    • 1. 发明专利
    • Apparatus for taking out coke sample
    • 用于烹调咖喱样品的装置
    • JPS6162837A
    • 1986-03-31
    • JP18366284
    • 1984-09-04
    • Nippon Steel CorpNissho Iwai Kk
    • HOSOKAWA KATSUYAKUGIMIYA SADAJIITO SHIGEOKASUYA NAOTO
    • C10B45/00G01N1/04
    • G01N1/04
    • PURPOSE:To properly determine the temp. information or the quality of dry distillation coke, by separately providing a chute, which has a sample outtake port radially enlarged to an extrusion member and a door, and a sample receiver to the side wall of a coke gauge. CONSTITUTION:When a coke sample is collected, the extrusion work of dry distilled coke is temporarily interrupted and a door 15 is fallen and revolved by a cylinder system 14 to open and close outtake ports 5b, 6b, 7b while chutes 8, 9, 10 are formed and cylinder rods 4 are operated from the outsides of extrusion ports 5a, 6a, 7a to extrude coke samples. Each extrusion port is enlarged radially to each rod 4.
    • 目的:正确确定温度。 信息或干馏焦炭的质量,通过分别提供一个斜槽,其具有径向扩大到挤出构件和门的样品出口端口,以及将样品容器连接到焦炭计的侧壁。 构成:当收集焦炭样品时,暂停中断干蒸馏焦炭的挤压加工,并且门15由圆筒系统14下落并旋转,以打开和关闭出口5b,6b,7b,同时滑槽8,9,10 并且从挤出口5a,6a,7a的外侧操作圆筒棒4以挤出焦炭样品。 每个挤出口径向扩大到每个杆4。
    • 2. 发明专利
    • METHOD FOR DESILICONIZING MOLTEN IRON
    • JPH03140406A
    • 1991-06-14
    • JP27804889
    • 1989-10-25
    • NIPPON STEEL CORP
    • KASHIWABARA TSUKASANAKAGAWA JUNICHIKUGIMIYA SADAJIKOMORI TOSHIYA
    • C21C1/04
    • PURPOSE:To efficiency execute pre-desiliconized refining with a small quantity of total oxygen in a short treating time by executing desiliconization by making ratio of gas oxidizer and solid oxidizer as Si oxidizer the specific ratio after lowering temp. of molten iron by adding the specific quantity of cold material at the time of executing the predesiliconizing refining to the molten iron. CONSTITUTION:Before refining the molten iron tapped from a blast furnace into molten steel, Si is oxidized to be converted into slag beforehand and steel making refining efficiency in a converter is improved. In this case, as oxidizing desiliconizing reaction of Si in the molten iron is further improved in the effect thereof as the temp. of molten iron is lower, in order to lower the temp. of molten iron, by adding the cold iron raw material with the quantity Sc shown in the equation 1 the temp. of molten iron is lowered to the suitable temp. the desiliconizing reaction. Successively, under condition of gaseous oxygen ratio [gaseous oxygen quantity/(gaseous oxygen quantity + oxygen quantity in iron oxide) X 100] shown in the equations 2, 3, the desiliconizing treatment is executed to the molten iron. The desiliconizing treatment in the molten iron can be efficiently executed with a small quantity of the oxidizer in a short time and temp. adjustment at the time of steelmaking refining in the converter subsequent to this is facilitated.
    • 4. 发明专利
    • Continuous casting method
    • 连续铸造方法
    • JPS6146360A
    • 1986-03-06
    • JP16853484
    • 1984-08-10
    • Nippon Steel Corp
    • SHIRAI TOKIYATSUNEOKA SATOSHISEZE AKIFUMIKUGIMIYA SADAJI
    • B22D11/124B22D11/12B22D11/128
    • B22D11/1206
    • PURPOSE:To eliminate the macro and micro segregation and center porosity of a billet by maintaining the surface temp. of the billet on the side nearer the mold side than the unsolidified front end at a prescribed temp. and reducing the part near the unsolidified front end according to the rate of shrinkage on solidification and making face support. CONSTITUTION:The billet 3 conducted from a mold 1 of a continuous casting machine to guide rolls 2... is passed through a walking bar type face supporting member 4 and while the part near the unsolidified front end of the billet 3 is grasped by the face, the billet is reduced according to the volume which shrinks on solidification. The surface temp. of the billet on the side nearer the mold than the unsolidified front end is maintained at 600-900 deg.C from about 1 minuet when the increasing to the rigidity to permit the uniform dispersion of the face supporting pressure over the entire shell surface can be expected to about 7 minutes when the expectation of the effective recuperation of the billet after the completion of the solidification under the face support is difficult. The casting of the ingot having no macro and micro segregation and center porosity is thus made possible.
    • 目的:通过维持表面温度消除钢坯的宏观和微观偏析和中心孔隙度。 比未固化的前端更靠近模具侧的钢坯。 根据固化收缩率和面部支撑,减少未固化前端附近的零件。 构成:从连续铸造机的模具1向引导辊2 ...穿过的坯料3通过行走型面支撑构件4,并且当坯料3的未固化前端附近的部分被 根据凝固时收缩的体积,钢坯减少。 表面温度 的钢坯比未固化的前端更靠近模具的钢坯从约1分钟保持在600-900℃,当增加到刚性以允许在整个壳体表面上的面支撑压力的均匀分散可以是 预计大约7分钟后,在面部支撑下凝固完成后有效恢复钢坯的期望是困难的。 因此,铸造不具有宏观和微观偏析和中心孔隙的铸锭成为可能。
    • 5. 发明专利
    • TUYERE FOR BLAST FURNACE
    • JPH07216421A
    • 1995-08-15
    • JP1176694
    • 1994-02-03
    • NIPPON STEEL CORP
    • KAWAMURA TAKUSHINAKAGAWA KOICHIROKUGIMIYA SADAJIINOUE YOSHIHIRO
    • C21B7/16
    • PURPOSE:To improve the cooling capacity of a tuyere only at the inside of a furnace and to drastically prolong the average service life of the tuyere by providing plural curving grooves along the end surface side of the tuyere tip part in the inner wall of the tip cooling water passage for cooling the tuyere tip part. CONSTITUTION:The curved grooves 4 are externally provided and communicated on the inner wall of the water passage 3 along the longitudinal direction of the water passage 3 for cooling the tip part of the tuyere A for blast furnace. When the depth and width of the groove 4 are defined as L and B respectively, the L/B is made to be >=0.5, and the tip part 4a and the base part 4b of the groove 4 are made to form the round curved surface. Further, the grooves 4 are preferably provided at the outer side from the straight line (Z) with which the center part (Y) of the cross sectional surface of the tip cooling water passage 3 is connected to the tip part (X) of the outer periphery of an inner cylinder of the tuyere A, i.e., at the outer cylinder side. By this method, the periodical exchanging term of the tuyere A can be prolonged.