    • JP2008240207A
    • 2008-10-09
    • JP2007084475
    • 2007-03-28
    • Toray Ind Inc東レ株式会社
    • KARASAWA RUMISEKI MASAO
    • D06M15/27A41B17/00A41D13/00A41D19/00A41D31/00A42B1/00D06M23/04
    • PROBLEM TO BE SOLVED: To obtain a fiber structure that is provided with a new air layer and has an excellent heat retaining property, antistatic property and durability without impairing an air layer which a fiber structure essentially possesses. SOLUTION: The fiber structure comprises a resin film obtained by polymerizing a polymerizable monomer containing a blowing agent on a fiber formed on a fiber surface. The resin film has foams and is obtained by polymerizing a polymerizable monomer containing at least two or more acrylic groups and/or methacrylic groups at both terminals or one terminal of a main chain containing a polyalkylene oxide segment or at the side chains of the main chain. COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了获得具有新的空气层的纤维结构,并且具有优异的保温性,抗静电性和耐久性,而不损害纤维结构基本上具有的空气层。 解决方案:纤维结构包括通过在纤维表面上形成的纤维上聚合含有发泡剂的可聚合单体获得的树脂膜。 树脂膜具有泡沫,并且通过在包含聚环氧烷链段的主链或主链的侧链的两个末端或一个末端聚合含有至少两个或更多个丙烯酸基和/或甲基丙烯酸基团的可聚合单体而获得 。 版权所有(C)2009,JPO&INPIT
    • 2. 发明专利
    • Fibrous structural material
    • 纤维结构材料
    • JP2008202187A
    • 2008-09-04
    • JP2007042081
    • 2007-02-22
    • Toray Ind Inc東レ株式会社
    • KARASAWA RUMISEKI MASAO
    • D06M23/08A41B9/04A41B17/00
    • PROBLEM TO BE SOLVED: To provide a fibrous structural material excellent in warmth-keeping property, antistatic property, and durability, which is obtained by imparting a new air layer without inhibiting an air layer that the fibrous structural material originally has.
      SOLUTION: In the fibrous structural material having the warmth-keeping property and antistatic property, a resin coating obtained by polymerizing a polymerizable monomer on fibers is formed on the surface of the fibers, and the resin coating contains hollow fine particles.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供通过赋予新的空气层而不抑制纤维结构材料最初具有的空气层而获得的保温性,抗静电性和耐久性优异的纤维结构材料。 解决方案:在具有保温性和抗静电性的纤维结构材料中,在纤维的表面上形成通过在纤维表面聚合可聚合单体获得的树脂涂层,并且树脂涂层含有中空微粒。 版权所有(C)2008,JPO&INPIT
    • 3. 发明专利
    • Fiber structure
    • 光纤结构
    • JP2008163474A
    • 2008-07-17
    • JP2006351131
    • 2006-12-27
    • Toray Ind Inc東レ株式会社
    • SEKI MASAOABE WATARU
    • D06M15/347A41D31/00D06M15/507
    • PROBLEM TO BE SOLVED: To stably provide a fiber structure which has an excellent durable anti-staining property against aqueous stains and oily stains. SOLUTION: This fiber structure has a resin coating film containing a triazine ring-containing polymerizable monomer as a polymerization component, on the surface of a single fiber, contains a hydrophilic polyester-based resin, in the coating film, and has a lipstick staining property, a sebum-staining property and a mud-staining property at the fourth grade or larger, when the fiber structure is washed by a method defined in JIS L0217-103 method and (grade) judged in a gray scale for staining. A garment has the fiber structures. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:稳定地提供对水性污渍和油性污渍具有优异的耐久性抗污染性的纤维结构。 解决方案:该纤维结构体具有含有三嗪环的可聚合单体作为聚合组分的树脂涂膜,在单一纤维的表面上,在涂膜中含有亲水性聚酯类树脂,并且具有 当按照JIS L0217-103方法中规定的方法洗涤纤维结构,并以灰度判定为染色时的(等级),在4级以上时的口红染色性,皮脂染色性和泥浆染色性。 服装有纤维结构。 版权所有(C)2008,JPO&INPIT
    • 5. 发明专利
    • Fiber structure
    • 光纤结构
    • JP2007146313A
    • 2007-06-14
    • JP2005339819
    • 2005-11-25
    • Toray Ind Inc東レ株式会社
    • SEKI MASAOKARASAWA RUMI
    • D06M15/27D06M11/79D06M15/423
    • PROBLEM TO BE SOLVED: To provide a fiber structure having the composite performance of functions such as water absorptivity, antistatic property, stain resistance and melting resistance which are excellent in durability.
      SOLUTION: This fiber structure comprising single fibers to which a resin coating film containing, as a polymerization component, a compound having two or more acryl groups or methacryl groups at both the terminals or one terminal of a main chain consisting mainly of a polyalkylene oxide segment or at the side chains of the main chain, and a resin coating film containing, as a polymerization component, a trimethylol melamine represented by the general formula (1) are laminated.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供具有耐久性优异的吸水性,抗静电性,耐污染性和耐熔融性等功能的复合性能的纤维结构体。 解决方案:该纤维结构体包括单纤维,其中树脂涂膜含有作为聚合组分的主链上两个或多个具有两个或多个丙烯酰基或甲基丙烯酰基的化合物或主链的一个末端,主要由 聚环氧烷链段或主链的侧链,以及含有作为聚合成分的由通式(1)表示的三羟甲基三聚氰胺的树脂涂膜。 版权所有(C)2007,JPO&INPIT
    • 6. 发明专利
    • Textile fiber structural product
    • 纺织纤维结构产品
    • JP2007070744A
    • 2007-03-22
    • JP2005256330
    • 2005-09-05
    • Sakainagoya Co LtdToray Ind Inc東レ株式会社株式会社サカイナゴヤ
    • HASEYAMA AYASEKI MASAOHORIE HIDEKAZUYAMADA KAZUJI
    • D06M11/79A41D31/00D06M13/144D06M15/27
    • PROBLEM TO BE SOLVED: To provide a textile fiber structural product coated with a coolness-acting sugar alcohol in high durability.
      SOLUTION: The textile fiber structural product is such that the fiber surface is coated with film containing inorganic particles and the sugar alcohol and formed by polymerizing a polymerizable monomer having at least two acrylic and/or methacrylic groups as one or both ends or side chains of the main chain based on polyalkylene oxide segments. In this textile fiber structural product, the coating film thickness is 5-40 nm, the mixing weight ratio of the polymerizable monomer to the inorganic particles is 1:(0.4-1.0) and that of the polymerizable monomer to the sugar alcohol is 1:(0.01-0.1), and the inorganic particles are each 5-400 nm in size.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供涂覆有冷汗糖醇的高耐久性的纺织纤维结构产品。 解决方案:纺织纤维结构产品使得纤维表面涂覆有含有无机颗粒和糖醇的膜,并通过聚合具有至少两个丙烯酸和/或甲基丙烯酸基团的可聚合单体作为一个或两个末端或 基于聚环氧烷链段的主链侧链。 在该纺织纤维结构体中,涂膜厚度为5-40nm,可聚合单体与无机颗粒的混合重量比为1:(0.4-1.0),可聚合单体与糖醇的混合重量比为1: (0.01-0.1),无机粒子的大小为5-400nm。 版权所有(C)2007,JPO&INPIT
    • 8. 发明专利
    • Polyester-based fiber structure
    • 基于聚酯的纤维结构
    • JP2006152451A
    • 2006-06-15
    • JP2004340027
    • 2004-11-25
    • Toray Ind Inc東レ株式会社
    • SHIBATA YASUHIROSEKI MASAO
    • D06M10/02D06M10/00
    • PROBLEM TO BE SOLVED: To provide a fiber structure having excellent stretchability and soft touch feeling as well as water absorption properties, water repellent and stainproof property.
      SOLUTION: In the fiber structure, the ratio of number of atoms represented by OIS/CIS and NIS/CIS of a polyester-based fiber surface obtained by measurement using electron spectroscopy for chemical analysis (ESCA) by X ray irradiation is increased by 0.02, compared with a value of a part which is least ≥0.5 μm deeper from the fiber surface.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供具有优异的拉伸性和柔软的触感以及吸水性,防水防污性的纤维结构。 解决方案:在纤维结构中,通过用X射线照射进行化学分析的电子光谱法(ESCA)测量而获得的聚酯基纤维表面的OIS / CIS和NIS / CIS表示的原子数的比例增加 与距离纤维表面较深的最少≥0.5μm的部分的值相比为0.02。 版权所有(C)2006,JPO&NCIPI