。 由压电层和复合层组成的螺旋压电致动器通过在高温下进行烧结而形成,同时通过在高温下加热螺旋进料来燃烧聚合物(S6)。
    • 8. 发明公开
    • 다층 구조를 가지는 2-2 압전 복합 초음파 발진자 및제조방법
    • 多层2-2型PIEZO复合超声波传感器及其相关方法
    • KR1020080000010A
    • 2008-01-02
    • KR1020060057192
    • 2006-06-26
    • 재단법인서울대학교산학협력재단경원산업 주식회사
    • 김현이이경우윤창번
    • H01L41/083H01L41/187
    • H01L41/083H01L41/0471H01L41/187H01L41/193H01L41/273
    • A multilayer 2-2 piezo-composite ultrasonic transducer and a manufacturing method thereof are provided to cause a large displacement by a low voltage and to use a wide range of frequency. Two first inner electrode layers are exposed from a left side of a piezoceramic plate and directly contacted with a first outer electrode layer. The first inner electrode layers are not exposed from a right side of the piezoceramic plate but buried under a piezoelectric layer apart from a second outer electrode layer. Two second inner electrode layers are arranged to be opposed to the first inner electrode layers and contacted with the outer electrode layer, which is not contacted with the first inner electrode layers. The first and second inner electrode layers are alternatively arranged in the piezoelectric layers. When electric power is supplied to the outer electrode layers, a voltage is induced between the first and second inner electrode layers.
    • 提供多层2-2压电复合超声波换能器及其制造方法,以通过低电压引起大的位移并且使用宽的频率范围。 两个第一内电极层从压电陶瓷板的左侧露出,并与第一外电极层直接接触。 第一内部电极层不从压电陶瓷板的右侧暴露,而是埋在与第二外部电极层隔开的压电层下方。 两个第二内部电极层被布置成与第一内部电极层相对并且与不与第一内部电极层接触的外部电极层接触。 第一和第二内部电极层交替布置在压电层中。 当向外部电极层供电时,在第一和第二内部电极层之间产生电压。
    • 10. 发明授权
    • 압전 초음파 모터의 제조 방법과 그 방법에 의해 제조된압전 초음파 모터
    • 超声波电机的制造方法和超声波电机的制造方法
    • KR100714440B1
    • 2007-05-04
    • KR1020050029616
    • 2005-04-08
    • 재단법인서울대학교산학협력재단경원산업 주식회사
    • 김현이윤창번이경우
    • H02N2/00H02N2/02
    • 본 발명은 압전 모터에 관한 것으로 보다 상세하게는 동시 사출법(Co-rxtrusion)에 의한 압전 초음파 모터의 제조 방법과 그 방법에 의해 제조된 압전 초음파 모터에 관한 것이다.
      본 발명에 따른 압전 초음파 모터의 제조 방법은 저온 소결이 가능한 납(Pb), 아연(Zn), 니오브(Nb)로 조성되는 PZN과 납(Pb), 아연(Zn), 티타늄(Ti)으로 조성되는 PZT가 소정 비율로 혼합된 PZN-PZT 파우더와 폴리머를 혼합하여 압전체를 제조하는 압전체 제조 공정과; 상기 압전체 제조 공정에 의해 제조된 PZN-PZT 파우더와 은(Ag)을 소정 비율로 혼합된 파우더에 폴리머를 혼합하여 복합체를 제조하는 복합체 제조 공정과; 상기 압전체 및 복합체 제조 공정에 의해 제조된 압전체 및 복합체와 카본 블랙을 이용하여 상기 압전 모터의 초기 형상에 따른 피드로드(Feedrod)를 제작하는 피드로드 제작 공정과; 제작된 상기 피드로드(Feedrod)를 소정 크기의 성형 틀을 통해 사출하고 사출된 압전 모터 시편을 소정 크기로 절단하는 사출 공정;을 포함하는 것을 특징으로 한다.
      따라서, 서로 다른 소재를 하나의 피드로드(Feedrod)로 제작하고, 제작된 피드로드(Feedrod)를 동시에 사출시켜 압전 초음파 모터를 제조함으로써, 충분한 압전효과를 가질 수 있는 압전체 및 구동력이 우수한 압전 초음파 모터를 적은 비용과 제조할 수 있는 장점이 있다.
      압전체, 압전 효과, 압전 모터, PZT, PZN