    • 1. 发明专利
    • Laminated structure
    • 层压结构
    • JP2010194983A
    • 2010-09-09
    • JP2009045105
    • 2009-02-27
    • Mitsui Chemicals Inc三井化学株式会社
    • MATSUMOTO HIRONORIOTA SEIJIONOKI TAKAYUKIASO YOSHIAKIMATSUKI TOMOAKISAITO JUNJI
    • B32B27/32
    • PROBLEM TO BE SOLVED: To provide a laminated structure which is laminated through a hot melt adhesive for strongly bonding base materials of various types and a base material such as olefin resin. SOLUTION: Provided is the laminated structure, wherein a part of the laminated structure has at least such a structure that a layer (A), a layer (B) and a layer (C) are laminated in this order, wherein (A) is a layer consisting essentially of polyolefin, (B) is a layer containing hybrid polymer [P] having a polyolefin segment [S 1 ] and a polar polymer segment [S 2 ], and (C) is a layer composed of at least one selected from polar vinyl plastic, aromatic vinyl polymer, polyester, and the like. The [S 2 ] is obtained through radial (co) polymerization of one or more kinds of monomers that contain radical polymerizable monomer having a reactive group. The number average molecular weight of [S 2 ] section is 300 to 1 ] section is 7,000 to COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供层压结构,其通过热熔粘合剂层压,用于强力粘合各种基材和烯烃树脂等基材。 解决方案:提供层压结构,其中层压结构的一部分至少具有层(A),层(B)和层(C)至少层叠的结构,其中( A)是基本上由聚烯烃组成的层,(B)是含有聚烯烃链段[S 1]和极性聚合物链段[S 2]的杂质聚合物[P] SB>],(C)是选自极性乙烯基塑料,芳族乙烯基聚合物,聚酯等中的至少一种的层。 通过一种或多种含有具有反应性基团的自由基聚合性单体的单体的径向(共)聚合获得[S 2 ]。 [S 2]部分的数均分子量为300〜3,000,[S 1]部分的数均分子量为7,000〜40,000。 版权所有(C)2010,JPO&INPIT
    • 5. 发明专利
    • Aliphatic polyester-based resin composition and molded product thereof
    • 基于聚氨酯的树脂组合物及其成型产品
    • JP2008088363A
    • 2008-04-17
    • JP2006273385
    • 2006-10-04
    • Mitsui Chemicals Inc三井化学株式会社
    • ONOKI TAKAYUKIKAGEYAMA FUMIOARAI TAKASHIWATANABE TAKAYUKINAKANISHI TOSHIHIDE
    • C08L67/00C08K3/00C08K7/02C08L23/02
    • PROBLEM TO BE SOLVED: To provide an aliphatic polyester-based resin composition improving heat resistance, suppressing bleedout of a plasticizer and having excellent moldability by adding the plasticizer and to provide a molded product thereof.
      SOLUTION: The aliphatic polyester-based resin composition comprises 10-90 pts.wt. of an aliphatic polyester-based resin (A), 10-90 pts.wt. of a polyolefinic resin (B) {with the proviso that the sum total of the resin (A) and resin (B) is 100 pts.wt. } and 0.1-50 pts.wt. of the plasticizer (C). Furthermore, the aliphatic polyester-based resin composition may contain 0.1-60 pts.wt. of a filler (D) having ≥5 μm diameter and ≥10 aspect ratio and may contain 0.1-30 pts.wt. of a compatibilizer (E).
      COPYRIGHT: (C)2008,JPO&INPIT
    • 解决问题:提供改善耐热性的脂肪族聚酯类树脂组合物,通过添加增塑剂来抑制增塑剂的渗出并具有优异的成型性,并提供其成型体。 解决方案:脂族聚酯基树脂组合物包含10-90重量份 的脂肪族聚酯类树脂(A),10-90重量份 的聚烯烃树脂(B),条件是树脂(A)和树脂(B)的总和为100重量份。 }和0.1-50重量份 的增塑剂(C)。 此外,脂肪族聚酯类树脂组合物可以含有0.1-60重量份 的直径≥5μm,长宽比≥10的填料(D),并且可以含有0.1-30重量份。 的增容剂(E)。 版权所有(C)2008,JPO&INPIT
    • 8. 发明专利
    • Fine polyolefin particles and modified fine polyolefin particles, resin composition containing them, and application of them
    • 精细聚烯烃颗粒和改性精细聚烯烃颗粒,含有它们的树脂组合物及其应用
    • JP2011080013A
    • 2011-04-21
    • JP2009235434
    • 2009-10-09
    • Mitsui Chemicals Inc三井化学株式会社
    • FUJIMURA FUTOSHIONOKI TAKAYUKIYANAGIMOTO YASUSHIASO YOSHIAKI
    • C08F6/00C08F10/00C08F255/00C08L23/02C08L51/06C08L101/00
    • PROBLEM TO BE SOLVED: To provide fine polyolefin particles and modified fine polyolefin particles both having a small particle diameter and having a narrow particle size distribution, to provide a resin composition containing them, and to provide various applications of the fine particles. SOLUTION: The fine polyolefin particles satisfies the following requirements (a) to (c), and modified fine polyolefin particles is prepared by grafting an ethylenically unsaturated compound onto the fine polyolefin particles and further satisfies the following requirements (d) and (e): (a) the intrinsic viscosity [η] as measured in decalin at 135°C is 1-50 dl/g, (b) the average particle diameter is 3-25 μm, (c) at least 95 wt.% of the particles can pass through a mesh sieve with an opening of 37 μm, (d) the infrared absorption spectrum after methanol treatment is substantially the same as the infrared absorption spectrum before the methanol treatment, and (e) the units derived from the ethylenically unsaturated compound account for 0.05-75 wt.% of the entire fine polyolefin particles. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:为了提供具有小粒径并且具有窄粒度分布的精细聚烯烃颗粒和改性的细聚烯烃颗粒,以提供含有它们的树脂组合物,并提供细颗粒的各种应用。 解决方案:聚烯烃微粒满足以下要求(a)至(c),通过将烯键式不饱和化合物接枝到细聚烯烃颗粒上并进一步满足以下要求(d)和( e):(a)在135℃萘烷中测得的特性粘度[η]为1-50dl / g,(b)平均粒径为3-25μm,(c)至少95wt% 的颗粒可以通过37μm的开口的筛网,(d)甲醇处理后的红外吸收光谱与甲醇处理前的红外吸收光谱基本相同,(e)衍生自烯属的单元 不饱和化合物占整个细聚烯烃颗粒的0.05-75重量%。 版权所有(C)2011,JPO&INPIT
    • 9. 发明专利
    • Laminated structure
    • 层压结构
    • JP2010194984A
    • 2010-09-09
    • JP2009045106
    • 2009-02-27
    • Mitsui Chemicals Inc三井化学株式会社
    • ONOKI TAKAYUKIASO YOSHIAKIMATSUMOTO HIRONORIMATSUKI TOMOAKIKANEKO HIDEYUKI
    • B32B27/32
    • PROBLEM TO BE SOLVED: To provide a laminated structure formed by laminating a layer containing an olefinic polymer, and a layer comprising at least one selected from aromatic vinyl resin, polycarbonate resin and acrylic resin, through an adhesive for powerfully bonding both layers. SOLUTION: The laminated structure has, at least partially, a structure in which (A) a layer containing the olefinic polymer, (B) a layer containing a hybrid polymer [P] having a polyolefine segment [S 1 ] and a polar polymer segment [S 2 ], and (C) the layer comprising at least one selected from aromatic vinyl resin, polycarbonate resin and acrylic resin, are laminated in this order. A solubility parameter ((J/cm 3 ) 1/2 ) of the resin that composes the layer (C) is 18.5 to 21, [S2] is composed of a radical polymerizable monomer substantially having no reactivity, and a solubility parameter ((J/cm 3 ) 1/2 ) of [S 2 ] is 19 to 21. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供通过层压含有烯烃聚合物的层和包含选自芳族乙烯基树脂,聚碳酸酯树脂和丙烯酸树脂中的至少一种的层的层压结构,通过粘合剂强力地结合两层 。 解决方案:层压结构至少部分地具有以下结构:(A)含有烯烃聚合物的层,(B)含有具有聚烯烃链段的杂化聚合物[P]的层[S 1 ]和极性聚合物链段[S 2],和(C)包含选自芳族乙烯基树脂,聚碳酸酯树脂和丙烯酸树脂中的至少一种的层依次层叠。 构成层(C)的树脂的溶解度参数((J / cm×SP> 3×SP)) 1/2 )为[18],[S2]由 基本上不具有反应性的自由基聚合性单体和[S 2 ]的溶解度参数((J / cm 3 1/2 ) (C)2010年,JPO&INPIT