    • 1. 发明专利
    • Catalyst structure and method for manufacturing carbon nanostructure using the same
    • 使用其制造碳纳米结构的催化剂结构和方法
    • JP2012016707A
    • 2012-01-26
    • JP2011233209
    • 2011-10-24
    • Osaka PrefectureSumitomo Electric Ind Ltd住友電気工業株式会社大阪府
    • HIKATA TAKESHIMIZUKOSHI TOMOYUKI
    • B01J23/89B01J37/34C01B31/02
    • PROBLEM TO BE SOLVED: To provide a catalyst structure that improves deposition efficiency in manufacturing carbon nanostructures consisting of carbon crystals through vapor phase deposition, and to provide a method for manufacturing the carbon nanostructures using the same.SOLUTION: In the catalyst structure to be used for manufacturing carbon nanostructures consisting of carbon crystals through vapor phase deposition, a plate body is penetrated in a thickness direction with a first metal and a second metal. The first metal is formed as a plurality of filaments. The filaments are held at intervals by a substrate with their longitudinal direction aligned with the thickness direction of the plate body. One end of the filament is exposed on a first surface while the other-end is connected to the second metal to expose the second metal on a second surface. The first metal includes a material composed primarily of cobalt or nickel. The second metal includes a material containing palladium. The catalyst structure is used for a method for manufacturing the carbon nanostructures.
    • 要解决的问题:提供一种催化剂结构,其提高通过气相沉积制造由碳晶体组成的碳纳米结构的沉积效率,并提供使用其制造碳纳米结构的方法。 解决方案:在通过气相沉积用于制造由碳晶体构成的碳纳米结构的催化剂结构中,板体在第一金属和第二金属的厚度方向上穿透。 第一金属形成为多根细丝。 长丝被基板保持间隔,其长度方向与板体的厚度方向一致。 灯丝的一端暴露在第一表面上,而另一端连接到第二金属,以暴露第二表面上的第二金属。 第一金属包括主要由钴或镍组成的材料。 第二金属包括含钯的材料。 催化剂结构用于制造碳纳米结构的方法。 版权所有(C)2012,JPO&INPIT
    • 2. 发明专利
    • Catalyst structure and method for manufacturing carbon nano-structure using the same
    • 使用其制造碳纳米结构的催化剂结构和方法
    • JP2008296196A
    • 2008-12-11
    • JP2007148064
    • 2007-06-04
    • Osaka PrefectureSumitomo Electric Ind Ltd住友電気工業株式会社大阪府
    • HIKATA TAKESHIMIZUKOSHI TOMOYUKI
    • B01J23/89B01J35/02B01J35/06C01B31/02
    • PROBLEM TO BE SOLVED: To provide a catalyst structure which can improve deposition efficiency when manufacturing a carbon nano-structure composed of carbon crystals by vapor phase growth, and a method for manufacturing a carbon nano-structure using the catalyst structure.
      SOLUTION: The catalyst structure used for manufacturing the carbon nano-structure composed of carbon crystals by the vapor phase growth method has a first surface in which at least a first metal is exposed, and a second surface in which at least a second metal is exposed. The first metal and the second metal are formed so as to come into contact with each other. The first metal is composed of a material of which the main component is one selected from iron, cobalt, and nickel, and the second metal is composed of a material containing palladium.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种催化剂结构,其可以通过气相生长制造由碳晶体构成的碳纳米结构时提高沉积效率,以及使用该催化剂结构的碳纳米结构体的制造方法。 解决方案:用于通过气相生长法制造由碳晶体构成的碳纳米结构的催化剂结构具有至少暴露第一金属的第一表面和至少第二表面的第二表面 金属被暴露。 第一金属和第二金属形成为彼此接触。 第一金属由主要成分选自铁,钴和镍的材料构成,第二金属由含钯的材料构成。 版权所有(C)2009,JPO&INPIT
    • 8. 发明专利
    • Method for manufacturing carbon nanostructure, catalyst metal base and catalytic reaction container
    • 制造碳纳米管结构的方法,催化剂金属基和催化反应容器
    • JP2007222959A
    • 2007-09-06
    • JP2006043735
    • 2006-02-21
    • Sumitomo Electric Ind Ltd住友電気工業株式会社
    • HISAGAI YUICHIHIKATA TAKESHI
    • B82B3/00C01B31/02
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a carbon nanostructure, in which a high purity long-length carbon nanostructure can be stably manufactured. SOLUTION: A catalytic reaction container equipped with: an airtight container; a catalyst metal base partitioning the inner space of the airtight container into a first space and a second space; and a fixing member to fix the catalyst metal base, is used. The catalyst metal base is disposed to have a first surface in contact with the first space and a second surface in contact with the second space, and the base is processed to have a recessed portion and/or a projected portion formed in at least a part of the second surface. A source gas containing at least carbon is supplied to the first space, and the carbon reaching the second surface from the first surface through the inner part of the catalyst metal base is grown into a carbon nanostructure from the recessed portion and/or the projectrd portion as a base point. COPYRIGHT: (C)2007,JPO&INPIT
    • 待解决的问题:提供可以稳定制造高纯度长度碳纳米结构的碳纳米结构体的制造方法。 解决方案:一种装有气密容器的催化反应容器; 将所述气密容器的内部空间分隔成第一空间和第二空间的催化剂金属基体; 和用于固定催化剂金属基底的固定构件。 催化剂金属基底设置成具有与第一空间接触的第一表面和与第二空间接触的第二表面,并且基底被加工成具有形成在至少一部分中的凹部和/或突出部分 的第二个表面。 将含有至少碳的源气体供给到第一空间,从催化剂金属基体的内部到达第一表面的第二表面的碳从凹部和/或突出部分生长成碳纳米结构体 作为基点。 版权所有(C)2007,JPO&INPIT
    • 9. 发明专利
    • Method for manufacturing carbon nano-structure
    • 制造碳纳米结构的方法
    • JP2005330175A
    • 2005-12-02
    • JP2004220432
    • 2004-07-28
    • Sumitomo Electric Ind Ltd住友電気工業株式会社
    • HIKATA TAKESHI
    • B01J23/89B82B3/00C01B31/02
    • C30B29/02B01J23/8906B01J23/8913B01J23/8993B01J35/06B82Y30/00B82Y40/00C01B32/162C30B25/02Y10S977/742
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a carbon nano-structure by which a carbon nano-structure having more uniform shape and high purity is stably manufactured. SOLUTION: The method for manufacturing the carbon nano-structure is for growing carbon crystal from the crystal growth surface of a catalytic base material containing a catalytic material by vapor phase deposition and particularly ≥2 kinds of gases including gaseous starting materials are simultaneously brought into contact with the catalytic base material. The two or more kinds of gases preferably comprise one or more kinds of gaseous starting materials and one or more kinds of carrier gases. It is preferable that the carrier gas is brought into contact with the crystal growth surface and the gaseous starting material is brought into contact with at least one part in a region excluding the crystal growth surface brought into contact with the carrier gas. It is preferable that the gaseous starting material contains ions, particularly carbon ions. COPYRIGHT: (C)2006,JPO&NCIPI
    • 解决的问题:提供一种制造碳纳米结构体的方法,通过该方法能够稳定地制造具有更均匀形状和高纯度的碳纳米结构。 解决方案:用于制造碳纳米结构的方法是通过气相沉积从含有催化材料的催化基材的晶体生长表面生长碳晶体,特别是包括气态原料的≥2种气体同时 与催化基材接触。 两种或更多种气体优选包含一种或多种气态原料和一种或多种载气。 优选使载气与晶体生长面接触,使气态原料与除了与载气接触的晶体生长面以外的区域中的至少一部分接触。 优选气态原料含有离子,特别是碳离子。 版权所有(C)2006,JPO&NCIPI