    • 4. 发明专利
    • System for producing modified sulfur solidified article
    • 生产改性硫磺固化物品的制度
    • JP2006315314A
    • 2006-11-24
    • JP2005140673
    • 2005-05-13
    • Nippon Oil CorpPetroleum Energy Center新日本石油株式会社財団法人石油産業活性化センター
    • CHATANI MASAAKIKURAKAKE MINORU
    • B28C9/02B28B15/00C01B17/00
    • C01B17/0243B28C5/466B28C7/003B28C9/002C04B28/36C04B14/06C04B24/00
    • PROBLEM TO BE SOLVED: To provide a system for producing a modified sulfur solidified article which can be stored as a nonhazardous material and is easy to transport.
      SOLUTION: The system comprises: a tank for producing a modified sulfur 3 in which molten sulfur and a sulfur modifying agent are received from a tank for the molten sulfur 1 and a tank for the sulfur modifying agent 2 respectively to produce the modified sulfur by mixing and to heat the content at a predetermined temperature or higher; a tank for a modified sulfur intermediate material 5 in which the modified sulfur and fine aggregate are received from the tank for producing the modified sulfur 3 and a fine aggregate hot bin 4 respectively to produce the modified sulfur intermediate material and to heat the content at a predetermined temperature or higher; a kneader 7 in which the modified sulfur intermediate material and coarse aggregate are received from the tank for the modified sulfur intermediate material 5 and a coarse aggregate hot bin 6 respectively to knead and to heat the content at a predetermined temperature or higher; and a casting apparatus 8 in which the raw material kneaded in the kneader 7 is received to store, to heat the content at a predetermined temperature or higher, and the raw material therein is weighed and casted into a casting mold 36.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供可以作为非危险材料储存并且易于运输的改性硫固化物品的制造系统。 解决方案:该系统包括:用于生产改性硫3的罐,其中熔融硫和硫改性剂从用于熔融硫1的罐和硫改性剂2的罐分别接收以产生改性的 通过混合并在预定温度或更高温度下加热含量的硫; 用于改性硫中间体5的罐,其中从容器中接收改性硫和细骨料以分别生产改性硫3和细骨料热箱4,以制备改性硫中间体,并在 预定温度或更高; 从改性硫中间体5的容器和粗骨料热箱6分别接收改性硫中间体和粗骨料的捏合机7,在预定温度或更高温度下捏合并加热含量; 以及铸造装置8,其中接收在捏和机7中捏合的原料以存储预定温度或更高的内容物,并将其中的原料称重并浇注到铸模36中。 (C)2007,JPO&INPIT