    • 1. 发明专利
    • Filter and filter unit
    • 过滤器和过滤器
    • JP2009148748A
    • 2009-07-09
    • JP2008293083
    • 2008-11-17
    • Toray Ind Inc東レ株式会社
    • OMORI TAIRAMATSUMURA KAZUYATAKEDA MASANOBU
    • B01D39/16B01D61/14B01D69/10D04H1/4382
    • PROBLEM TO BE SOLVED: To provide a filter of a low pressure drop and high filtration accuracy capable of removing fine dust, bacteria, viruses and the like floating in air or in water.
      SOLUTION: The filter is characterized by comprising a filter layer of a thickness of 50 μm or greater comprised of a fiber made from a thermoplastic rein and of a nanofiber of a fiber diameter of 1 to 500 nm by 0.5 to 70 mass%, having collection efficiency of 90% or greater with respect to particles of a mean diameter of 0.3 μm at an air flow rate of 3.2 m/min, and having an initial pressure drop of not greater than 980 Pa at an air flow rate of 3.2 m/min.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供能够除去浮在空气或水中的细粉尘,细菌,病毒等的低压降和高过滤精度的过滤器。 过滤器的特征在于包括厚度为50μm以上的过滤层,其由热塑性树脂制成的纤维和纤维直径为1〜500nm的纳米纤维为0.5〜70质量% 相对于平均直径为0.3μm的颗粒,在3.2m / min的空气流速下的收集效率为90%或更高,并且在空气流速为3.2时具有不大于980Pa的初始压降 m / min。 版权所有(C)2009,JPO&INPIT
    • 2. 发明专利
    • Electromagnetic wave absorber
    • 电磁波吸收器
    • JP2009076620A
    • 2009-04-09
    • JP2007243458
    • 2007-09-20
    • Toray Ind Inc東レ株式会社
    • SUNAHARA TETSUYASUGAWARA TORUMATSUMURA KAZUYA
    • H05K9/00E04B1/92
    • PROBLEM TO BE SOLVED: To provide an electromagnetic wave absorber that is used to reduce electromagnetic wave disturbances, such as an electromagnetic wave interferences, electromagnetic wave leakages under an RFID system or wireless LAN environment, which can be used with ease and can be compactly housed, when a wireless communication system is not to be used.
      SOLUTION: In this electromagnetic wave absorber, in which a flexible resisting film layer and electromagnetic wave reflecting film layer are folded up or wound, wherein the flexible resisting film layer and electromagnetic wave reflecting film layer are deployed substantially in parallel, in a spreading manner separated by intervening spaces, expressing an electromagnetic wave absorptivity.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种用于减少电磁波干扰,RFID系统或无线局域网环境下的电磁波泄漏等电磁波干扰的电磁波吸收体,其可以容易地使用,并且可以 当不使用无线通信系统时,应紧凑地安装。 解决方案:在柔性电阻膜层和电磁波反射膜层折叠或缠绕的电磁波吸收体中,其中柔性抗蚀膜层和电磁波反射膜层基本上平行地展开, 通过中间空间分开的展开方式,表现出电磁波吸收率。 版权所有(C)2009,JPO&INPIT
    • 6. 发明专利
    • Reproduced molding material and manufacturing method thereof
    • 复制成型材料及其制造方法
    • JP2006115877A
    • 2006-05-11
    • JP2004303928
    • 2004-10-19
    • Toray Ind Inc東レ株式会社
    • NAKAHARA MAKOTOMITO OSAMUMATSUMURA KAZUYA
    • A63F7/02A63F5/04B09B3/00B09B5/00
    • PROBLEM TO BE SOLVED: To provide a reproduced molding material which can protect environments by the reduction of waste, is highly rigid, is excellent in the driving property and drawing strength of nails and does not easily cause nail deformation and member cracking at the time of driving the nail, especially the reproduced molding material suitably used as a game machine member such as a casing plate for a pachinko slot machine, and a manufacturing method thereof.
      SOLUTION: The reproduced molding material includes a recovered material obtained by recovering used members, a thermoplastic synthetic resin bonding agent having a fusing point below 200°C and fibers having a fiber length within the range of 3-30mm, the modulus of blending of the fibers to the total weight is within the range of 5-40 wt.%, and the recovered material and the fibers are bonded by the bonding agent.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了提供通过减少废物来保护环境的再现成型材料,是高度刚性的,具有优异的指甲的驱动性能和拉伸强度,并且不容易引起指甲变形和构件开裂 特别是适用于弹球机的外壳板等游戏机构件的再生成型材料的驱动时间及其制造方法。 解决方案:复制的成型材料包括通过回收使用的部件获得的回收材料,具有低于200℃的熔点的热塑性合成树脂粘合剂和纤维长度在3-30mm范围内的纤维, 纤维与总重量的混合在5-40重量%的范围内,回收的材料和纤维通过粘合剂粘结。 版权所有(C)2006,JPO&NCIPI
    • 7. 发明专利
    • Base cloth for air belt and manufacturing method therefor
    • 用于航空皮带的基带及其制造方法
    • JP2006096258A
    • 2006-04-13
    • JP2004286516
    • 2004-09-30
    • Toray Ind Inc東レ株式会社
    • MORIMOTO ATSUSHITSUCHIZAKI TORUMATSUMURA KAZUYA
    • B60R21/16D03D1/00D03D1/02
    • PROBLEM TO BE SOLVED: To provide a base cloth for an air belt, an air belt made of the base cloth, and a manufacturing method for them, which allow the employment of a thinner base cloth composing an air belt to provide the air belt offering a feeling of unity that is highly convenient in storage, lighter in weight to relieving an occupant from a feeling of stress and fatigue, and suppresses a shift between base cloths due to abrasion.
      SOLUTION: The base cloth for the air belt is made by coating at least one surface of a fabric, which is made up of filaments whose each single element has a flat section, with a resin. The base cloth is provided by using the manufacturing method for the fabric for the air belt at least including such a weaving process and a finishing process that a weaving tension is determined to be within 30 to 200 g/fabric in the weaving process and a knife coating is employed in the finishing process.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了提供一种用于气带的基布,由基布制成的气带及其制造方法,其可以使用构成气带的较薄的基布来提供 空气带具有在储存中非常方便的统一感,更轻的重量以减轻乘员的压力和疲劳感,并抑制由于磨损引起的基布之间的偏移。 解决方案:用于空气带的基布通过涂布由每个单一元件具有平坦部分的细丝组成的织物的至少一个表面与树脂制成。 基布通过使用用于气带的织物的制造方法提供,至少包括织造过程和织造过程中编织张力在30至200g /织物内的精加工过程和刀 在整理过程中采用涂层。 版权所有(C)2006,JPO&NCIPI
    • 10. 发明专利
    • Polyester fiber structure
    • 聚酯纤维结构
    • JP2011208346A
    • 2011-10-20
    • JP2011052562
    • 2011-03-10
    • Toray Ind Inc東レ株式会社
    • NARITA SHUSAKUKAJIYAMA HIROSHIMATSUMURA KAZUYA
    • D01F6/62D01F6/92D04H1/435D04H1/46
    • PROBLEM TO BE SOLVED: To provide a polyester fiber structure which has low shrinkage and low tensile strength at a high temperature, and attains compatibility between dimensional stability and formability in hot forming.SOLUTION: The polyester fiber structure is a fiber structure which uses a part or all of polyester fiber formed by kneading 5-95 mass% of polytrimethylene terephthalate resin and 95-5 mass% of polyethylene terephthalate resin, and is a polyester fiber structure having one peak of 210-220 as a melting point peak of the fiber. The tensile strength retention at high temperature of the fiber structure is 67% or less in length and 82% or less in width. The fiber structure is a needle-punched nonwoven fabric.
    • 要解决的问题:提供一种在高温下具有低收缩率和低拉伸强度的聚酯纤维结构,并且在热成型中获得尺寸稳定性和成型性之间的相容性。溶解性:聚酯纤维结构是使用部分的纤维结构 或通过捏合5-95质量%的聚对苯二甲酸丙二醇酯树脂和95-5质量%的聚对苯二甲酸乙二醇酯树脂形成的全部聚酯纤维,并且是具有210-220的一个峰作为纤维的熔点峰的聚酯纤维结构体。 纤维结构体的高温下的拉伸强度保持率为67%以下,宽度为82%以下。 纤维结构是针刺无纺布。