会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 6. 发明专利
    • AERIAL POT FOR FLOATING HOT DIPPING METAL
    • JPH11209858A
    • 1999-08-03
    • JP1016998
    • 1998-01-22
    • MITSUBISHI HEAVY IND LTDKAWASAKI STEEL CONISSHIN STEEL CO LTD
    • YAMASHITA ICHIROFUKADA YASUOKATO CHIAKIAMAGASA TOSHIAKIANDO ATSUSHIHASHIDA TAKUYA
    • C23C2/00
    • PROBLEM TO BE SOLVED: To form the uniform magnetic flux density in the width direction of a steel strip and to prevent the unstable free movement of hot dipping metal by forming faced magnetic pole surfaces of an electric magnet interposing a carry-in opening part for a steel strip so as to compensate the variation of the magnetic flux density in the width direction of the strip with the steel strip passing through the carry-in opening part. SOLUTION: In order to prevent the hot dipping metal from flowing down from the carry-in opening part 13, in an aerial pot for exciting the plating by introducing the steel strip 1 into the hot dipping metal from the carry-in opening part 13 at the bottom part, the magnetic pole surfaces 17 of the electric magnet 10 generating the electromagnetic force are arranged so as to interpose the steel strip 1 at both sides of the carry-in opening part 13. At this time, the magnetic pole surfaces 17 are formed as convex shape so that the magnetic flux density between the magnetic pole surfaces becomes constant in the width direction of the strip, and as approaching the center part, the larger magnetic flux density B develops so as to develop the electromagnetic pushing-up force corresponding to this magnetic flux density B. In this way, in the whole width containing 'the strip passing part' (a) and 'no strip passing part' (b) in the carry-in opening part 13, the uniform prescribed magnetic flux density B can be held.
    • 10. 发明专利
    • Phosphation steel plate
    • 磷化钢板
    • JP2006241495A
    • 2006-09-14
    • JP2005056382
    • 2005-03-01
    • Nisshin Steel Co Ltd日新製鋼株式会社
    • UENO SUSUMUSHIMIZU TAKESHIANDO ATSUSHI
    • C23C22/12
    • PROBLEM TO BE SOLVED: To provide a phosphation Zn-Al-Mg alloy plated steel plate having improved coating film blister corrosion resistance by modifying a phosphate film.
      SOLUTION: In a chemical-converted steel plate, a phosphate film with the volume-regulation of metal elements other than Zn is deposited on a surface of the Zn-Al-Mg alloy plated steel plate. A plating layer on the surface of a base material contains, by mass, 3-15% Al and 2-5% Mg. Deposition such as Ni, Co, and Fe to be substitution-deposited on the surface of the base material through phoaphating is set to be ≤10 mg/m
      2 . Phosphate crystal of the chemical conversion film contains at least Mn or Mg of ≥0.04 mol ratio to Zn other than Zn, and the mol ratio of Ni, Co and Fe contained in the phosphate crystal to Zn is controlled to be ≤0.05.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:通过改变磷酸盐膜来提供具有改进的涂膜起泡耐腐蚀性的磷酸锌Zn-Al-Mg合金电镀钢板。 解决方案:在化学转化的钢板中,在Zn-Al-Mg合金镀覆钢板的表面上沉积具有除Zn以外的金属元素的体积调节的磷酸盐膜。 基材表面的镀层含有3〜15%的Al和2-5%的Mg。 沉积物如Ni,Co和Fe被沉积在基体材料的表面上通过印迹被设定为≤10mg/ m 2。 化学转化膜的磷酸盐晶体至少含有与Zn以外的Zn以上≥0.04摩尔比的Mn或Mg,将磷酸盐晶体中所含的Ni,Co和Fe的摩尔比控制为≤0.05。 版权所有(C)2006,JPO&NCIPI